Effect of Semiconductor Layer and Breakdown Strength of MDPE films (MDPE 필름의 절연파괴강도와 반도전층효과)

  • 유성수;리종찬;류부형;박수길;박대희
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 1999.05a
    • /
    • pp.239-242
    • /
    • 1999
  • In this study, we evaluates the dependence of thickness and temperature in the breakdown strength of MDPE and effect of semiconductor. As the result, breakdown strength trend to decrease according to the increase of thickness and temperature but there is no dependence of temperature in the 70${\mu}{\textrm}{m}$ MDPE film. We obtained the result that the breakdown strength was a little lower in the structure of Semil/MDPE than Semi/MDPE/Semi, but breakdown strength of MDPE was greater both of all. Therefore we are investigating the effect of semiconductor in the breakdown strength.

  • PDF

Dielectric and Breakdown Characteristics of MDPE included Semiconductor layer (반도전층을 갖는 MDPE의 운전 및 절연파괴 특성)

  • Yoo, Sung-Soo;Lee, Jong-Chan;Park, Dae-Hee
    • Proceedings of the KIEE Conference
    • /
    • 1999.07d
    • /
    • pp.1633-1635
    • /
    • 1999
  • In this study, we evaluated the dependence of thickness and temperature in the breakdown strength of MDPE and effect of semiconductor. As the result, breakdown strength trend to decrease according to the increase of thickness and temperature. We obtained the result that the breakdown strength was a little lower in the structure of Semi/MDPE than Semi/MDPE/Semi, but breakdown strength of MDPE was greater both of all. The dependency of permittivity, tan ${\delta}$ and conductance on frequency and temperature were investigated. Both of the specimans showed the trend of decreased in permittivity as the temperature increased but increase as the frequency increased.

  • PDF

Characterization of Water Vapor Transmission & Dielectric Breakdown in Insulation Materials for Jacket Compound (자켓 컴파운드용 절연재의 수증기투과 및 절연파괴 특성)

  • Song, Jae-Joo;Han, Jae-Hong;Song, IL-Keun;Han, Yong-Hee;Han, Byung-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11b
    • /
    • pp.52-56
    • /
    • 2001
  • Experiments of 2 type on insulating compounds accomplished to change PVC using in URD(Underground) power cable jacketing. one was DB (Dielectric Breakdown) test on the pure base resins and the others were WVT(Water Vapor Transmission) test on the compounds which contained C/B(Carbon Black), anti-oxidant to base resin. a kind of specimens made by pressing to resin of pellet or lump form was HDPE(High Density Polyethylene), MDPE(Medium Density Polyehylene), LDPE(Low Density Polyethylene), LLDPE(Linear Low Density Polyethylene), PVC (Polyvinyl Chloride). As a results of AC DB and WVT test, we saw that strength of Insulation was HDPE > LLDPE ≒ MDPE > LDPE and WVT ratio was HDPE < LLDPE < MDPE < LLDPE ≒ LDPE${\ll}$PVC. WVT of PVC using for jacket showed characteristic 15 times more than MDPE or LLDPE. Therefore, to development of watertightness cable, our works present need of Changing in insulating materials

  • PDF

Effects of Defect Size on Crush Test Load of Butt Fusion Welded MDPE Pipes

  • Tun, Nwe Ni;Lai, Huan Sheng;Jeon, Gyu Min;Yoon, Kee Bong;Kil, Seong Hee
    • Journal of Energy Engineering
    • /
    • v.24 no.4
    • /
    • pp.55-62
    • /
    • 2015
  • It is expected that the size of welding defect affects the mechanical performance of welded medium density polyethylene (MDPE) pipe joints. In this study, butt fusion welded MDPE pipe joints with a single spherical or planar defect of various sizes were studied using experimental crush testing and also by finite element method. The crush test showed that the mechanical performance of crush was not affected by the size and geometry of a single welding defect when the defect size was increased to 45% of the pipe's wall thickness. The simulation results indicated that the effect of the single welding defect on the Von Mises stress distribution near the defect explained the reason of the test results.

Chararcteristics of Water Vapor Transmission in Base Resin for Underground Residential Distribution Power Cable (지중배전케이블 기저수지의 수증기 투과 전달특성)

  • Song, Jae-Joo;Han, Byung-Sung
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.05b
    • /
    • pp.149-153
    • /
    • 2003
  • In URD(Underground Residential Distribution) power cable, experiments of WVT(Water Vapor Transmission) test on the Base Resin accomplished to specimens which contained CB(Carbon Black), anti-oxidant to base resin and made by pressing to resin of pellet or lump form. a kind of specimens was HDPE(High Density Polyethylene), MDPE(Medium Density Polyethylene), LDPE(Low Density Polyethylene), LLDPE(Linear Low Density Polyethylene), PVC(Polyvinyl Chloride). as a results of WVT test, we saw that WVT ratio was HDPE < LLDPE < MDPE≒LDPE${\ll}$ PVC. WVT properties of PVC using for jacket showed properties 15-20 times more than MDPE or LLDPE. Therefore, to development of watertightness cable, our works present need of Changing in insulating materials.

