Joining of Presureless Sintered SiC Ceramics using $MgO-Al_2O_3-SiO_2$ System

$MgO-Al_2O_3-SiO_2$계를이용한 상압소결 SiC의 접합

  • 이홍림 (연세대학교 세라믹공학과) ;
  • 남서우 (연세대학교 세라믹공학과) ;
  • 한봉석 (연세대학교 세라믹공학과) ;
  • 박병학 (포항산업과학연구원 구조세라믹스팀) ;
  • 한동빈 (포항산업과학연구원 구조세라믹스팀)
  • Published : 1997.07.01

Abstract

Pressure sintered SiC specimens were joined using MgO-Al2O3-SiO2 (MAS) glass which has a thermal expansion coefficient similar to that of SiC. MAS melt showed excellent behavior of wetting on the SiC substrate over 148$0^{\circ}C$, and the wettability was much influenced by the joining atmosphere. The joining was conducted at 150$0^{\circ}C$ for 30 min in Ar atmosphere. The flexural strength of the joined specimen shows 342~380 MPa up to 80$0^{\circ}C$, which is almost the same as that of as-recieved SiC specimen. However, the flexural strength of the joined specimen decreased to about 80 MPa at 90$0^{\circ}C$ due to softening of the glass melt. The analyses od XRD and WDS show that the reaction between the SiC specimen and the MAS melt produces the oxycarbide glass, which had a high strength and a good stability at high temperatures.

Keywords

References

  1. 엔지니어링 세라믹스 이홍림(譯);山口喬(著)
  2. 고온재료의 과학과 응용 이홍림(譯);山口名良(著)
  3. J. Am. Cer. Soc. v.68 no.6 Feasibility Study of the Welding of SiC T. J. Moore
  4. Am. Ceram. Soc. Bull. v.69 no.3 Joining of Non-Oxide Ceramics for High Temperature Applications C. H. Bates;H. R. Foley;G. A. Rossi;G. L. Sundberg;F. J. Wu
  5. J. Mat. Sci. Lett. v.15 Joining of Dense Silicon Carbide by Hot Pressing T. Iseki;K. Arakawa;H. Suzuki
  6. Am. Cer. Soc. Bull. v.60 no.2 Joining of S₁C to SiC Using Polyborosiloxane S. Yajima;K. Okamura;T. Shishido;Y. Hasegawa;T. Matsuzawa
  7. J. Am. Ceram. Soc. v.75 no.1 Joining of Silicon Carbide/Silicon Carbide Composites and Dense Silicon Carbide Using Combustion Reactions in the Titanium-Carbon-Nickel System Barry H. Rabin
  8. J. Mater. Sci. v.22 Brazing of Presuress Sintered SiC Using Ag-Cu-Ti Alloy J. K. Boadi;T. Yano;T. Iseki
  9. J. Mater. Sci. v.20 Bonding Methanism between Silicon Carbide and Thin Foils of Reactive Metals S. Morozumi;M. Endo;M. Kikuchi;K. Hamajima
  10. J. Am. Ceram. Soc. v.74 no.8 Thermodynamic Brazing Alloy Design for Joining Silicon Carbide Josheph R. McDermid;Robin A. L. Drew
  11. J. Mat. Sci. v.30 Contact Phenomena and Interactions in the System SiC-SiO₂-$R_xO_y$ in Condensed Matter, Part 1, Wetting Behaviour of Silicate Glasses on the Surface of Silicon Carbide at Elevated Temperatures A L Yurkov;B. I. Polyak
  12. J. Am. Ceram. Soc. v.79 no.8 Mechanical Charaterization of Sol-Gel Derived Silicon Oxycarbide Glasses G. D. SorarU;Elisabetta Dallapiccola;Gennaro D'Andrea
  13. Mater. Lett. v.3 no.11 Novel Multianion Mg-Si-Al-O-C Oxycarbide Glass J. Homeny;S. H. Risburd
  14. J. Am. Ceram. Soc. v.70 no.5 Comparison of the Properties of Oxycarbide and Oxynitride Glasses J. Homeny;G. G. Nelson;S. W. Paulik;S. H. Risbud
  15. J. Non-Cryst. Solids v.42 Oxynitride Glasses R. E. Loehman
  16. J. Non-Cryst. Solids v.56 Mechanical Properties of Silicon-Oxynitride Glasses D. N. Coon;J. G. Rapp;R. C. Bradt;C. G. Pantano
  17. J. Am. Ceram. Soc. v.67 no.11 Mg-Al-Si-O-N Glasses; Preparation and Mechanical Properties J. Homeny;D. L. McGarry
  18. J. Am. Ceram. Soc. v.71 no.5 Oxycarbide Glasses in the Mg-Al-Si-O-C System J Homeny;G.G. Nelson;S H. Risburd
  19. J. Am. Ceram. Soc. v.67 no.12 Effect of Interlayers in Ceramic-Metal Joints with Thermal Expansion Mismatches K. Suganuma;T. Okamoto;M. Koizumi