Effect of Green Microstructure on the Sintering and Properties of Aluminum Nitride (성형미세구조가 질화알루미늄의 소결 및 물성에 미치는 영향)

  • 이해원;전형우;송휴섭
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.2
    • /
    • pp.209-216
    • /
    • 1995
  • In order to investigate the effect o green microstructure on the sintering behavior and properties of AlN ceramics, samples were prepared by slip casting and dry pressing. The slip cast samples had high green density, fine pore size and narrow pore size distribution. They showed much higher sinterability and more homogeneous sintered microstructure compared to the dry pressed samples. Both increased thermal conductivity and flexural strength for samples prepared by slip casting could be attributed to the improved microstructural homogeneity with isolated second phase(s).

  • PDF

Correlation of the Green Microstructure of ZrO2 with the Colloid/Interface Variables (Zirconia성형체의 미세구조와 콜로이드/계면변수와의 상관관계에 대한 분석)

  • 장현명;한규호;이기강;정한남
    • Journal of the Korean Ceramic Society
    • /
    • v.27 no.1
    • /
    • pp.91-101
    • /
    • 1990
  • The green microstructure and sintering behavior of ZrO2 were analyzed in terms of kinetic stability (measured by the stability ratio ; W) and interfacial characteristics of colloidal suspension. Green density and the most frequent pore radius(MFPR) of green body were directly correlated with the stability ratio. These observations were explained using a concept of the critical stability ratio(Wc) and the potential energy of two interacting particles in colloidal suspension. Analysis of the data also indicates that the potential energy barrier between two interacting colloid particles should be higher than its critical value for a fabrication of ZrO2 green body with dense and uniform microstructure. Besides, we have successfully applied a concept of the donoracceptor interaction to increase the kinetic stability of ZrO2 slip and density of green body.

  • PDF

Effects of particle size on processing variables and green microstructure in gelcast alumina green bodies (겔-케스팅한 알루미나 성형체에서 출발입도가 공정변수 및 성형 미세구조에 미치는 영향)

  • Ha, Chang-Gi;Kim, Jae-Won;Jo, Chang-Yong;Baek, Un-Gyu;Jeong, Yeon-Gil
    • Korean Journal of Materials Research
    • /
    • v.11 no.10
    • /
    • pp.869-878
    • /
    • 2001
  • Alumina $(Al_2O_3)$ green bodies were fabricated by gel-casting using three kinds of alumina with different particle size (mean particle size: 4.6 $\mu\textrm{m}$, 0.32 $\mu\textrm{m}$, 10nm). The effects of particle size on gel-casting process and green microstructure were investigated. The optimum dispersion conditions using ammonium salt (D-3019) as dispersant were 0.2 wt% (4.63 $\mu\textrm{m}$), 0.5 wt% (0.32 $\mu\textrm{m}$), and 5.0 wt% (10 nm), in high solid loading. The optimum solid loading of each starting material for gel-casting was obtained as 59 vol% (4.63 $\mu\textrm{m}$), 57 vol% (0.32 $\mu\textrm{m}$), 15 vol% (10 nm), depending on particle size, indicating that nano-size particle (10 nm) represent lower solid loading as high specific surface area than those of other two starting materials. The drying at ambient conditions (humidity; $\thickapprox$90%) was performed more than 48hrs to enable ejection of the part from the mold and then at $120^{\circ}C$ for 2hrs in an air oven, showing no crack and flaw in the dried green bodies. The pore size and distribution of the gelcast green bodies showed the significant decrease with decreasing particle size. Green microstructure was dependent on the pore size and distribution due to the particle size, and on the deairing step. The green density maximum obtained was 58.9% (4.63 $\mu\textrm{m}$), 60% (0.32 $\mu\textrm{m}$), 47% (10 nm) theoretical density (TD), and the deairing step applied before gel-casting did not affect green density.

  • PDF

Effect of Green Microstructure on Sintered Microstructure and Mechanical Properties of Reaction-Bonded Silicon Carbide (성형미세구조가 반응소결 탄화규소체의 소결미세구조 및 기계적 특성에 미치는 영향)

  • 박현철;김재원;백운규;최성철
    • Journal of the Korean Ceramic Society
    • /
    • v.36 no.1
    • /
    • pp.97-105
    • /
    • 1999
  • In the binary system of SiC and carbon, porosity and pore size distribution of green body was controlled by varying pH, by the addition of polyelectrolyte dispersants, and by using different particle size of starting powders. The preforms having different green microstructure were fabricated by slip casting from suspensions having different dispersion condition. The reaction bonding process was carried out for these preforms. The condition of reaction bonding was 1600$^{\circ}C$ and 20 min. under vacuum atmosphere. The analyses of optical and SEM were studied to investigate the effect of green microstructure on that of reaction bonded silicon carbide and subsequently the mechanical properties of sintered body was investigated. Different green microstructures were obtained from suspensions having different dispersion condition. It was found that the pore size could be remarkably reduced for a fine SiC(0.5$\mu\textrm{m}$). The bimodal microstructure was not found in the present study, which is frequently observed in the typical reaction bonded silicon carbide. It is considered that the ratio between SiC and C was responsible for the formation of bimodal microstructure. For the preform fabricated from the well dispersed suspension, the 3-point bending strength of reaction-bonded silicon carbide was 310${\pm}$40 MPa compared to the specimen fabricated from relatively agglomerated particles having lower value 260${\pm}$MPa.

