• 제목/요약/키워드: Anode Oxidation

검색결과 218건 처리시간 0.024초

Electrochemical treatment of cefalexin with Sb-doped SnO2 anode: Anode characterization and parameter effects

  • Ayse, Kurt;Hande, Helvacıoglu;Taner, Yonar
    • Advances in nano research
    • /
    • 제13권6호
    • /
    • pp.513-525
    • /
    • 2022
  • In this study, it was aimed to evaluate direct oxidation of aqueous solution containing cefalexin antibiotic with new generation Sn/Sb/Ni: 500/8/1 anode. The fact that there is no such a study on treatment of cefalexin with these new anode made this study unique. According to the operating parameters evaluation COD graphs showed clearer results compared to TOC and CLX and thus, it was it was chosen as major parameter. Furthermore, pseudo-first degree kd values were calculated from CLX results to show more accurate and specific results. Experimental results showed that after 60 min of electrochemical oxidation, complete removal of COD and TOC was accomplished with 750 mg L-1 KCl, at pH 7, 50 mA cm-2 current density and 1 cm anode-cathode distance. Also, the stability of the Sn/Sb/Ni anode was evaluated by taking SEM and AFM images and XRD analysis before and after of electrochemical oxidation processes. According to the results, it was not occurred too much change on the anode surface even after 300 h of electrolysis. Thus, it was thought that the anode material was not corroded to a large extent. Furthermore, the removal efficiencies were very high for almost all the time and conditions. According to the results of the study, electrochemical oxidation with new generation Sn/Sb/Ni anodes for the removal of cefalexin antibiotic was found very successful and applicable due to require less reaction time complete mineralization and doesn't require pH adjustment step compared to other studies in literature. In future studies, different antibiotic types should be studied with this anode and maybe with real wastewaters to test applicability of the process in treatment of pharmaceutical wastewaters containing antibiotics, in a better way.

Cyclitol 유도체 합성에 관한 연구 (제3보)-myo-Inositol의 전해 산화- (Synthesis of Cyclitol Derivatives (Ⅲ). Electrolytic Oxidation of myo-Inositol)

  • 손주환;남종우;김유옥
    • 대한화학회지
    • /
    • 제15권3호
    • /
    • pp.127-132
    • /
    • 1971
  • To obtain the various kinds of inosose stereomers, the process of electrochemical oxidation is more effective than chemical oxidation of myo-inositol. So that myo-inositol aqueous solution was electrolyzed by platinum and lead peroxide anode to confirming the occurrence of electrochemical oxidation. The result is that myo-inosose-2 is producing with high yield comparatively by electrolytic oxidation of myo-inositol. Also we studied about the relation between the electrolytic current efficiency and electrolytic temperature and anodic current density. The current efficiency is rising with lowering of electrolytic temperature identically in both anode such as platinum and lead peroxide and also rising with increasing of anodic current density in platinum anode, but inversely in lead peroxide.

  • PDF

알루미늄 실리콘 나노분말을 이용한 리튬이온전지 음극재료에 관한 연구 (The Research on Aluminum and Silcon Nanoparticles as Anode Materials for Lithium Ion Batteries)

  • 김형조;;김형진;박원조
    • 동력기계공학회지
    • /
    • 제17권1호
    • /
    • pp.110-115
    • /
    • 2013
  • The electrochemical performance and microstructure of Al-Si, Al-Si/C was investigated as anode for lithium ion battery. The Al-Si nano composite with 5 : 1 at% ratio was prepared by arc-discharge nano powder process. However, some of problem is occurred, when Al nano composite was synthesized by this manufacturing. The oxidation film is generated around Al-Si particles for passivating processing in the manufacture. The oxidation film interrupts electrical chemistry reaction during lithium ion insertion/extraction for charge and discharge. Because of the existence the oxidation film, Al-Si first cycle capacity is very lower than other examples. Therefore, carbon synthsized by glucose ($C_6H_{12}O_6$) was conducted to remove the oxidation film covered on the composite. The results showed that the first discharge cycle capacity of Al-Si/C is improved to 113mAh/g comparing with Al-Si (18.6mAh/g). Furthermore, XRD data and TEM images indicate that $Al_4C_3$ crystalline exist in Al-Si/C composite. In addition the Si-Al anode material, in which silicon is more contained was tested by same method as above, it was investigated to check the anode capacity and morphology properties in accordance with changing content of silicon, Si-Al anode has much higher initial discharge capacity(about 500mAh/g) than anode materials based on Aluminum as well as the morphology properties is also very different with the anode based Aluminum.

