자동차용 강판의 접착특성 - 접착부위 접합 강도와 영향인자 - (Characteristics of Adhesive bonded Joints of Steels for Automobile(I))

  • 윤병현;권영각
    • Journal of Welding and Joining
    • /
    • 제13권2호
    • /
    • pp.106-114
    • /
    • 1995
  • The characteristics of adhesive bonded joint of steels for automobile were investigated. Shear and tear strength were tested and analyzed for the joints of cold rolled steel sheets bonded with three kinds of epoxy and urethane based adhesive. The results showed that the tensile shear strength and the tear strength of adhesive joint were affected by the shape of adhesive joint such as the length and width of adhesive joint. The thickness of adhesive layer was very important factor affecting the bonding strength. The shear strength increased with decrease of the thickness of adhesive layer, while the tear strength decreased as the thickness of adhesive layer decreased. In comparison with the strength of spot welded joint, the shear strength of adhesive Joint was higher than that of spot welded joint, but the tear strength of adhesive Joint was lower than that of spot welded joint.

  • PDF

접착이음의 계면덧살에 대한 응력특이성 해석 (Analysis of Stress Singularity for the Excess Adhesive of Interface in Adhesively Bonded Joint)

  • 정남용;박철희
    • 한국생산제조학회지
    • /
    • 제21권3호
    • /
    • pp.439-445
    • /
    • 2012
  • The stress singularity for the excess adhesive on interface of adhesively bonded joint was investigated by using the 2-dimensional elastic boundary element method (BEM). To establish a reasonable strength evaluation method and a fracture criterion for the excess adhesive of interface in adhesively bonded joint, it is necessary to evaluate fracture parameters with various bonding conditions. Under the variations of adhesively bonded thickness (h) and diameter (d) for the excess adhesive, a stress analysis was performed, and from the results, the stress singularity index (${\lambda}$) and the stress singularity factor (${\Gamma}$) were calculated. The variations have a great influences on the stress singularity for the excess adhesive of interface in adhesively bonded joint, and the ${\Gamma}$ is reduced as the "h" and "d" increase.

T형 이음 접합에 의한 경량구조물용 접착이음강도의 평가 (Strength Evaluation of Adhesive Bonded Joint for Light Weight Structure by T-Peel Joint Test)

  • 이강용;공병석;우형표
    • 한국자동차공학회논문집
    • /
    • 제6권4호
    • /
    • pp.56-65
    • /
    • 1998
  • The bonding strength evaluation of the light weight materials for an electrical vehicle has been performed through the T-peel joint test in which the design paramete- rs such as joint style, adherend type, adherend thickness, adhesive thickness, and adhesive type are considered. It is experimentally observed that the peel strength of joint increases with the increase of the adherend thickness. With the increase of the adhesive thickness, however, the peel strength of joint increases a little. Aluminum-FRP adherend combination shows such higher peel strength than that of Aluminum-Aluminum adherend combination. For the adhesive bonded joint, the results of FEM analysis agree with those of experiment. The adhesive bonded joint reinfored with a rivet gives higher peel strength than that of the joint without rivet.

  • PDF

Non-tubular bonded joint under torsion: Theory and numerical validation

  • Pugno, Nicola;Surace, Giuseppe
    • Structural Engineering and Mechanics
    • /
    • 제10권2호
    • /
    • pp.125-138
    • /
    • 2000
  • The paper analyzes the problem of torsion in an adhesive non-tubular bonded single-lap joint. The joint considered consists of two thin rectangular section beams bonded together along a side surface. Assuming the materials involved to be governed by linear elastic laws, equilibrium and compatibility equations were used to arrive at an integro-differential relation whose solution makes it possible to determine torsional moment section by section in the bonded joint between the two beams. This is then used to determine the predominant stress and strain field at the beam-adhesive interface (stress field along the direction perpendicular to the interface plane, equivalent to the applied torsional moment and the corresponding strain field) and the joint's elastic strain (absolute and relative rotations of the bonded beam cross sections). All the relations presented were obtained in closed form. Results obtained theoretically are compared with those given by a three dimensional finite element numerical model. Theoretical and numerical analysis agree satisfactorily.

