AE Characteristics on Microscopic Failure Behavior of Carbon/Epoxy Comosite Prepared by Cocure and Precure Process (Cocure/Precure 경화공정에 의해 제조된 Carbon/Epoxy 복합재료의 미시적 파손거동에 대한 AE 특성)

  • Lee, Jin-Gyeong;Lee, Jun-Hyeon;Lee, Min-Rae;Choe, Heung-Seop
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.24 no.10 s.181
    • /
    • pp.2520-2528
    • /
    • 2000
  • Mechanical and physical properties of composite materials make a great difference due to their cure process condition. In order to clarify the effect of cure process condition on the microscopic damage behavior and failure mechanism of Carbon/Epoxy composites, three point bend test has been performed. For this purpose, two kinds of specimens with single adhesive and multiple adhesive layers were prepared. For single adhesive layer, four different types of specimen were used, that is, non-sanding, sanding, cocured, laminated specimens. Three different types of specimen were also used for the multiple adhesive layer, non-sanding, sanding, cocured specimens. Acoustic emission technique has also been employed to monitor the damage progresses associated with each micro-failure mechanism. The characteristics of AE parameters associated with micro-failure mechanism of each specimen were discussed.

INFLUENCE OF MULTIPLE ADHESIVE COATINGS ON THE SHEAR BONDING STRENGTH OF COMPOSITE RESIN (접착제의 다층적용이 복합레진의 전단결합강도에 미치는 영향)

  • Park, Heon-Dong;Lee, Chang-Seop;Lee, Sang-Ho;Lee, Nan-Young
    • Journal of the korean academy of Pediatric Dentistry
    • /
    • v.33 no.3
    • /
    • pp.377-387
    • /
    • 2006
  • The objective of this study was to evaluate the influence of multiple adhesive coatings on the thickness of hybrid and adhesive layer and shear bond strength(SBS) of self-etch adhesives and self-etch primer adhesives. The buccal or lingual crown dentin of extracted human molars was used. Self-etch adhesives or self-etch primer adhesives were applied 1, 2 and 3 times on the dentin before light curing. In another group adhesives were reapplied after light curing first layer. Treated surfaces were prepared to measure the thickness of hybrid and adhesive layer with SEM, and shear bond strength to dentin using an Instron machine. The following results were obtained : 1. The adhesive layers increased with the number of coatings(p<0.05) with all adhesives. Adpor Prompt L-Pop and Xeno III were significantly thinner than self-etch primer adhesives (p<0.05). 2. The thickness of hybrid layers increased with the number of coatings (p<0.05). 3. The shear bonding strength of Unifil Bond and Clearfill SE Bond were higher than Scotchbond Multipurpose Plus and Adpor Prompt L-Pop (p<0.05), and similar with Xeno III. 4. The shear bond strength increased significantly with the number of coatings in Adpor Prompt L-Pop(p<0.05), but decreased at 3 times in AdheSE Bond(p>0.05). 5. In Adpor Prompt L-Pop and Xeno III, the shear bond strength decreased when adhesives were reapplied after curing the first adhesive layer.

  • PDF

THE EFFECT OF MULTIPLE APPLICATION ON MICROTENSILE BOND STRENGTH OF ALL-IN-ONE DENTIN ADHESIVE SYSTEMS (All-in-one adhesive의 다층적용이 미세인장결합강도에 미치는 영향)

  • Son, Sung-Ae;Hur, Bock
    • Restorative Dentistry and Endodontics
    • /
    • v.29 no.5
    • /
    • pp.423-429
    • /
    • 2004
  • The purpose of this study was to evaluate the effect of multiple application of all-in-one dentin adhesive system on microtensile bond strength using confocal laser scanning microscope and microtensile bond strength test. Flat occlusal dentin surfaces were prepared using low-speed diamond saw. In group I, Scotchbond Multipurpose (SM) was applied by manufacturer's recommendation. In group II, after Adper Prompt L-Pop was applied for 15s and light cured for 10s. the second coat was re-applied and light-cured. In group III, after light-curing the second layer. the third coat was re-applied and light-cured. Specimens bonded with a resin-composite were sectioned into resin-dentin stick for measuring the adhesive layer thickness by confocal laser scanning microscope and evaluating micro-tensile bond strength. The adhesive layers of three-step dentin adhesive system. 3 coats of Adper Prompt L-Pop had significantly thicker than SM. 2 coats of Adper Prompt L-Pop (p < 0.05). However. there was no significant differences in bond strengths between SM and 3 coats of Adper Prompt L-Pop (p > 0.05). And SM. 3 coats of Adper Prompt L-Pop had significantly higher than 2 coats of Adper Prompt L-Pop in bond strengths (p < 0.05).

