  • 이상헌 (선문대학교 전자공학과) ;
  • 최용 (선문대학교 전자재료공학과)
  • Lee, Sang-Heon (Department of Electronic Engineering, Sunmoon University) ;
  • Choi, Yong (Department of Electromaterial Engineering, Sunmoon University)
  • 발행 : 2010.06.16

초록

YBCO ceramic specimens were fabricated by added $BaTiO_3$ as donors and sintered $950^{\circ}C$/24hrs. Average grain size decreased with increased in added $BaTiO_3$. Affect to grain growth. XRD result, peak strength was lowed then crystallization not well all specimens. All specimens critical temperature about 90k.