Adhesion Strength and Interface Chemistry with Cr, 50%Cr-50%Ni or Ni Buffer Layer in Cu/buffer Layer/polyimide System

Cu/buffer layer/polyimide 시스템에서 Cr, 50%Cr-50%Ni 및 Ni 버퍼층에 따른 접착력 및 계면화학

  • Kim, Myung-Han (Department of Materials Engineering, Chungbuk National University)
  • 김명한 (충북대학교 공과대학 신소재공학과)
  • Published : 2009.03.27

Abstract

In the microelectronics packaging industry, the adhesion strength between Cu and polyimide and the thermal stability are very important factors, as they influence the performance and reliability of the device. The three different buffer layers of Cr, 50%Cr-50%Ni, and Ni were adopted in a Cu/buffer layer/polyimide system and compared in terms of their adhesion strength and thermal stability at a temperature of $300^{\circ}C$ for 24hrs. A 90-degree peel test and XPS analysis revealed that both the peel strength and thermal stability decreased in the order of the Cr, 50%Cr-50%Ni and Ni buffer layer. The XPS analysis revealed that Cu can diffuse through the thin Ni buffer layer ($200{\AA}$), resulting in a decrease in the adhesion strength when the Cu/buffer layer/polyimide multilayer is heat-treated at a temperature of $300^{\circ}C$ for 24hrs. In contrast, Cu did not diffuse through the Cr buffer layer under the same heat-treatment conditions.

Keywords

References

  1. R. R. Tummala and E. J. Rymaszewski (eds), Microelectronics Packaging Handbook, p.673, VNR, New York (1989)
  2. B. Chapman, Glow Discharge Processes, p.201, John Wiley & Sons, New York (1980)
  3. Y. S. Lin, H. M. Liu and C. L. Chen, Surf. Coat. Techol., 200, 3773 (2006) https://doi.org/10.1016/j.surfcoat.2004.11.031
  4. A. M. Ektessabi and S. Hakamata, Thin Solid Films, 377, 621(2000) https://doi.org/10.1016/S0040-6090(00)01444-9
  5. M. H. Kim and K. W. Lee, Met. Mater.-Int. 12, 425 (2006) https://doi.org/10.1007/BF03027710
  6. M. J. Goldberg, J. G. Clabes and C. A. Kovac, Sci. Technol., A6, 991 (1988)
  7. A. K. Oultache and R. E. Prud'homme, Polym. Adv. Technol., 11, 316 (2000) https://doi.org/10.1002/1099-1581(200006)11:6<316::AID-PAT983>3.0.CO;2-S
  8. L. P. Buchwalter and K. Holloway, J. Adhes. Sci. Technol., 12(1), 95 (1998) https://doi.org/10.1163/156856198X00678
  9. K. W. Lee, H. C. Chae, C. M. Choi and M. H. Kim, Kor. J. Mater. Res., 17(2), 61 (2007) https://doi.org/10.3740/MRSK.2007.17.2.061
  10. R. Haight, R. C. White, B. D. Silverman and P. S. Ho. J. Vac. Sci. Technol., A6, 2188 (1988) https://doi.org/10.1116/1.575010
  11. J. Yu, J. Kor. Inst. Met. & Mater., 40, 518 (2002)
  12. C. M. Choi, H. C. Chae and M. H. Kim, Kor. J. Mater. Res., 17(12), 664 (2007) https://doi.org/10.3740/MRSK.2007.17.12.664