Abstract

Fatigue life and retardtion behavior after through-thickness were examined experimentally by using a CT specimen and surface-cracked specimen. The material used was 3% Ni-Cr-Mo steel. The fatigue crack shape before through-thickness is almost semicircular, and the measured aspect ratio is larger than the value obtained by calculation using the K value proposed by Newman-Raju. It is found that the crack growth behavior on the back side after through-ghickness is unique and can be divided into three stages a, b and c. A retardation parameter has been used successfully to predict the growth of cracks in specimen, and in this time, retardation factor is 4.3. By using the crack propagation rule considering on retardation state and the K value proposed by the authors, the remarkable crack growth behavior and the change in crack shape can be evaluated quantitatively.

Keywords

References

  1. Resolution v.A328 no.Ⅸ IMCO
  2. 원자력공업 v.30-11 失川(외2명)
  3. 일본기계학회논문강연, No. 86-0793B, No. 86-0794B 岩館(외3명)
  4. 일본조선학회논문집 v.132 金澤(외2명)
  5. 일본조선학회논문집 v.137 川原(외1명)
  6. ASTM STP 631 Cruse,T.A.(외 2명)
  7. ASTM STP 677 Hodulak,L.(외 3명)
  8. 일본기계학회논문집 v.52-483,A 安藤(외4명)
  9. JSME Int. J. v.30-270 Ando,K.(외4명)
  10. 일본기계학회논문집 v.58-487,A 南起祐(외3명)
  11. JSME Int. J. v.31-2 NAM,K.W.(외3명)
  12. 일본기계학회논문집 v.55-516,A 南起祐(외3명)
  13. 일본고압력기술 v.27-4 南起祐(외3명)
  14. Eng. Fract. Mech. v.8 Natsuoka,S.(외2명)
  15. Eng. Fract. Mech. v.10 Bathias,C.(외2명)
  16. 일본재료학회논문집 v.32-363 城野(외3명)
  17. ASTM STP 513 von Euw,E.F.J.(외2명)
  18. ASTM STP 560 Newman,J.C.Jr
  19. Eng. Fract. Mech. v.11 Newman,J.C.Jr.;Raju,I.S.
  20. ASME Series D v.94 Wheeler,O.E.