  • PDF

Effect of Suspension Property on Granule Characteristics and Compaction Behavior of Fine Si3Na4 Powder (분산계 특성이 질화규소 미분의 과립특성 및 충진거동에 미치는 영향)

  • 이해원;오성록
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.4
    • /
    • pp.462-470
    • /
    • 1995
  • The characteristics of spray-dried granules are important for dry pressing operation since they have great influences on die-filling, compaction ratio, and resulting green microstructure. An attempt was made to control granule morphology and the packing structure of fine Si3N4 particles in granules by adjusting suspension property. Mercury porosimetry was used to characterize the pore structures of both granules and green compacts. Finally, the effects of particle packing structure in granules and green microstructure on sintering behavior were investigated.

  • PDF

Electrodeposition Characteristics of Corrosion Resistant Tantalum Coating Layer for Hydrogen Production Sulfide-Iodine Process (수소생산을 위한 Sulfide-Iodine 공정장치용 초내식 탄탈코팅층 전착특성)

  • Lee, Youngjun;Kim, Daeyoung;Han, Moonhee;Kang, Keangsoo;Bae, Gigwang;Lee, Jonghyeon
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.23 no.6
    • /
    • pp.573-580
    • /
    • 2012
  • Corrosion resistance and basic physical properties of solid tantalum are not comparable to most of the structural metallic materials. The relative high cost and melting temperature of tantalum are obstacles to be widely applied to general engineering processes. Electrodeposition in molten salt enables compact and uniform tantalum coating. In this study, Ta was coated onto base metal (SUS316L) with different current densities (0.5, 5, $20mA/cm^2$) by using MSE (Molten Salt Electrodeposition). In this study, it showed that deposition efficiency and microstructure of Ta coating layer were strongly depended on current density. In the case of the current density of $5mA/cm^2$, densest microstructure was obtained. The current density above $5mA/cm^2$ caused non-uniform microstructure due to rapid deposition rate. Dense microstructure and intact coating layer contributed to significant corrosion resistance enhancement.

Effect of Aggregates on the Microstructure in Manganese Zinc Ferrite

  • Shin, Hyo-Soon;Lee, Dae-Hee;Kim, Chang-Bum;Kim, Nam-Kyung;Lee, Suk-Kee;Lee, Byung-Kyo
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.1
    • /
    • pp.1-4
    • /
    • 2003
  • To study the effect of aggregates on the microstructure of sintered bodies, Mn-Zn ferrite powders were prepared by an alcoholic dehydration method. Aggregate powders and reground powders were used as seeds and matrices, respectively. The mixing ratios for the aggregate and reground powders were varied with the sintering temperatures. Green densities were measured with changes in forming pressure and they were related to the microstructures of the sintered bodies. The aggregates proved to be capable of acting as seeds for abnormal grain growth. When the green density difference between the aggregate and the matrix was large, the aggregate could become the seed of abnormal grain growth. As the forming pressure increased, the more aggregates became seeds of abnormal grain growth.

Fabrication of Light Aggregates Using the Fly Ash-Clay Slurry

  • Seunggu Kang;Lee, Kigang;Kim, Jungwan
    • Proceedings of the Korea Association of Crystal Growth Conference
    • /
    • 1998.06a
    • /
    • pp.81-86
    • /
    • 1998
  • The light aggregates were fabricated by sintering green bodies made form the fly ash-clay alip. The content of fly ashes in the slip could be increased up to 70wt.% due to controlled rheological behavior of the slip, and the green body of uniform microstructure could be obtained by DCC(Direct Coagulation Casting)method. The apparent density, microstructure and compressive strength for sintered bodies fired at 1100∼1200$^{\circ}C$ were evaluated. The properties of light aggregates fabricated depend on slip density, particle behavior in the slip and sintering conditions. The sintered body prepared by firing a green body made from slip of density 1.60 at 1150$^{\circ}C$/2hr satisfied conditions of a light aggregate as apparent density of 1.49${\pm}$0.02 and compressive strength of 584${\pm}$62kg/$\textrm{cm}^2$.

  • PDF

Fabrication and Characteristics of Low Temperature Firing Substrate by Tape Casting in Fluormica System (Tape Casting에 의한 fluormica계 제조 및 특성 저온 소결 기판의 제조 및 특성)

  • 박대현;최정헌;강원호;김병익
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.673-676
    • /
    • 1999
  • We fabricated green sheet by tape casting method with fluormica glass-ceramic powders for fabrication of low temperature co-firing substrate. After ball milling with organic additives, we investigated green strength and density of green sheets which were casted by doctor blade machine. Green sheets were sintered at 700 ~ 1,00$0^{\circ}C$ for 1 ~3hrs. Microstructure, linear shrinkage and dielectric constant of substrates were surveyed.

  • PDF

Effects of Organic and Inorganic Binder Core on Microstructure and Mechanical Properties of Al Casting Products (알루미늄 주조품의 미세조직 및 기계적 특성에 미치는 유·무기 화합물 중자의 영향)

  • Shin, Sang-Soo;Kim, Woo-Chun;Kim, Eok-Soo;Lim, Kyoung-Mook;Park, Jeong-Wook
    • Journal of Korea Foundry Society
    • /
    • v.33 no.4
    • /
    • pp.147-156
    • /
    • 2013
  • The effects of core materials on the microstructure and mechanical properties of Al casting products have been investigated. The Al casting samples and cylinder head were fabricated by using organic and inorganic binder core respectively, and their microstructure and mechanical properties were evaluated. The Al casting samples fabricated by using inorganic core showed the better mechanical properties such as tensile strength and elongation than those of the Al casting samples fabricated by using organic core. That's because the Al casting samples contained small amount of pore defects and had fine microstructure compared with the Al casting samples fabricated by using organic core. Also, the use of inorganic core effectively reduced harmful gas emission and pollution.