Preparation of Nano Disperse Dyes from Nanoemulsions and Their Dyeing Properties on Ultramicrofiber Polyester

  • Choi Jae-Hong;Kang Min-Ju
    • Fibers and Polymers
    • /
    • v.7 no.2
    • /
    • pp.169-173
    • /
    • 2006
  • Six nano disperse dyes were prepared using corresponding O/W nanoemulsions which were obtained with sodium laurylsulphate and caprylic triglyceride. The average particle size of the dyes prepared were in the range of $110{\sim}130nm$. Exhaust dyeing using nano dyes resulted in low exhaustion yields of $17{\sim}26%$ on regular polyester fiber and $28{\sim}38%$ on ultramicrofiber polyester. The observed low exhaustion yields of nano disperse dye can be explained by the solubilization of dye particles into surfactant micelles as well as the high stability of the nanoemulsions, these might reduce the capacity of dye uptake onto the fibers. However, higher K/S values of dyeings with nano dyes on ultramicrofiber sites compared to those on regular polyester sites suggested their potential to be more efficient dyes for finer denier microfiber polyesters.

Effect of Raising Process of Warp-knitted Fabric Containing Silver Nano-particles (기모공정에 따른 나노은입자함유 경편성물의 제품 특성에 관한 연구)

  • Son, Eun-Jong;Jung, Sung-Hoon;Hwang, Young-Gu;Jung, Hyun-Mi
    • Textile Coloration and Finishing
    • /
    • v.22 no.4
    • /
    • pp.356-361
    • /
    • 2010
  • This study was aimed to investigate the antibacterial efficiency of silver nano-particles and the dyeing properties of a brushed warp-knitted fabric. The properties of the brushed warp-knitted fabric containing silver nano-particle by field production processes were evaluated by analyzing its silver contents, antibacterial activity, color difference, exhaustion curve, fastness and tearing strength. Bacterial reduction ratio amounts to 91.4 and 99.9 for Staphylococcus aureus and Klebsiella pneumoniae respectively. As the brushed pile length of its fabrics is longer, the exhaution rate of disperse dye becomes higher. The brushing process of its fabrics reduces the tearing strength. The results indicate that the brushed warp knitted fabric containing silver nano-particle can be a practically promising product.