EFFECT OF INTERMEDIATE RESIN HYDROPHILICITY ON BOND STRENGTH OF SINGLE STEP ADHESIVE (중간레진의 친수성이 상아질 접착에 미치는 영향)

  • Kim, Yong-Sung;Park, Sang-Hyuk;Choi, Gi-Woon;Choi, Kyoung-Kyu
    • Restorative Dentistry and Endodontics
    • /
    • v.32 no.5
    • /
    • pp.445-458
    • /
    • 2007
  • The purpose of this study was to evaluate the bond strength of a new Single step system with different curing mode composites, and to evaluate the effect of the intermediate resins which have different hydrophilicity on bonding ability by means of the micro shear bond testing and TEM examination for the adhesive interface. The adhesive used in this study was an experimental single step system (Bisco Inc., Schaumburg IL). Experimental groups were produced by using six kinds of intermediate resin having different hydrophilicity that was hydrophilic, hydrophobic and most hydrophobic resin and as filled or not after applying adhesive. Each experimental group was further divided into two subgroups whether the adhesive was light cured or not. Dual cured composite (Bis Core, Bisco Ltd., Schaumburg, IL) was placed on the adhesive layer as light cure or self cure mode. The results or bond strength were statistically analyzed using one way ANOVA and multiple comparisons are made using Tukey's test at ${\alpha}\;<\;0.05$ level. The results of this study were as follows ; 1. The application of intermediate resin did not increase the bond strength for light cured composite. 2. The bond strength of an experimental adhesive with self cured composite was significantly increased by the application of intermediate resin layer. 3. The bond strength of adhesive was irrespective of the cure or not of itself before intermediate resin layer applied. 4. As applied hydrophilic resin layer was, the initial bond strength was higher than both hydrophobic and most hydrophobic one used but there was no significance. Using a single step adhesive with dual/self cured composite, the incompatibility between both of them should be solved by the application of intermediate hydrophobic resin to reduce the adhesive permeability. However, Single step adhesive can be used in the light cured composite restoration without any decrease of the initial bond strength.

Visibility Enhancement of the Ultrasonic Signal Reflected from Adhesive Layers (접착층에서 반사된 초음파 신호의 가시도 개선)

  • Shin, Jin Seob;Lee, Jeong-Ihll
    • The Journal of the Institute of Internet, Broadcasting and Communication
    • /
    • v.8 no.6
    • /
    • pp.153-157
    • /
    • 2008
  • Recently, electronic devices is produced by multilayer structure, therefore analysis for hidden layers is important nondestructive inspection. This paper presents visibility enhancement methods for the ultrasonic multiple echoes reflected from adhesive layer in the multilayers using digital signal processing. The reflected signals from the multilayers come out interval of the peaks in the power cepstrum. In the experiment, the adhesive layers of settled thickness using epoxy were formed. The reflected signals from the multilayer is detected by pulse-echo method and power cepstrum is processed for enhancement of visibility.

