Dielectric Properties of SBT capacitor with annealing temperatures

열처리 온도에 따른 Pt/SBT/Pt 캐패시터의 유전특성

  • Published : 2001.07.18

Abstract

The $Sr_{0.8}Bi_{2.4}Ta_2O_9$(SBT) thin films are deposited on Pt-coated electrode(Pt/$TiO_2$/ $SiO_2$/Si) using RF magnetron sputtering method. With increasing annealing temperature from 600[$^{\circ}C$] to 850[$^{\circ}C$], Bi-layered perovskite phase was crystallized above 650[$^{\circ}C$]. The dielectric constant is 213 at annealing temperature of 750[$^{\circ}C$] and dielectric loss have a stable value within 0.1. Leakage current density is $1.01{\times}10^{-8}A/cm^2$ at annealing temperature of 750[$^{\circ}C$].