Study on Thermal Expansion of $Si_2O-Al_2O_3$ System

$Si_2O-Al_2O_3$계의 열팽창성에 관한 연구

  • 이종근 (한양대 무기재료공학과) ;
  • 이병하 (한양대 무기재료공학과) ;
  • 전승관 (한양대 무기재료공학과)
  • Published : 1980.03.01

Abstract

Thermal expansion property of $SiO_2-Al_2O_3$ system consisted of Muan clay, Hadong Pink Kaolin and Dangjin Silica was studied. Specimens were heated at the constant rate of 18$0^{\circ}C$/hr to the max. temperatures of 115$0^{\circ}C$ to 130$0^{\circ}C$ with an interval of $25^{\circ}C$, and matured for 3hrs. The result of X-Ray diffraction analysis showed that main crystals formed were $\alpha$-quartz, $\alpha$-cristobalite and mullite. Linear thermal expansion was measured at 90$0^{\circ}C$. The results of the linear thermal expansion were decreased regularly with the increase of the sintering temperature in accordance with the following equation. $y=5$\chi$\perp1100^{\circ}$. Where $\chi$ is amounts of kaolin (wt%), and y is temperature of the changing point of linear thermal expansion.

Keywords

References

  1. Introduction to ceramic W.D. Kingery;H.K. Bowen;D.R. Uhlmann
  2. Bull. Amer. Ceram. Soc v.43 no.2 Thermal Expanision of Refractory Brick E. Ruh;R.W. Wallace
  3. Refractories. J v.1 Strain Generation During the Firing of Dense Silica Shapes M. Cross;B.A. Lewis;J.K. Forster;G.A. Carter
  4. Refractories. J. v.7;8 no.4 Aspects of bloating fireclay reractories P.K. Bhaumik
  5. J. Amer. Ceram. Soc v.42 no.7 Reaction Between Firing Ladle Bricks and Basic slags E.A. Monroe
  6. Trans.Brit.Ceram Soc v.57 The Theoretical Effects of Brick Composition on Ladle Life W.F.Ford
  7. Refractories J. v.7;8 Refractories performance in mixers and Ladles T.D.E. Reeves;P. Payne