A Study on the Surfaces Modification of Tool Steel by YAG LASER (YAG LASER에 의한공구강의 표면개질에 관한 연구)

  • 강형식
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.2
    • /
    • pp.66-71
    • /
    • 2000
  • Laser induced surface hardening of Tool steel(STC5) can be achieved either with or without surface melting. In trans-formation hardening as the surface is heated to a temperature below its melting point and is rapidly cooled solidified microstructures are usually much finer and stronger than those of the base matals. For this reason surface modification of tool steel by YAG laser irradiation has been studied as a function of processing parameters such as power density pulse width defocusing distance and molten depth. The high energy density changes and refines the microstructure of the near surface layer. In the case of beam passes martensite formed in the melt zone exhibited very high vickers hardness values. Molten depth and width depend on defocusing distance and energy of black color painting is more absorptive than other color painting.

  • PDF

Laser hardening and Wear Characteristics of Surfaces hardening steel by YAG LASER (′YAG 레이저에 의한 표면경화강의 레이저 경화와 마멸특성)

  • 옥철호;서영백;조연상;배효준;박흥식;전태옥
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1999.11a
    • /
    • pp.63-70
    • /
    • 1999
  • Surface hardening of plain carbon steel (SM45C) by Laser are usually much finer and stronger than those of the base metals. The present study was under taken to investigate the wear resistance and a processing parameters such as, power density, pulse width, defocusing distance, and molten depth for surface modification of plain carbon steel. The wear test was carried out under experimental condition using the wear test device, and in which the annular surfaces of wear test specimens as well as mating specimen of alumina ceramics($Al_2O_3$) was rubbed in dry sliding condition. It is shown that molten depth and width depend on defocusing distance. The wear loss on variation of sliding speed was much in lower speed range below 0.2m/sec and in higher speed range above 0.7m/sec, but wear loss was little in intermediate speed range. It depends on oxidation speed and wear speed.

  • PDF

A Study on the Surfaces Modification of Tool Steel by YAG LASER (YAG LASER에 의한 공구강의 표면개질에 관한 연구)

  • 옥철호;강형식;이광영;박홍식;전태옥
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 1998.04a
    • /
    • pp.292-299
    • /
    • 1998
  • Case hardening behavior of tool steel(SK5) was investigated after YAG laser irradiation. In the case of beam passes, martensite formed in the melt zone and in former pearlite regions of the austenization zone exhibited very high Vickers Hardness values. The molten depth and radius, micro structure, hardness were investigated as a function of defocusing distance, pulse width, and power density.

  • PDF

Improved 3D Resolution Analysis of N-Ocular Imaging Systems with the Defocusing Effect of an Imaging Lens

  • Lee, Min-Chul;Inoue, Kotaro;Cho, Myungjin
    • Journal of information and communication convergence engineering
    • /
    • v.13 no.4
    • /
    • pp.270-274
    • /
    • 2015
  • In this paper, we propose an improved framework to analyze an N-ocular imaging system under fixed constrained resources such as the number of image sensors, the pixel size of image sensors, the distance between adjacent image sensors, the focal length of image sensors, and field of view of image sensors. This proposed framework takes into consideration, for the first time, the defocusing effect of the imaging lenses according to the object distance. Based on the proposed framework, the N-ocular imaging system such as integral imaging is analyzed in terms of depth resolution using two-point-source resolution analysis. By taking into consideration the defocusing effect of the imaging lenses using ray projection model, it is shown that an improved depth resolution can be obtained near the central depth plane as the number of cameras increases. To validate the proposed framework, Monte Carlo simulations are carried out and the results are analyzed.

LASER WELDING OF TI-NI SHAPE MEMORY ALLOY WIRE

  • Kim, Young-Sik;Kim, Jong-Do
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.139-144
    • /
    • 2002
  • Ti-50.9at%Ni wires were welded using pulsed YAG laser. The laser welded wires were tested for investigating the shape memo교 effect and the ability of super elasticity. The fatigue properties of the welded wires were investigated using the rotary bending fatigue tester specially designed for wires. Moreover, the effect of defocusing distance during laser welding on the static and fatigue properties was investigated. The shape memory effect and super elasticity of the laser welded wires were approximately identical with that of base metal at the test temperature below 353K. However, the welded wires were broken within elastic limit at the test temperature above 353k. Under the cyclic bending loading conditions, the welded wires could be useful only below the elastic limit, while the base metal had sufficient fatigue life even the stress induced M-phase region. The fatigue strength of the welded wires was about half of that of the base metal. The deterioration of the static and fatigue properties in the welded wires was proven to be from the large difference of the transformation behavior between the base metal and welded part that is caused by vaporization of Ni-content at the welded part during the welding process. The defocusing distance below 3mm acted more largely on lowering the strength of the welded wires than that of 6mm or 8mm.