  • PDF

Effect of adhesive application method on repair bond strength of composite

  • Hee Kyeong Oh;Dong Hoon Shin
    • Restorative Dentistry and Endodontics
    • /
    • v.46 no.3
    • /
    • pp.32.1-32.10
    • /
    • 2021
  • Objectives: This study aimed to evaluate the effect of the application method of universal adhesives on the shear bond strength (SBS) of repaired composites, applied with different thicknesses. Materials and Methods: The 84 specimens (Filtek Z350 XT) were prepared, stored in distilled water for a week and thermocycled (5,000 cycles, 5℃ to 55℃). They were roughened using 400-grit sandpapers and etched with phosphoric acid. Then, specimens were equally divided into 2 groups; Single Bond Universal (SU) and Prime&Bond Universal (PB). Each group was subdivided into 3 subgroups according to application methods (n = 14); UC: 1 coat + uncuring, 1C: 1 coat + curing, 3C: 3 coats + curing. After storage of the repaired composite for 24 hours, specimens were subjected to the SBS test and the data were statistically analyzed by 2-way analysis of variance and independent t-tests. Specimens were examined with a stereomicroscope to analyze fracture mode and a scanning electron microscope to observe the interface. Results: Adhesive material was a significant factor (p = 0.001). Bond strengths with SU were higher than PB. The highest strength was obtained from the 1C group with SU. Bonding in multiple layers increased adhesive thicknesses, but there was no significant difference in SBS values (p = 0.255). Failure mode was predominantly cohesive in old composites. Conclusions: The application of an adequate bonding system plays an important role in repairing composite resin. SU showed higher SBS than PB and the additional layers increased the adhesive thickness without affecting SBS.

Tensile Strengths of Demineralized Dentin derived from Self-Priming Adhesives (Self-Priming Adhesives를 침투시킨 탈회 상아질의 인장강도)

  • Lee, Hye-Yun;Yoon, Mi-Ran;Lee, Rin;Lee, Jeong;Lee, Kwang-Won
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.22 no.2
    • /
    • pp.181-191
    • /
    • 2006
  • The objectives of this study were to evaluate the tensile strength of resin-infiltrated demineralized dentin according to the demineralization time, and to evaluate the tensile strength of hybrid layer that is formed by infiltrating different priming adhesives or primer/adhesive into demineralizd dentin matrix. Seventy five hour-glass shaped dentin specimens were prepared in mid-coronal dentin from extracted human molars. Thirty specimens were distributed into three groups according to demineralization time - 2 hours, 4 hours and 8 hours. Each specimen was placed in primer/adhesive of All-Bond 2 for 5 hours of infiltration. Another forty-five specimens of them were demineralized in 37% phosphoric acid for 4 hours. They were randomly assigned to three experimental groups - AB, SB and OS - to designate All-Bond 2, Single Bond and One-Step. Each specimen was placed in one of three different adhesives for 5 hours of infiltration. The specimens were visible light-cured for 5 minutes, and then stored for 24 hours in distilled water at $37^{\circ}C$. After that, microtensile bond strength for each specimen was measured, and the fractured surfaces were then observed by SEM. The data were statistically analysed by one-way ANOVA and Tukey's multiple comparison test and Bonferroni's multiple comparison test. The results were as follows; 1. Tensile strength of the group demineralized for 4 hours was significantly higher than that of groups demineralized for 2 hours and 8 hours (P < .01). 3. Tensile strength of the AB group was significantly higher than that of the SB group and OS group (P < .01).

EFFECT OF FILM THICKNESS OF RESIN CEMENT ON BONDING EFFICIENCY IN INDIRECT COMPOSITE RESTORATION (레진 시멘트의 film thickness가 간접 복합 레진 수복물의 접착 효율에 미치는 영향에 관한 연구)

  • Lee, Sang-Hyuck;Choi, Gi-Woon;Choi, Kyung-Kyu
    • Restorative Dentistry and Endodontics
    • /
    • v.35 no.2
    • /
    • pp.69-79
    • /
    • 2010
  • The purpose of this study was to evaluate the effect of film thickness of various resin cements on bonding efficiency in indirect composite restoration by measurement of microtensile bond strength, polymerization shrinkage, flexural strength and modulus, fractographic FE-SEM analysis. Experimental groups were divided according to film thickness (< $50\;{\mu}m$-control, $50\;{\mu}m$-T50, $100\;{\mu}m$-T100, $150\;{\mu}m$-T150) using composite- based resin cements (Variolink II, Duo-Link) and adhesive-based resin cements (Panavia F, Rely X Unicem). The data was analyzed using ANOVA and Duncan's multiple comparison test (p < 0.05). The results were as follows ; 1. Variolink II showed higher microtensile bond strength than that of adhesive-based resin cements in all film thickness (p < 0.05) but Duo-Link did not show significant difference except control group (p > 0.05). 2. Microtensile bond strength of composite-based resin cements were decreased significantly according to increasing film thickness (p < 0.05) but adhesive-based resin cements did not show significant difference among film thickness (p > 0.05). 3. Panavia F showed significantly lower polymerization shrinkage than other resin cements (p < 0.05). 4. Composite-based resin cements showed significantly higher flexural strength and modulus than adhesive-based resin cements (p < 0.05). 5. FE-SEM examination showed uniform adhesive layer and well developed resin tags in composite-based resin cements but unclear adhesive layer and poorly developed resin tags in adhesive-based resin cements. In debonded surface examination, composite-based resin cements showed mixed failures but adhesive-based resin cements showed adhesive failures.

