Vickeres Indentation법에 의한 페라이트와 접합유리에서의 응력해석

Interpretation of Stresses in the Glass Bonded Ferrites by Vickeres Indentation Method

  • 안정환 (아주대학교 재료공학과) ;
  • 제해준 (한국과학기술연구원 세라믹스부) ;
  • 홍국선 (한국과학기술연구원 세라믹스부) ;
  • 안재환 (아주대학교 재료공학과) ;
  • 고경현 (아주대학교 재료공학과)
  • 발행 : 1993.06.01

초록

Residual stresses is one of the major factors to degrade the magnetic properties of VCR magnetic heads. Vicker's indentation technique was adapted to estimate the residual stresses Residual stresses and distribution in the glass and ferrite were obtained after bonding ferrite with glass, varing the cooling rate. The compressive and tensile stresses were developed in the interface and gradually decreased with increasing distance from the interface. The stresses were decreased with a cooling rate. The mean values of residual stress in ferrite were 10MN/㎡, 8MN/㎡, 5MN/㎡ with cooling rate 10℃/min, 5℃/min, 1℃/min respectively. When the bonded sample was annealed above the glass transition temperature followed by cooling at 5℃/min cooling rate, the residual stress was reduced to 6MN/㎡.

키워드

참고문헌

  1. Nat. Tech. Rep. v.22 no.6 Ferrites for Magnetic Recording Heads E. Hirota;K. Kugimya
  2. IEEE Trans Mag v.Mag-10 The Effects of Stress on some Properties of Mn-Zn Ferrite E.C. Snelling
  3. IEEE. Trans. Mag v.Mag-14 no.2 Mechanically Induced Anisotropy and its Effects on Magnetic on Magnetic Permeability in Single Crystal Ferrite K. Aso
  4. Ceramic Materals for Magnetic Heads v.69 no.4 Ceramic Materials for Magnetic Heads K. Kugimiya
  5. 요업재료의 과학과 기술 v.6 no.4 VCR자기헤드용 접합유리 홍국선;재혜준;장성도
  6. Nat. Tech. Rep. v.25 no.1 Residual Stresses of Mn-Zn Ferrite Polished Surface and Effect on Magnetic Properties T. Yonezawa;K.Yokoyama;N. Ito
  7. Sumimoto Tokushu Sinzoku Giho v.9 Stress Dependence of Magnetic Properties of Ferrite S. Kawahara;S. Toyota
  8. J. Am. Ceram. Soc. v.60 no.1-2 An Indentation Technique for Measuring Stresses in Tempered Glass Surfaces D.B. Marshall;B.R. Lawn
  9. J. Mat. Sci. v.10 Equilibrium Penny-like Cracks in Indentation Fracture B.R. Lawn;E.R. Fuller
  10. J. Am. Ceram. Soc. v.59 no.7-8 Fracture Toughness Determination by Indentation A.G. Evans;E.A. Charles
  11. J. Am. Ceram. Soc. v.63 no.9-10 Elastic/Plastic Indentation Damage in Ceramics: The Median/Radial Crack System B.R. Lawn;A.G. Evans;D.B. Marshall
  12. J. Am. ceram. Soc. v.64 no.9 A Critical Evaluation of Indentation Techniques for Measuring Frature Toughness:Ⅰ, Direct Crack Measurements G.R. Ansris;P. Chantikul;B.R. Lawn;D.B. Mashall
  13. J. Mat. Sci. Lett. v.1 Evaluation of Kic of Brittle Solids by the Indentation Method with Low Crack-to-Indent Ratio K. Niihara;R. Morena;H. Hasselman
  14. Acta. metal v.32 no.10 Facture Analysis of Single Crystal Manganese Zine Ferrites Using Indentation Flows K. Tanaka;Y. Kitahara;Y. Ichnose;T. Ilmura
  15. Hand Book of Glass Properties N. P. Bansal;R.H. Doremus
  16. 應用物理 v.36 no.8 Light Figures and Surface Structures Developed by Chemical Etching fo Mn Ferrite, Zn Ferrite and some Mn-Zn Ferrite Crystal M. Yamamoto;J. Watanabe;H. Suenaga
  17. Yogyo-Kyokai-Shi v.91 no.4 Fracture Toungness of Mn-Zn Ferrite Single Crystal T. Nishikawa;Y. Okamoto;S. Inakami