High purity, submicron BaTiO3 powder was prepared by a hydrothermal technique using Ba(OH)2.8H2O, TiCl4 and NH4OH as starting raw materials. The submicron BaTiO3 powder was synthesized at 130~23$0^{\circ}C$ for 2.5h to yield highly crystalline particles with a narrow particle distribution. The mole ratio of Ba(OH)2.8H2O/TiO(OH)2 was 1.5. It is possible to obtain BaTiO3 with Ba : Ti=1.00$\pm$0/01. The samples densified well at 13$25^{\circ}C$, showing a uniform and fine grain structure. The grain size ranged between 0.3 and 0.5${\mu}{\textrm}{m}$. The products obtained by hydrothermal treatment at various temperatures from 130 to 23$0^{\circ}C$ were characterized by XRD, DTA, BET and SEM etc.

Keywords

References

  1. Introduction to Ceramics W.D. Kingery(et al.)
  2. Ferroelectrics v.5 Ferroelectric and Antiferro Electric Materials E.C. Subbarao
  3. Ferroelectrics v.10 Electrode and Materials Problems in Ceramic Capacitors W R. Buessem;T.I. Procopowicz
  4. J. Am. Ceram. Soc. v.30 G.N. Howaff;R.G. Breckenridge;J.M. Brownlow
  5. J. Phys. Chem. Solids v.23 E.C. Subbarao
  6. J. Am. Ceram. Soc. v.47 no.10 W. Heywang
  7. Piezoelectric Crystals and Their Application to Ultrasonics W.P. Mason
  8. J. Res. N. B. S. v.56 no.5 W.S. Clabaugh;E.M. Swiggard;R. Gilchrist
  9. Preparation of BaTiO₃and Other Ceramic Powder by Coprecipitation of Citrates in an Alcohol v.49 no.11 B.J. Mulder
  10. J. Am. Ceram. Soc. v.49 no.6 K. Kiss;J. Madger;M.S. Vukasovich;R.J. Lockhart
  11. Ultrastructure Process of Ceramics, Glasses and Composite L.L. Hench;D.R. Ulrich
  12. U.S. Patent, 2, 985, 506 Method of Producing Barium Titanate S. Divita;R. Fisher