Fatigue Crack Growth Behavior of Non-Magnetic Steel with Large Grain Size

조대결정 비자성강의 피로균열진전특성

  • Published : 2001.04.01

Abstract

Fatigue crack growth tests were carried out using high manganese cast steel under constant amplitude loading. Crystal grain size of the material is about 1000$\mu\textrm{m}$. For this material, the fatigue crack growth mechanism of high manganese steel was clarified from results such as observation of crack growth path and fracture surface. $\Delta$$K_{th}$ is about 8MPa$\surd$m which is quiet large as compared to the general structural steels and the crack growth rate is lower than the general structural steels especilly in the low $\Delta$K regsion. The reason of this behavior is crack closure due to fracture surface roughness.

Keywords