The Fatigue Behavior by Variety of Crack Length of Surface Cracked Plate with Stress Concentration Part

응력집중부를 갖는 표면균열재의 균열길이 변화에 따른 피로거동

  • 남기우 (부산수산대학교, 공과대학) ;
  • 김선진 (부산수산대학교, 공과대학)
  • Published : 1995.06.01

Abstract

Surface defects in structural members are apt to be origins of fatigue cracks growth, which may cause serious failure of whole structures. Most structure has a part where stress concentrates such as welded joints, corner parts, etc. And then, analysis on crack growth and penetration from these defects, therefore, is one of the most important subjects for the reliability of LBB design. The present paper has performed an experimental and analysis on the fatigue crack propagation by variety in crack length of surface cracked plate with stress concentration part. The crack growth behavior can be explained quantitatively by using Newman-Raju equation and the stress partitioning method proposed by ASME B&P Code Sec. XI. The stress concentration factor $K_t$ has affected on the crack growth. The crack growth after penetration depends upon the initial front side crack length.

Keywords

References

  1. 日本原子力學會要旨集(第1分冊) BWR一次系Stainlessの健全性評價-第4報 表面龜裂の板厚貫通後の進展評價 坂田信一;罔村 降;夏本邦夫;町田 進; 深倉壽一
  2. JSME Int. J. v.30 The fatigue life and crack through-thickness behaviour of a surface-cracked plate (for the case of tensile load) K.Ando;S.Fujibayashi;K.W.Nam;M.T.Takahashi;N.Ogura
  3. 대한기계학회논문집 v.5 no.6 고장력강의 피로수명과 균열관통거동에 관한 연구 남기우
  4. 한국어업기술 v.28 no.2 평활시험편에 있어서 균열형상비 변화에 따른 표면균열의 피로수명과 균열관통거동 남기우;엄윤성
  5. 대한기계학회 '92년도 춘계학술강연회 논문집(I) 응력집중 표면균열의 성장 및 관통거동 남기우
  6. Boiler and pressure vessel code. Sec,XI ASME
  7. Engng. Fract. Mech. v.15 An Empirical stress intensity factor equation for the surface crack J.C.Newman,Jr;I.S.Raju
  8. 日本原子力學會要旨集(第1分冊) BWR一次系Stainless鋼配管の健全性評價-第5報 配營の表面龜裂進展解析法 吉澤弘泰;薺藤正博;小泉和夫;坂田信一;結城良治,金澤武
  9. 日本壓力技術 v.28 no.4 波勞龜裂の板厚貫通擧動とその寸法效果 南起祐;宮里直矢;安藤柱;小倉信和