  • PDF

Characterization of Water Vapor Transmission & Dielectric Breakdown in Insulation Materials for Jacket Compound (자켓 컴팍운드용 절연재의 수증기투과 및 절연파괴 특성)

  • 송재주;한재홍;송일근;한용희;한병성
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2001.11a
    • /
    • pp.52-56
    • /
    • 2001
  • Experiments of 2 type on insulating compounds accomplished to change PVC using in URD(Underground) power cable jacketing. one was DB(Dielectric Breakdown) test on the pure base resins and the others were WVT(Water Vapor Transmission) test on the compounds which contained C/B(Carbon Black), anti-oxidant to base resin. a kind of specimens made by pressing to resin of pellet or lump form was HDPE(High Density Polyethylene), MDPE(Medium Density Polyehylene), LDPE(Low Density Polyethylene), LLDPE(Linear Low Density Polyethylene), PVC(Polyvinyl Chloride). As a results of AC DB and WVT test, we saw that strength of Insulation was HDPE> LLDPE = MDP E> LDPE and WVT ratio was HDPE

  • PDF

A Study on Proper Location of Welding Defect in Three Point Bend Testing with MDPE Pipe

  • Lai, Huan Sheng;Yoon, Kee Bong;Kil, Seong Hee
    • Journal of Energy Engineering
    • /
    • v.24 no.1
    • /
    • pp.1-9
    • /
    • 2015
  • Welding defects affect the performance of welded pipe joints. In this study, a three point bend test of welded steel and medium density polyethylene (MDPE) pipe joints with defects of various defect locations and defect materials was studied using the finite element method. The defect was assumed to be located at 12 o'clock, 3 o'clock or 6 o'clock direction. The results showed that pipes failed more easily on the compression side due to stress or local buckling. The air defect was more dangerous than the steel defect if the defect was located in the compression side; otherwise, the defect material effect on the integrity of pipes was ignorable. It is argued that the integrity of pipes with defects in the compression side is weaker than that in other regions, and the defect should be located in the compression side or the 12 o'clock position in the three point bend test to maximize the effect of defect existence on the pipe structural integrity.

Wet Environmental and Mechanical Characteristics for Polyethylene-based Insulating Materials (Polyethylene 계열 절연재료의 환경적·기계적 특성)

  • Song, Woo-Chang;Choi, Won-Seok;Park, Ha-Yong
    • The Transactions of the Korean Institute of Electrical Engineers P
    • /
    • v.63 no.2
    • /
    • pp.119-123
    • /
    • 2014
  • In this study, four kinds of specimens of PE(polyethylene)-based insulating materials were prepared for selecting the optimum insulation materials in a wet environment. The specimens were tested by various methods, the anti tracking test, the transmittance test in the water vapor transmittance(WVT) and the abrasion resistive test, etc. The HDPE(high-density polyethylene) specimen was showed excellent property in the tracking resistance test and the lowest transmittance in water vapor transmittance test. In the abrasion resistive test, the LLDPE(linear low-density polyethylene) and MDPE(medium-density Polyethylene) were showed excellent mechanical properties. The value of cut-through resistance for MDPE and HDPE were superior to that for LLDPE and LDPE(low-density polyethylene).

Development of Waterproof Jacket Materials for Power Cables

  • Han, Yong-Huei;Jung, Jong-Wook;Kwon, Tae-Ho;Song, Hyun-Seok;Koo, Kyo-Sun;Han, Byung-Sung
    • KIEE International Transactions on Electrophysics and Applications
    • /
    • v.3C no.4
    • /
    • pp.146-154
    • /
    • 2003
  • This paper describes various characteristics of the new compounds for cable jackets and model cables advanced in waterproof performance in order to essentially solve the problems of underground (URD) distribution class power cable failures. Several compounds were manufactured by the inclusion of additives to base resins available in Korea and tested for basic property, mechanical and electrical characteristics. Two model cables were created by using the compounds determined in the test as being the most appropriate for new structured model cable jacket material. The waterproof performance and mechanical strength of the new cable jackets were verified by applicable tests. As a result, MDPE and LLDPE compounds were superior as cable jackets in both mechanical and electrical characteristic aspects when compared with conventional PVC. In addition, the model cables composed of the new compounds based on MDPE showed good quality results in the water permeability test.

열처리 채소의 MAP에 적합한 포장재 구명

  • 강준수;조학래
    • Proceedings of the Korean Society of Postharvest Science and Technology of Agricultural Products Conference
    • /
    • 2003.04a
    • /
    • pp.142.2-142
    • /
    • 2003
  • 본 연구에서는 풋고추, 대파와 깻잎에 물리적인 장해를 주지 않고 저장성을 향상시킬 수 있는 열처리 조건을 설정하고, 열처리한 채소의 MAP에 적합한 포장재를 검색하기 위한 실험을 수행하였다. 대파를 55$^{\circ}C$ 온수에서 1분 침지하고, 풋고추와 깻잎은 5$0^{\circ}C$ 온수에서 10초와 5초 각각 침지하면 저장 중 관능적 품질이 비열처리한 대조구보다 우수하게 나타났다. 열처리한 채소의 호흡속도는 비열처리 채소에 비하여 30~45%정도 상승하였다. 열처리 채소의 MAP에 적합한 포장재를 검색하기 위하여 기체 투과도가 서로 다른 포장재 LDPE, CPP, PD900, MPD2055, SM60에 열처리한 채소를 포장한 후 1$0^{\circ}C$에서 4주간 저장을 하였다. 포장 표면에 5mm의 구멍을 뚫은 대조구와 핀홀이 있는 SM60은 저장 2주 이후 부터 중량감소가 심하게 일어났다. 깻잎은 포장내부의 $CO_2$ 농도가 높게 유지되는 CPP에 포장할 때, 저장 2주부터 $CO_2$ 장해로 인하여 표면의 갈변과 연화가 심하게 일어났으며, 풋고추는 저장 3주부터 표면의 색상이 약간 붉은 색을 나타내기 시작하였다. 열처리 풋고추와 깻잎을 MDPE 포장에 저장을 하면 각각 저장 4주와 3주까지는 시장품질의 한계선으로 신선도가 유지되었다. 그러나 대파는 포장 내부의 $CO_2$ 농도가 높은 CPP에 포장할 경우 발근이 억제되며 저장 4주까지 시장품질 이상을 유지하였다.

  • PDF