Ni의 산화가 고체산화물 연료전지용 Ni/YSZ 연료극의 미세조직과 전해질의 균열에 미치는 영향 (Effect of Oxidation of Ni on the Microstructure of Ni/YSZ Anode and Crack Formation in YSZ Electrolyte Layer for SOFC)

  • 임준실;최종훈;권오종
    • 한국세라믹학회지
    • /
    • 제43권12호
    • /
    • pp.805-811
    • /
    • 2006
  • The microstructural changes in Ni/YSZ anode substrate and crack formation during Ni oxidation were investigated. The composition of as-sintered anodes was 56 wt% NiO+44 wt% YSZ and that of electrolyte was 8 mol% yttria. After complete reduction, specimens were oxidized in $N_2$ + air at $600\sim800^{\circ}C$. Oxygen partial pressure was controlled in between 0.05 atm and 0.2 atm $O_2$. When the anode was oxidized, at higher than $690^{\circ}C$, three layers were formed in the specimens. The first was fully oxidized layer(NiO/YSZ), the second was a mixed layer and the third, near-intact layer. Under $640^{\circ}C$ such distinctive layers were not observed. Cracks formed at electrolyte layer when weight gain attained at $65\sim75%$ of the total gain due to complete oxidation despite of different oxidation temperature and oxygen partial pressure.

고체 산화물 연료전지 음극에서 개질 가스의 경쟁적 전기화학 반응 (Competitive electrochemical oxidation of reformate gas in SOFCs)

  • 김용민;배중면;배규종;김정현;이창보
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2008년도 춘계학술대회 논문집
    • /
    • pp.5-8
    • /
    • 2008
  • SOFC (Solid oxide fuel cell) has an advantage in the term of fuel flexibility, comparing with other kinds of fuel cells. In SOFC and fuel reformer cooperation system, the reformate gas with the various $H_2$/CO ratios is delivered into the anode of SOFC. In this situation, electrochemical oxidation reactions of the reformate gas in the anode are complex and competitive. In this paper, the effects of the composition of $H_2$ and CO on the overall electrochemical oxidation at Ni-YSZ anode are studied by testing the open circuit voltage (OCV) and current-voltage characteristics of single cells.

  • PDF

Electrochemical oxidation of sodium dodecylbenzenesulfonate in Pt anodes with Y2O3 particles

  • Jung-Hoon Choi;Byeonggwan Lee;Ki-Rak Lee;Hyun Woo Kang;Hyeon Jin Eom;Seong-Sik Shin;Ga-Yeong Kim;Geun-Il Park;Hwan-Seo Park
    • Nuclear Engineering and Technology
    • /
    • 제54권12호
    • /
    • pp.4441-4448
    • /
    • 2022
  • The electrochemical oxidation process has been widely studied in the field of wastewater treatment for the decomposition of organic materials through oxidation using ·OH generated on the anode. Pt anode electrodes with high durability and long-term operability have a low oxygen evolution potential, making them unsuitable for electrochemical oxidation processes. Therefore, to apply Pt electrodes that are suitable for long-term operation and large-scale processes, it is necessary to develop a new method for improving the decomposition rate of organic materials. This study introduces a method to improve the decomposition rate of organic materials when using a Pt anode electrode in the electrochemical oxidation process for the treatment of organic decontamination liquid waste. Electrochemical decomposition tests were performed using sodium dodecylbenzenesulfonate (SDBS) as a representative organic material and a Pt mesh as the anode electrode. Y2O3 particles were introduced into the electrolytic cell to improve the decomposition rate. The decomposition rate significantly improved from 21% to 99%, and the current efficiency also improved. These results can be applied to the electrochemical oxidation process without additional system modification to enhance the decomposition rate and current efficiency.

Electrochemical Advanced Oxidation of Lamotrigine at Ti/DSA (Ta2O5-Ir2O5) and Stainless Steel Anodes

  • Meena, Vinod Kumar;Ghatak, Himadri Roy
    • Journal of Electrochemical Science and Technology
    • /
    • 제13권2호
    • /
    • pp.292-307
    • /
    • 2022
  • The study presents kinetics of degradation and mineralization of an anti-epileptic drug Lamotrigine (LAM) in the aqueous matrix by electrochemical advanced oxidation process (EAOP) on Ti/DSA (Ta2O5-Ir2O5) and Stainless Steel (SS) anodes using sodium sulphate as supporting electrolyte. On both the anodes, kinetic behaviour was pseudo-first-order for degradation as well as mineralization of LAM. On Ti/DSA anode, maximum LAM degradation of 75.42% was observed at an associated specific charge of 3.1 (Ah/litre) at a current density of 1.38 mA/cm2 and 100 ppm Na2SO4 concentration. Maximum mineralization attained was 44.83% at an associated specific charge of 3.1 (Ah/litre) at a current density of 1.38 mA/cm2 and 50 ppm concentration of Na2SO4 with energy consumption of 2942.71 kWh/kgTOC. Under identical conditions on SS anode, a maximum of 98.92% LAM degradation was marked after a specific charge (Q) of 3.1 (Ah/litre) at a current density of 1.38 mA/cm2 and 100 ppm concentration of Na2SO4. Maximum LAM mineralization on SS anode was 98.53%, marked at a specific charge of 3.1 (Ah/litre) at a current density of 1.38 mA/cm2 and 75 ppm concentration of Na2SO4, with energy consumption of 1312.17 kWh/kgTOC. Higher Mineralization Current Efficiency (MCE) values were attained for EAOP on SS anode for both degradation and mineralization due to occurrence of combined electro-oxidation and electro-coagulation process in comparison to EAOP on Ti/DSA anode due to occurrence of lone electro-oxidation process.

