Effects of Welding Processes on the Low Temperature Impact Toughness of Structural Steel Welded Joints

용접방법에 따른 구조용강 용접 접합부의 저온 충격인성 특성

  • Received : 2012.05.02
  • Accepted : 2012.12.10
  • Published : 2012.12.27

Abstract

In this study, the Charpy impact test along with metallurgical observation was conducted to evaluate low temperature impact toughness of structural steel welds with different welding processes to find out the optimal welding process to guarantee the required impact toughness at low temperatures. The welding processes employed are shield metal arc welding (SMAW) and flux cored arc welding(FCAW), which are commonly used welding methods in construction. The Charpy impact test is a commercial quality control test for steels and other alloys used in the construction of metallic structures. The test allows the material properties for service conditions to be determined experimentally in a simple manner with a very low cost. To investigate the impact toughness at low temperatures of the steel welds, specimens were extracted from the weld metal and the heat affected zone. Standard V-notch Charpy specimens were prepared and tested under dynamic loading condition. The low temperature impact performance was evaluated based on the correlation between the absorbed energy and the microstructure. Analysis of the results showed that the optimal welding process to ensure the higher low temperature impact toughness of the HAZ and the weld metal is SMAW process using the welding consumable for steels targeted to low temperature use.

본 논문에서는 서로 다른 용접방법 및 용접재료를 사용하여 제작한 강구조물 용접부 및 열영향부에 대하여 샤르피 충격시험 (Charpy Impact Test) 및 조직검사를 통한 저온에서의 충격인성 평가를 실시하여, 극지 및 시베리아와 같은 저온환경에 노출된 강구조물 용접 접합부의 충격인성을 확보할 수 있는 용접방안에 대한 연구를 수행하였다. 사용된 용접방법은 강구조물 제작시 널리 쓰이는 SMAW (Shielded Metal Arc Welding)와 FCAW (Flux Cored Arc Welding)이며, 각 용접방법에 따른 저온강용 용접봉을 사용하여 시험판을 제작하였다. 서로 다른 용접방법으로 제작된 시험판의 용접부 및 열영향부에 대하여 샤르피 충격시험을 통한 저온에서의 충격흡수에너지 값과 미세조직 분석을 통하여 용접방법에 따른 구조용강 용접 접합부의 저온 충격인성을 평가하였다. 시험결과 극한지에 강구조물을 적용하기 위해서는 저입열 용접인 SMAW 용접방법 및 그에 따른 저온강용 용접봉을 사용하는 것이 충격인성 확보 측면에서 유리하다는 것을 알 수 있었다.

