초록
We have measured the optical properties, thickness, and energy band gap of the P $b_{1-x}$/100/L $a_{x}$100/ $Ti_{1-}$0.25x/100/ $O_{3}$ (PLT(x)) thin film prepared by the sol-gel method with varying the La concentration, x, fyom 15 nto 33 mol%. We have obtained the values from the tranmission spectrum and employed the envelope method in anayzing the spectrum. We have also performed the simulation of the transmission spectrum on the PC (personal computer) to verify the accuracy of the values 15 to 33mol%, the refractive index (at .lambda.=632.8nm) increases from 2.39 to 2.44. The extinction coefficient does not depend on the la concentration but mainly on te wavelength, and has the values between 0.2 and 0.5 at the wavelength shorter than 330nm and between 0.001 and 0.008 at the wavelength longer than 700nm. The energy band gap of the PLT (x) thin film has been obtained on the assumption of the direct band-to-band transition. It decreases from 3.28 to 3.17eV as the La concentration increases from 15 to 33 mol%. The thickness of the PLT(x) thin film has been also obtained in high accuracy by the envelope method..