DOI QR코드

DOI QR Code

The Charateristics of Melting Slag from MSWI and Sewage Water Filter Application

소각용융슬래그의 특성 및 수처리 여과재 활용에 관한 연구

  • 박상구 (인하대학교 사회기반시스템공학부 토목공학과) ;
  • 김건흥 (인하대학교 사회기반시스템공학부 토목공학과)
  • Received : 2012.03.27
  • Accepted : 2012.09.25
  • Published : 2012.11.30

Abstract

The objective of the study is to find a way to utilize MSWI slag as filter material and to verify it. To do so, stability as filter material was tested, and used Ju-Munjin filter sand as control group to run actual filtering experiment to analyze filtering efficiency. According to result, MSWI slag is usable within designated waste acceptable standards. Also, it showed similar level of filtering capability to filter sand. Thus, MSWI slag could help to save and recycle resources if used as filtering material instead of filter sand As result of filtering test, SS and COD showed about same level of filtering capability similar to standard filter sand. MSWI slag has shown 26.96% higher with T-N, and 6.55% higher with T-P compared to standard filter sand. Also, remove efficiency comparison result with No. 40#(0.43mm) and mixed diameter showed equal or greater filtering capability.

본 연구의 목적은 폐기물에서 발생되는 소각재 용융슬래그의 여과재 활용가능성을 검증하는데 있다. 이를 위하여 소각재 용융슬래그의 여과재 기능을 수행할 수 있는지 안전성 검토를 수행하고, 일반적인 여과재로 사용되는 주문진 표준사를 대조군으로 하여 실제 여과실험을 수행함으로서 그 여과능을 분석하였다. 연구결과에 따르면 용융슬래그 여과재는 중금속 용출율이 지정폐기물 허용기준 내로 사용이 가능한 수준이며, 여과 실험 결과 SS와 COD의 경우 표준여과사와 유사한 수준의 여과능을 나타내었으며, T-N, T-P의 경우는 표준여과사 보다 소각용융슬래그가 T-N은 26.96%, T-P는 6.55% 더 높은 처리율을 보였다. 또한, 소각용융슬래그의 입경에 따른 제거율 비교를 수행한 결과 No.40#(0.43mm)와 혼입경의 경우 표준여과사와 동등 또는 그 이상의 여과능을 보였다. 따라서, 용융슬래그를 여과사로 활용할 경우 주문진 표준사에 비하여 자원절약과 자원재활용의 효과를 가져 올 수 있을 것으로 판단된다.

Keywords