Hydration of Active-Belite Cement with Gypsum and Slag

석고와 슬래그를 첨가한 Active-Belite Cement의 수화특성

  • 이성호 (한양대학교 세라믹 공정연구센터) ;
  • 박동철 (동양중앙연구소) ;
  • 김남호 (동양중앙연구소) ;
  • 최상홀 (한양대학교 세라믹 공정 연구센터)
  • Published : 1998.04.01

Abstract

Active belite cement clinkers were synthsized by using natural raw materials with borax and calcium phosphate ({{{{ {Ca }_{3 }( {PO}_{4}) }}2) In both case {{{{alpha ^、 {C }_{2 }S }} were formed but borax was more efficient. The cement syn-thesized with the addition of borax was hydrated with the addition of anhydrite(5 wt%) and slag(30wt%, 40wt% 50wt%) The addition of 50wt% slag with anhydrite was good for strength development in 7days and the compressive strength was developed to twice than no addition of slag at 28 days strength.