Coating Properties of Single and Multi-Layer Graphene Oxide on a Polystyrene Surface (산화그래핀 층수에 따른 폴리스타이렌 표면 코팅 특성)

  • Lee, Jihoon;Park, Jaebum;Park, Danbi;Huh, Jeung Soo;Lim, Jeong Ok
    • Korean Journal of Materials Research
    • /
    • v.31 no.7
    • /
    • pp.420-426
    • /
    • 2021
  • Graphene, a new material with various advantageous properties, has been actively used in various fields in recent years. Applications of graphene oxide are increasing in combination with other materials due to the different properties of graphene oxide, depending on the number of single and multiple layers of graphene. In this study, single-layer graphene oxide and multi-layer graphene oxide are spray coated on polystyrene, and the physicochemical properties of the coated surfaces are characterized using SEM, Raman spectroscopy, AFM, UV-Vis spectrophotometry, and contact angle measurements. In single-layer graphene oxide, particles of 20 ㎛ are observed, whereas a 2D peak is less often observed, and the difference in surface height increases according to the amount of graphene oxide. Adhesion increases with an increase in graphene oxide up to 0.375 mg, but decreases at 0.75 mg. In multi-layer graphene oxide, particles of 5 ㎛ are observed, as well as a 2D peak. According to the amount of graphene oxide, the height difference of the surface increases and the adhesive strength decreases. Both materials are hydrophilic, but single-layer graphene oxide has a hydrophilicity higher than that of multi-layer graphene oxide. We believe that multi-layer graphene oxide and single-layer graphene oxide can be implemented based on the characteristics that make them suitable for application.

Influence of the curing time for the adhesive on the oxygen-inhibited layer thickness and the shear bond strength to dentin (광조사 시간이 접착제의 표면 미중합층의 두께와 전단접착강도에 미치는 영향에 관한 연구)

  • Choi, Yong-Hoon;Bae, Ji-Hyun;Son, Ho-Hyun;Lee, In-Bog;Um, Chung-Moon;Baek, Seung-Ho;Kim, Oh-Young;Kim, Chang-Keun;Cho, Byeong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.29 no.2
    • /
    • pp.177-184
    • /
    • 2004
  • Objectives : This study investigated the hypothesis that increasing light-curing time would leave the oxygen-inhibited layer (OIL) of the adhesive thinner, and in turn, result in lower shear bond strength (SBS) than those obtained by the routine curing procedures. Methods:120 human extracted posterior teeth were randomly divided into three groups for bonding with three adhesives:All Bond 2/sup (R)/, One Step/sup (R)/, and Adper Prompt/sup (R)/. They were subsequently divided into four subgourps with different light-curing time (10, 20, 30 and 60s). The assigned adhesives were applied on superficial occlusal dentin according to the manufacturer's instructions and cured with one of the four curing times. Composite resin cylinder, 2.35㎜ in diameter, were built on the cured adhesive and light-cured for 40s. SBS were measured after 24h from the bonding using a universal testing machine (crosshead speed 1.0 ㎜/min). The relative thickness of the OIL and the degree of conversion (DC) were determined from the adhesive on a slide glass using FT-NIR in an absorbance mode. Data were analysed with One-way ANOVA and Duncan's multiple test (p〈0.05), Results:With increasing cure time, although there were no significant difference in th SBS of One-step and Adper Prompt (p〉0.05), those of All Bond 2 decreased significantly (p〈0.05). The relative thicknesses of the OIL on each adhesive were not affected by the cure time (p〉0.05). Although the DC of All-Bond 2 were statistically not different with increasing cure time (p〉0.05), those of One-Step and Adper Prompt showed an increasing trends with increasing cure time (p〈0.05). Conclusions:Increasing light-curing time did not affect on the relative thickness of the OIL of the adhesives, and in turn, on the SBS to dentin.