  • PDF

Defocusing image generation corresponding to focusing plane by using spatial information of 3D objects (3차원 물체의 공간정보를 이용한 임의의 집속면에 대응하는 디포커싱 영상 구현)

  • Jang, Jae-Young;Kim, Young-Il;Shin, Donghak;Lee, Byung-Gook;Lee, Joon-Jae
    • Journal of the Korea Institute of Information and Communication Engineering
    • /
    • v.17 no.4
    • /
    • pp.981-988
    • /
    • 2013
  • In this paper, we propose a method to generate defocusing images at the focusing plane using the 3D spatial information of object through pickup process of integral imaging technique. In the proposed method, the focusing and defocusing images are generated by the convolution operation between elemental images and ${\delta}$ function array. We observed the image difference by defocusing degree according to the distance of focusing plane. To show the feasibility of the proposed method, some preliminary experiments are carried out and the results are presented.

Wear Behavior of Laser Modified SM45C Steel (레이저 표면개질된 SM45C강의 마멸거동)

  • 배춘익;옥철호;박흥식;전태옥
    • Tribology and Lubricants
    • /
    • v.16 no.1
    • /
    • pp.15-21
    • /
    • 2000
  • Radiation of Nd-YAG laser changes and refines the surface microstructure of steels, which gives rise to enhancement of hardness and resulting wear resistance. In the present work, the effect of processing parameters during the surface modification with laser on the wear behavior of the SM45C steel was studied by means of wear testing. The counter material was alumina ceramics. The microstructure observation revealed the dependence of molten depth and width on the defocusing distance. The laser modification of steel surface give rise to improved wear resistance in the testing speed range of either <0.2 m/s or >0.9 m/s Material transfer from steel was wear observated the surface of counter material when testing speed was lower than 0.7 m/s.

A Study on the Wear Resistance and Modification Condition for Laser Surface Modified Steel (레이저 표면개질강의 개질조건과 마멸저항에 관한 연구)

  • 옥철호
    • Proceedings of the Korean Society of Machine Tool Engineers Conference
    • /
    • 1999.10a
    • /
    • pp.332-338
    • /
    • 1999
  • Surface hardening of plain carbon steel (SM$%C) by Laser are usually much finer and stronger than those of the base metals. The present study was undertaken to investigate the wear resistance and a processing parameters such as, power density, pulse width, defocusing distance, and molten depth for surface modification of plain carbon steel. The wear test was carried out under experimental condition using the wear test device, and in which the annular surfaces of wear test specimens as well as mating specimen of alumina ceramics(Al2O3) was rubbed in dry sliding condition. It is shown that molten depth and width depend on defocusing distance. The wear loss on variation of sliding speed was much in lower speed range below 0.2m/sec and in higher speed range above 0.7m/sec, but wear loss was little in intermediate speed range. It depends on oxidation speed and wear speed.

  • PDF

Fatigue Properties of Ti-Ni Shape Memory Alloy Wire Welded by Nd: YAG Laser

  • Kim, Y.S.;Kim, J.D.;Kil, B.L.
    • International Journal of Korean Welding Society
    • /
    • v.3 no.1
    • /
    • pp.39-44
    • /
    • 2003
  • The welded specimens were made by butt welding of the 2 wires of 50mm length using the pulsed YAG laser. The laser welded wires were tested for investigating the shape memory effect and the ability of super elasticity. The fatigue properties of the welded wires were investigated using the rotary bending fatigue tester specially designed for wires. Moreover, the effect of defocusing distance during laser welding on the static and fatigue properties was Investigated. The shape memory effect and super elasticity of the laser welded wires were approximately identical with that of base metal at the test temperature below 353K. However, the welded wires were broken within elastic limit at the test temperature above 353k. Under the cyclic bending loading conditions, the welded wires could be useful only below the elastic limit, while the base metal had sufficient fatigue life even the stress induced M-phase region. The fatigue strength of the welded wires was about half of that of the base metal. The deterioration of the static and fatigue properties in the welded wires was proven to be from the large difference of the transformation behavior between the base metal and welded part that is caused by vaporization of Ni-content at the welded part during the welding process. The defocusing distance below 3mm acted more largely on lowering the strength of the welded wires than that of 6mm or 8mm.

  • PDF

카메라 디포커싱을 이용한 로보트의 시각 서보

  • 신진우;고국현;조형석
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1994.10a
    • /
    • pp.559-564
    • /
    • 1994
  • Recently, a visual servoing for an eye-in-hand robot has become an interesting problem. A distance between a camera and a task object is very useful information for visual servoing. In the previous works for visual servoing, the distance can be obtained from the difference between a reference and a measured feature value of the object such as area on image plane. However, since this feature depends on the object, the reference feature value must be changed when other task object is taken. To overcome this difficulty, this paper presents a novel method for visual servoing. In the proposed method, a blur is used to obtain the distance. The blur, one of the most important features, depends on the focal length of camera. Since it is not affected by the change of object, the reference feature value is not changed although other task object is taken. In this paper, we show a relationship between the distance and the blur, and define the feature jacobian matrix based on camera defocusing to operate the robot. A series of experiments is performed to verify the proposed method.