Cast austenitic stainless steel piping pump, valve casings, and elbows are susceptible to reductions in toughness and ductility because of long term exposure at the operating temperatures in LWR(light water reactor). In this paper, we have measured the material properties of long term aged CF-8A cast stainless steel, accelerated aging at $400^{\circ}C$. These studies have been carried out using Indentation tests(automated ball indentation and nano-indentation) and EDS(energy dispersive spectroscopy). The fracture toughness of CF-8A cast stainless steel was also determined by using standard fracture toughness and Automated Ball Indentation.