이종재료 접착제 접합부의 환경 피로강도 평가 (Evaluation of Environmental Fatigue Strength in Adhesive Bonding of Different Materials)

  • 임재규;이중삼;윤호철;유성철
    • Journal of Welding and Joining
    • /
    • 제20권5호
    • /
    • pp.99-105
    • /
    • 2002
  • One of the important advantage of adhesive bonded joint can combine the different materials. The joint that bonded by structural adhesive bond must keep a large force and its strength is affected by some environmental factors such as temperature and submergence time in water. In order to advance the fatigue strength of adhesive bonded joint, mostly put a surface treatment on the surface. This study was researched the effect of air temperature, submergence time, submergence temperature and surface treatment on the fatigue strength. We found that submergence temperature has the most effect and low plasma treatment specimens have the most fatigue strength.

Numerical analysis of the combined aging and fillet effect of the adhesive on the mechanical behavior of a single lap joint of type Aluminum/Aluminum

  • Medjdoub, S.M.;Madani, K.;Rezgani, L.;Mallarino, S.;Touzain, S.;Campilho, R.D.S.G.
    • Structural Engineering and Mechanics
    • /
    • 제83권5호
    • /
    • pp.693-707
    • /
    • 2022
  • Bonded joints have proven their performance against conventional joining processes such as welding, riveting and bolting. The single-lap joint is the most widely used to characterize adhesive joints in tensile-shear loadings. However, the high stress concentrations in the adhesive joint due to the non-linearity of the applied loads generate a bending moment in the joint, resulting in high stresses at the adhesive edges. Geometric optimization of the bonded joint to reduce this high stress concentration prompted various researchers to perform geometric modifications of the adhesive and adherends at their free edges. Modifying both edges of the adhesive (spew) and the adherends (bevel) has proven to be an effective solution to reduce stresses at both edges and improve stress transfer at the inner part of the adhesive layer. The majority of research aimed at improving the geometry of the plate and adhesive edges has not considered the effect of temperature and water absorption in evaluating the strength of the joint. The objective of this work is to analyze, by the finite element method, the stress distribution in an adhesive joint between two 2024-T3 aluminum plates. The effects of the adhesive fillet and adherend bevel on the bonded joint stresses were taken into account. On the other hand, degradation of the mechanical properties of the adhesive following its exposure to moisture and temperature was found. The results clearly showed that the modification of the edges of the adhesive and of the bonding agent have an important role in the durability of the bond. Although the modification of the adhesive and bonding edges significantly improves the joint strength, the simultaneous exposure of the joint to temperature and moisture generates high stress concentrations in the adhesive joint that, in most cases, can easily reach the failure point of the material even at low applied stresses.

접착제 접합된 자연섬유강화 복합재료의 파괴강도 특성에 미치는 접착제 필릿의 영향 (Effect of Spew Fillet on Failure Strength Properties of Natural Fiber Reinforced Composites Including Adhesive Bonded Joints)

  • 윤호철;최준용;김연직;임재규
    • Journal of Welding and Joining
    • /
    • 제23권6호
    • /
    • pp.67-71
    • /
    • 2005
  • This paper is concerned with a study on fracture strength of composites in an adhesive single lap joint. The tests were carried out on joint specimens made with hybrid stacked composites consisting of the polyester and bamboo natural fiber layer. The main objective of this work was to evaluate the fracture properties adjacent to adhesive bonded joint of natural fiber reinforced composite specimens. From the results, natural fiber reinforced composites have lower tensile strength than the original polyester. But tensile-shear strength of natural fiber reinforced composites with bamboo layer far from adhesive bond is as high as that of the original polyester adhesive bonded joints. Spew filet at the end of the overlap reduced the stress concentration at the bonded area. Spew fillet and position of bamboo natural fiber layer have a peat effect on the tensile-shear strength of natural fiber reinforced composites including adhesive bonded joints.