Keywords

References

  1. Eurocode 3 (2005) Design of steel structures - Part 1-10: Material toughness and throughthickness properties, CEN
  2. Bayraktar, E., Hugele, D., Jansen, J.P., and Kaplan, D. (2004) Evaluation of pipeline laser girth weld properties by Charpy (V) toughness and impact tensile tests, Journal of Materials Processing Technology, Vol. 147, pp.155-162. https://doi.org/10.1016/j.jmatprotec.2003.10.008
  3. Devillers, L., Kaplan, D., and Testard, P. (1993) An approach to predicting microstructures and toughness properties in heat affected zones of multipass welds of structural steels, Welding World, Vol. 31, pp.256-267
  4. Jang, Y.C., Hong, J.K., Park, J.H., Kim, D.W., and Lee, Y. (2008) Effects of notch position of the Charpy impact specimen on the failure behavior in heat affected zone, Journal of Materials Processing Technology, Vol. 201, pp. 419-424. https://doi.org/10.1016/j.jmatprotec.2007.11.272
  5. Kim, J.H. and Yoon, E.P. (1998) Notch position in the HAZ specimen of reactor pressure vessel steel, Journal of Nuclear Materials, Vol. 257, pp.303-308. https://doi.org/10.1016/S0022-3115(98)00451-6
  6. Moitra, A., Parameswaran, P., Sreenivasan, P. R., and Mannan, S.L. (2002) A toughness study of the weld heat-affected zone of a 9Cr-1Mo steel, Materials Characterization, Vol. 48, pp.55-61. https://doi.org/10.1016/S1044-5803(02)00247-4
  7. Tvergaard, V. and Needleman, A. (2000) Analysis of the Charpy V-notch test for welds, Engineering Fracture Mechanics, Vol. 65, pp.627-643. https://doi.org/10.1016/S0013-7944(99)00146-0
  8. 김일평, 허용, 박영석, 윤태양(2008) 도로교 설계기준 개정 소개, 대한토목학회 기술기사, 제56권, 제10호, pp.59-66. Kim, I.P., Heo, Y., Park, Y.S., and Yoon, T.Y. (2008) Introduction of bridge design specification, KSCE Technical report, Vol. 56, No. 10, pp.59-66 (in Korean).
  9. 김종락, 김상섭, 이철호, 이은택, 백기열(2008) 600MPa 급(SM570 TMC) 강재의 소재 및 용접특성에 관한 연구, 한국강구조학회 논문집, 한국강구조학회, 제20권, 제 6호, pp.773-781. Kim, J.R., Kim, S.S., Lee, C.H., Lee, E.T, and Beak, K.Y. (2008) A Study on the Material Characteristics and the Welding Properties of 600MPa Grade Steel (SM570 TMC) Journal of Korean Society of Steel Construction, Vol. 20, No. 6, pp.773-781 (in Korean)
  10. 이진형, 신현섭, 박기태, 양승현(2011) 샤르피 충격시험을 통한 구조용강재의 극한지 적용성 검토, 한국강구조학회논문집, 한국강구조학회, 제23권, 제4호, pp.483-491. Lee, C.H., Shin H.S., Park, K.T., and Yang, S.H. (2011) Evaluation of the Applicability of Structural Steels to Cold Regions by the Charpy Impact Test, Journal of Korean Society of Steel Construction, Vol. 23, No. 4, pp.483- 491 (in Korean).
  11. 김희동, 양재근, 이은택, 김우범, 오영석(2012) 400 MPa 급 건축구조용 열간압연 H형강(SHN400)의 용접특성, 한국강구조학회 논문집, 한국강구조학회, 제24권, 제1호, pp. 129-136. Kim, H.D., Yang, J.G., Lee, E.T., Kim, W.B and Oh, Y.S. (2012) Welding Characteristics of 400MPa Grade Hot Rolled H-beam (SHN400) for Building Structure, Journal of Korean Society of Steel Construction, Vol. 24, No. 1, pp.129-136 (in Korean). https://doi.org/10.7781/kjoss.2012.24.1.129
  12. Porter, D., Laukkanen, A., Nevasmaa, P., Rahka, K., and Wallin, K. (2004) Performance of TMCP steel with respect to mechanical properties after cold forming and post-forming heat treatment, International Journal of Pressure Vessels and Piping, Vol. 81, pp.867-877. https://doi.org/10.1016/j.ijpvp.2004.07.006
  13. Shin, Y.T., Kang, S.W., and Lee, H.W. (2006) Fracture characteristics of TMCP and QT steel weldments with respect to crack length, Materials Science Engineering A, Vol. 434, pp.364-371
  14. Tamehiro, H., Yamada, N., and Matsuda, H. (1985) Effect of the thermo-mechanical control process on the properties of high strength low alloy steel, ISIJ International, Vol. 25, pp.54-61. https://doi.org/10.2355/isijinternational1966.25.54
  15. Tsay, L.W., Chern, T.S., Gau, C.Y., and Yang, J.R. (1999) Microstructures and fatigue crack growth of EH36 TMCP steel weldments, International Journal of Fatigue, Vol. 21, pp.857-864. https://doi.org/10.1016/S0142-1123(99)00021-3
  16. 대한용접․접합학회(1998) 용접․접합 편람. The Korean Welding and Joining Society (1998) A handbook of Welding and Joining (in Korean).
  17. KS B 0809 (2001) Test pieces for impact test for metallic materials, Korean Standards.
  18. AKS B 0810 (2003) Method of impact test for metallic materials, Korean Standards
  19. KS B 0821 (2007) Methods of tension and impact tests for deposited metal, Korean Standards.
  20. ASME (2004) Impact testing requirements, Boiler & pressure vessel code, Sec. VIII, Div. I.
  21. Magudeeswaran, G., Balasubramanian, V., Reddy, G.M., and Balasubrarnanian, T.S. (2008) Effect of welding processes and consumables on tensile and Impact properties of high strength quenched and tempered steel joints, Journal of Iron and Steel Research International, Vol. 15, pp.87-94.
  22. Parker, J.D. and Stratford, G.C. (1999) Review of factors affecting condition assessment of nickel based transition joints, Science and Technology of Welding and Joining, Vol. 4, pp.29-39. https://doi.org/10.1179/136217199322910734
  23. Yang, J.R., Huang, C.Y., and Huang, C.F. (1993) Influence of acicular ferrite and bainite microstructures on toughness for an ultra-low-carbon alloy steel weld metal, Journal of Materials Science Letter, Vol. 12, pp.1290-1293. https://doi.org/10.1007/BF00506341

Cited by

  1. 저온영역에서의 A516-60, A283-C, A285-C, SB410 소재 특성 평가 vol.20, pp.9, 2012, https://doi.org/10.5762/kais.2019.20.9.405