구상흑연주철재의 흑연에 의한 피로강도의 평가

Evaluation of Fatigue Strength by Graphite in Ductile Cast Iron

  • 이경모 (거창기능대학 기계설계학과) ;
  • 윤명진 (경일대학교 기계공학부) ;
  • 이종형 (금오공과대학교 기계공학부)
  • 발행 : 2003.01.01

초록

In this study, based on the effect of the interaction of fracture mechanics by graphite and fatigue limit phenomena of the microscopic observation various matrix structure, spheroidal ratio, size of graphite and distribution etc. parameters containd with Ductile Cast Iron. Therefore, in this study, different ferrite-pearlite matrix structure and spheroidal ratio of graphite of 70%, 80% and 90%, GCD40, GCD45-1 and GCD45-2 series and three different ferrite-pearlite matrix structure, GCD 45-3, GCD 50, GCD 60 series, all of which contain more than 90% spheroidal ratio of graphite, were used to obtain the correlation between mean size of spheroidal graphite and fatigue strength. (1) 73% pearlite structure had the highest fatigue limitation while 36% pearlite structure had the lowest fatigue limitation among ferrite-pearlite matrix. the increase in spheroidal ratio with increasing fatigue limitation, 90% had the highest, 14.3% increasing more then 10%, distribution range of fatigue life was small in same stress level. (2) (equation omitted) of graphite can be used to predict fatigue limit of Ductile Cast Iron. The Statistical distribution of extreme values of (equation omitted) may be used as a guideline for the control of inclusion size in the steelmaking processes.

키워드

참고문헌

  1. Masahiro Endo, Yukitaka Murakami, 'Effects of an Artificial Small Defect on Torsional Fatigue Strength of Steels, ASME, Vol. 109, pp. 124-129, 1987
  2. Yukitaka Murakami, M. Endo, 'Effects of Defects, inclusions and inhomogeneities on Fatigue Strength, Vol. 16, pp. 163-182, 1994 https://doi.org/10.1016/0142-1123(94)90001-9
  3. Yukitaka Murakami, Effects of Small Defects and Nonmetallic Inclusions on The Fatigue Strength of Metals, JSME, Vol. 32, No. 2, pp. 167-180, 1989
  4. Y. Muraksmi, Inclusion Rating by Statistics of Extreme Values and Its Application to Fatigue Strength Prediction and Quality Control of Materials, J. Res. Natl. Inst. Stand. Technol., Vol. 99, pp. 345-351, 1994 https://doi.org/10.6028/jres.099.032
  5. Smith R. A., Short Fatigue Cracks, Fatigue Mechanisms Advances in Quantitative Measurement of Physical Damage, ASTM STP 811, J. Lankford, D. L. Davidson, W. L. Morris, and R. P. Wei, Eds., American Society for Testing and Materials, pp. 264-279, 1983
  6. Smith R. A., On The Short Crack Limitations of Fracture Mechanics, Int. J. of Fracture, 13, PP. 717-721, 1977 https://doi.org/10.1007/BF00017308
  7. Tsuneshichi Tanaka, Hideak Nakayama, Akiyoshi Sakaida, Takashi Imamichi, Evaluation of Weibull Parameters For Static Strengths of Ceramics Monte Carlo Simulation, MSRI, Vol. 1, No. 1, pp. 51-58, 1995
  8. Y. Murakami and S. Nemat-Nasser, Growth and Stability of Interacting Surface Flaws Of Arbitrary Shape, EFM, Vol. 17, No. 3-A, pp. 193-210, 1983 https://doi.org/10.1016/0013-7944(83)90027-9
  9. Murakami Y., Endo M., Effects of Hardness and Crack Geometries on ${\delta}\;K_{th}$ of Small Cracks Emanating from Small Defects, The Behaviour of Short Fatigue Cracks, EGF Pub. 1 (Edited by K. J. Miller and E. R. de los Rios), pp. 275-293, 1986
  10. Kendall, J. M., James, M. N., and Knott, J. F., The Behaviour of Physically Short Fatigue Cracks in Steels, The Behaviour of Short Fatigue Cracks, EGF Pub. 1 (Edited by K.J. Miller and E. R. de los Rios), pp. 241-258, 1986
  11. Hideo, Kitagawa, Yuji Nakasone, and Satoru Miyashita, Measurement of Fatigue Damage by Randomly Distributed Small Cracks Data, ASTM STP 811, pp. 233-263, 1983
  12. T. Kunio, M. Shimizu, K. Yamada, K. Sakura, T. Yamamoto, 'The Early Stage of Fatige Crack Growth in Martensitic Steel,' Int. J. of Fracture, Vol. 17, No. 2, pp. 111-119, 1981 https://doi.org/10.1007/BF00053515
  13. Nisitani, H. and Goto, M., A Small-Crack Growth Law and its Application to the Evaluation of Fatigue Life, The Behaviour of Short Fatigue Cracks, EGF Pub. 1 (Edited by K. J. Miller and E. R. de los Rios), pp. 461-478, 1986
  14. 加藤容三, 中野典彦, '回轉曲げを受ける球狀黑鉛鑄鐵の微小き裂發生および進展擧動,' 日本機械學會論文集 (A), 第 50 券, 第 457 號, pp. 1565-1573, 1984
  15. H. Nisitani and I. Takeo, 'Significance of Initiation, Propagation and Closure of Micro cracks in High Cycle Fatigue of Ductile Metals,' Eng. Fract. Mech., Vol. 15, No. 3-4, pp. 445-456, 1981 https://doi.org/10.1016/0013-7944(81)90070-9
  16. 土居滋, '狀黑鉛鑄鐵の疲勞破面解析と黑鉛の擧動,' 日本機械學會論文集(A), 제 60 卷, 第570號, pp. 331-336, 1994
  17. K. Tokaji, T. Ogawa, 'Fatigue LifE Distribution and Its Simulation in Spheroidal graphite cast iron,' Material Sience Research International, Vol. 2, No. 1, pp. 39-45, 1996
  18. 尹命辰, 李慶模, '구상흑연 주철재의 피로크랙발생 및 피로강도에 미치는 기지조직의 영향,' 한국공작기계학회지, 第7卷, 第5號, pp. 66-71, 1998
  19. 尹命辰, '低炭素鋼의 表面缺陷의 影響에 의한 疲勞强度의 定量的評價,' 한국공작기계기술학회지, 第 4 卷, 第 4 號, pp. 42-49, 1995
  20. Jong hyung Lee, Kyung Mo Lee, and Sung Hung Yoon, 'A study on the Fatigue Properties of Boron Steel(AISI 51B20),' Korean Society of Precision Engineering, Vol. 18, No. 11, pp. 174-178, 2001
  21. 尹命辰, '中炭素鋼의 피로크랙 開閉口의 특성 및 疲勞强度의 評價,' 한국공작기계기술학회지, 第6卷, 製1號, pp. 45-50, 1997