Properties of Shrinkage Reducing Agent and Mortar with C12A7-based Slag and Petroleum Cokes Ash

C12A7계 슬래그와 석유 코크스 연소재를 사용한 수축저감재 및 모르타르의 특성

  • Chu, Yong Sik (Energy & Environmental Division, Korea Institute of Ceramic Eng. & Tech.) ;
  • Park, Soo Hyun (Energy & Environmental Division, Korea Institute of Ceramic Eng. & Tech.) ;
  • Seo, Sung Kwan (Energy & Environmental Division, Korea Institute of Ceramic Eng. & Tech.) ;
  • Park, Jae Wan (Energy & Environmental Division, Korea Institute of Ceramic Eng. & Tech.)
  • 추용식 (한국세라믹기술원 에너지환경소재본부) ;
  • 박수현 (한국세라믹기술원 에너지환경소재본부) ;
  • 서성관 (한국세라믹기술원 에너지환경소재본부) ;
  • 박재완 (한국세라믹기술원 에너지환경소재본부)
  • Received : 2013.04.18
  • Accepted : 2013.08.20
  • Published : 2013.09.30

Abstract

In this study, petroleum cokes ash and $C_{12}A_7$-based slag were used for the shrinkage reduction and strength enhancement of mortar. The hydration properties of shrinkage reduction agents were analysed. The flow, change of length and compressive strength were experimented with mortar-added shrinkage reduction agents. As a result of this study, petroleum cokes ash : $C_{12}A_7$-based slag = 60~80% : 20~40% showed excellent results. In the case of mortar with 20% $C_{12}A_7$-based slag, the setting time and change of length were similar to Ref. mortar. The flow and compressive strength were superior to Ref. mortar. In the case of mortar with a 40% $C_{12}A_7$-based slag, the setting time was longer than Ref. mortar. The compressive strength of 3 days and 7 days were superior to Ref. mortar.

Keywords

References

  1. S. H. Alsayed and M. A. Amjad, "Effect of Curing Conditions on Strength, Orosity, Absorptivity, and Shrinkage of Concrete in Hot and Dry Climate," Cem. Concr. Res., 24 [7] 1390-98 (1994). https://doi.org/10.1016/0008-8846(94)90124-4
  2. Y. S. Son, D. H. Lee, S. H. Lee, and S. K. Kim, "Analysis of the Mechanism of Crack Stop-bar for Floor Plastering of Apartment Buildings (in Korean)," J. Kor. Inst. of Bldg. Const., 11 [4] 333-44 (2011). https://doi.org/10.5345/JKIBC.2011.11.4.333
  3. Y. H. Kwon, "A Study on the Causes and Repairs of Cracks in Concrete (in Korean)," Kor. Remicon Indust. Assoc., 73, 2-12 (2002).
  4. J. M. Kim, "A Study on the Causes and Repairs of Cracks in Concrete (in Korean)," Kor. Remicon Indust. Assoc., 16-25 (1997).
  5. C. H. Jung and B. H. Lee, "A Quality Research as Proportion of Subslab Concrete (in Korean)," J. Kor. Inst. of Bldg. Const., 9 [2] 308 (2009).
  6. M. C. Han, "Estimation of the Autogenous Shrinkage of the High Performance Concrete Containing Expansive Additive and Shrinkage Reducing Agent (in Korean)," J. Kor. Inst. of Bldg. Const., 7 [3] 123-30 (2007). https://doi.org/10.5345/JKIC.2007.7.3.123
  7. S. A. Kwon, "Crack Retardant Mixture for Cement Mortar and Cementmortar by Using it for Heating Floor (on-dool) (in Korean)," Kor. Unexamined Pat. Publication, 10-0303235-0000 (2000).
  8. A. Boumiz, C. Vernet, and F. C. Tenoudji, "Mechanical Properties of Cement Pastes and Mortars at Rarly Ages: Evolution with Time and Degree of Hydration," Adv. Cem. Based Mater., 3 [3] 94-106 (1996).
  9. A. J. Majumdar, B. Singh, and R. N. Edmonds, "Hydration of Mixture of $C_{12}A_7$ and Granulated Blast Furnace Slag," Cem. Concr. Res., 19, 848-56 (1989). https://doi.org/10.1016/0008-8846(89)90097-5
  10. F. M. Lea and P. C. Hewlett, "Lea's Chemistry of Cement and Concrete," 4th Ed., pp. 723-27, Butterworth-Heinemann, U. S., 2010.
  11. H. K. Park, "Wet Shotcrete Method Using Casting Equipment, Consisting of a Composite Grade Billing and Cement-based Water-cooled Amorphous $C_{12}A_7$ Mineral Kingdom of the Air Injection System," Samsung development Co. Inst. of Tech., 50-62 (2004).

Cited by

  1. Up-cycling of Air-cooled Ladle Furnace Slag : Environmental Risk Assessment and Mortar Compressive Strength Assesment of Binary and Ternary Blended Cement Using Air-cooled Ladle Furnace Slag vol.37, pp.3, 2015, https://doi.org/10.4491/KSEE.2015.37.3.159