Pd 나노입자의 자가 회복이 가능한 지능형 페로브스카이트 산화물 음극의 직접 탄화수소계 SOFC 성능 평가 (Self-Regeneration of Intelligent Perovskite Oxide Anode for Direct Hydrocarbon-Type SOFC by Nano Metal Particles of Pd Segregated)

  • 오미영;;신태호
    • 한국전기전자재료학회논문지
    • /
    • 제31권5호
    • /
    • pp.345-350
    • /
    • 2018
  • Nanomaterials have considerable potential to solve several key challenges in various electrochemical devices, such as fuel cells. However, the use of nanoparticles in high-temperature devices like solid-oxide fuel cells (SOFCs) is considered problematic because the nanostructured surface typically prepared by deposition techniques may easily coarsen and thus deactivate, especially when used in high-temperature redox conditions. Herein we report the synthesis of a self-regenerated Pd metal nanoparticle on the perovskite oxide anode surface for SOFCs that exhibit self-recovery from their degradation in redox cycle and $CH_4$ fuel running. Using Pd-doped perovskite, $La(Sr)Fe(Mn,Pd)O_3$, as an anode, fairly high maximum power densities of 0.5 and $0.2cm^{-2}$ were achieved at 1,073 K in $H_2$ and $CH_4$ respectively, despite using thick electrolyte support-type cell. Long-term stability was also examined in $CH_4$ and the redox cycle, when the anode is exposed to air. The cell with Pd-doped perovskite anode had high tolerance against re-oxidation and recovered the behavior of anodic performance from catalytic degradation. This recovery of power density can be explained by the surface segregation of Pd nanoparticles, which are self-recovered via re-oxidation and reduction. In addition, self-recovery of the anode by oxidation treatment was confirmed by X-ray diffraction (XRD) and scanning electron microscopy (SEM).

환경친화적인 실리콘 웨이퍼 세정 연구 (A Study on environmental-friendly Cleaning for Si-wafers)

  • 윤호섭;류근걸
    • 청정기술
    • /
    • 제6권1호
    • /
    • pp.79-84
    • /
    • 2000
  • 반도체 세정공정에서 사용되는 화학약품의 소모량을 줄이기 위하여 소량의 전해질 혹은 초순수만을 전기분해 시켜 생성되는 전리수를 이용하여 금속 불순물들이 오염된 실리콘 웨이퍼를 습식세정을 하였다. 전리수는 다양한 범위의 pH 및 산화환원전위(oxidation-reduction potential, ORP)를 형성할 수 있으며, 전리수의 양극수는 pH 및 산화환원전위를 각각 4.7 및 +1000mV의 산화성 수용액을, 전리수의 음극수는 pH 및 산화환원전위가 각각 6.3 및 -550mV를 40분 이상 유지하고 있었다. 실리콘 웨이퍼 세정 전과 후의 금속 불순물 측정은 ICP-MS(Inductively coupled plasma spectroscopy)를 사용하였다. 전리수 가운데 양극수는 구리 불순물 제거에, 음극수는 철 불순물 제거에 효과적임을 확인하였다.

  • PDF

Effect of Electrochemical Oxidation Potential on Biofilter for Bacteriological Oxidation of VOCs to $CO_2$

  • Kang Hye-Sun;Lee Jong-Kwang;Kim Moo-Hoon;Park Doo-Hyun
    • Journal of Microbiology and Biotechnology
    • /
    • 제16권3호
    • /
    • pp.399-407
    • /
    • 2006
  • In this study, an electrical conductive carbon fiber was used as a biofilter matrix to electrochemically improve the biofilter function. A bioreactor system was composed of carbon fiber (anode), titanium ring, porcelain ring, inorganic nutrient reservoir, and VOC reservoir. Electric DC power of 1.5 volt was charged to the carbon fiber anode (CFA) to induce the electrochemical oxidation potential on the biofilter matrix, but not to the carbon fiber (CF). We tested the effects of electrochemical oxidation potential charged to the CFA on the biofilm structure, the bacterial growth, and the activity for metabolic oxidation of VOCs to $CO_2$, According to the SEM image, the biofilm structure developed in the CFA appeared to be greatly different from that in the CF. The bacterial growth, VOCs degradation, and metabolic oxidation of VOCs to $CO_2$ in the CFA were more activated than those in the CF. On the basis of these results, we propose that the biofilm structure can be improved, and the bacterial growth and the bacterial oxidation activity of VOCs can be activated by the electrochemical oxidation potential charged to a biofilter matrix.