Microstructure and Properties of ST-based Ceramic Thin Film

ST계 세라믹 박막의 미세구조 및 특성

  • Published : 2005.05.27

Abstract

The $(Sr_{1-x}Ca_x)TiO_3$(SCT) thin films are deposited on Pt-coated electrode (Pt/TiN/$SiO_2$/Si) using RF sputtering method with substitutional contents of Ca. The optimum conditions of RF power and Ar/$O_2$ ratio were 140[W] and 80/20, respectively. Deposition rate of SCT thin film was about 18.75[$\AA$/min]. The dielectric constant was increased with increasing the substitutional contents of Ca, while it was decreased if the substitutional contents of Ca exceeded over 15[mol%]. The capacitance characteristics had a stable value within ${\pm}4$[%] in temperature ranges of -80~+90[$^{\circ}C$].