튜브형 단면겹치기 접착조인트의 비선형 반복연산해에 관한 연구 (Nonlinear Iterative Solution for Adhesively Bonded Tubular Single Lap Joints with Nonlinear Shear Properties)

  • 이수정;이대길
    • 대한기계학회논문집
    • /
    • 제19권7호
    • /
    • pp.1651-1656
    • /
    • 1995
  • The adhesively bonded tubular single lap joint shows large nonlinear behavior in the loaddisplacement relation, because structural adhesives for the joint are usually rubber toughened, which endows adhesives with nonlinear shear properties. since the majority of load transfer of the adhesively bonded tubular single lap joint is accomplished by the nonlinear behavior of the adhesive, its torque transmission capability should be calculated incorporating nonlinear shear properties. However, both the analytic and numerical analyses become complicated if the nonlinear shear properties of the adhesive are included during the calculation of torque transmission capabilities. In this paper, in order to obtain the torque transmission capabilities easily, an iterative solution which includes the nonlinear shear properties of the adhesive was derived using the analytic solution with the linear shear properties of the adhesive. Since the iterative solution can be obtained very fast due to its simplicity, it has been found that it can be used in the design of the adhesively bonded tubular single lap joint.

압전특성을 이용한 접착 조인트의 안전성 모니터링 (Reliability Monitoring of Adhesive Joints by Piezoelectricity)

  • 권재욱;진우석;이대길
    • 대한기계학회논문집A
    • /
    • 제27권8호
    • /
    • pp.1388-1397
    • /
    • 2003
  • Since the reliability of adhesively bonded joints for composite structures is dependent on many parameters such as the shape and dimensions of joints, type of applied load, and environment, so an accurate estimation of the fatigue life of adhesively bonded joints is seldom possible, which necessitates an in-situ reliability monitoring of the joints during the operation of structures. In this study, a self-sensor method for adhesively bonded joints was devised, in which the adhesive used works as a piezoelectric material to send changing signals depending on the integrity of the joint. From the investigation, it was found that the electric charge increased gradually as cracks initiated and propagated in the adhesive layer, and had its maximum value when the adhesively bonded joint failed. So it is feasible to monitor the integrity of the joint during its lifetime. Finally, a relationship between the piezoelectric property of the adhesive and crack propagation was obtained from the experimental results.

일방향 복합재료 Single Lap접합 조인트의 파손 모드 및 강도 I. 실험 (Failure Mode and Strength of Unidirectional Composite Single Lap Bonded Joints I. Experiments)

  • 김광수;유재석;안재모;장영순
    • Composites Research
    • /
    • 제17권6호
    • /
    • pp.14-21
    • /
    • 2004
  • 본 연구에서는 몇 가지 접합 방법에 따라 일방향 복합재료 단일 겹치기 접합 조인트의 파손 과정, 모드 및 강도를 실험적으로 평가하였다 접합 방법으로는 접착제 없는 동시성형, 접착제를 사용한 동시성형 및 이차 접합의 세 가지를 고려하였다 또한 이차 접합 조인트에서 몇 가지 파라미터의 영향도 살펴보았다. 접착제 없는 동시성형 시편은 가장 우수한 조인트 강도를 나타내었다. 이차접합 조인트에서는 접착제 층의 점진적인 파손이 발생하였다. 접착제의 재료 및 접합 강도가 상대적으로 강한 필름 접착제의 동시성형 조인트는 갑작스런 층간분리 파손이 발생하였으며 이차 접합 조인트보다 더 낮은 파손 강도를 나타내었다. 이차 집합 조인트에서 층간분리 파손이 발생하지 않은 것은 접착제 층에서의 균열 진전 및 점진적 파손이 층간분리 파손을 방지한 것으로 보인다. 따라서 복합재료 접합 조인트의 파손 강도는 접착제의 재료 강도 또는 접착 성능과 항상 비례하지 않으며 이것은 복합재료가 층간 분리 파손에 약하기 때문이다.