• Title/Summary/Keyword: Nano-diamond

Search Result 172, Processing Time 0.039 seconds

Wear Characteristics of Lubricant with Nano-diamond Particles on Al-6061 Aluminum Alloy (나노 다이아몬드 입자를 첨가한 엔진 오일의 알루미늄 6061 합금에 대한 마모 특성)

  • Hwang, Sung-Wan
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.20 no.12
    • /
    • pp.16-23
    • /
    • 2021
  • Pin-to-disc wear testing experiments were conducted to investigate the wear characteristics of commercial oil (5W-40) with nano-diamond particles. The upper specimen was a SUJ-2 high-carbon chromium steel ball with a diameter of 4 mm, and the lower specimen was made of the Al-6061 alloy. The applied load was 5 N, and the sliding speed was 0.25 m/s. The wear tests were conducted at a sliding distance of 500 m. The friction coefficients and wear rates of the Al-6061 specimens were tested using commercial oil with different nano-diamond concentrations ranging from 0 to 0.02 wt.%. The addition of nano-diamond particles to commercial oil reduced both the wear rate and coefficient of friction of the Al-6061 alloy. The use of nano-diamond particles as a solid additive in oil lubricants was found to improve the tribological behavior of the Al-6061 alloy. For the Al-6061 alloy, the optimal concentration was found to be 0.005 wt.% in view of the friction coefficient and wear rate. Further investigation is needed to determine the optimal concentration of nano-diamond particles for various loadings, sliding speeds, oil temperatures, and sliding distances.

Direct Conversion Sintering of Super-hard Nano-polycrystalline Diamond from Graphite

  • Sumiya, Hitoshi;Irifune, Tetsuo
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.1309-1310
    • /
    • 2006
  • High-purity and super-hard nano-polycrystalline diamond has been successfully synthesized by direct conversion from high-purity graphite under static pressures above 15 GPa and temperatures above $2300^{\circ}C$. This paper describes research findings on the formation mechanism of nano-structure and on the contributing factor leading to high hardness.

  • PDF

Study on Hardness and Corrosion Resistance of Magnesium by Anodizing and Sealing Treatment With Nano-diamond Powder (양극산화와 나노 다이아몬드 분말 봉공처리에 의한 마그네슘의 경도와 부식에 관한 연구)

  • Kang, Soo Young;Lee, Dae Won
    • Journal of Powder Materials
    • /
    • v.21 no.4
    • /
    • pp.260-265
    • /
    • 2014
  • In this study, in order to increase surface ability of hardness and corrosion of magnesium alloy, anodizing and sealing with nano-diamond powder was conducted. A porous oxide layer on the magnesium alloy was successfully made at $85^{\circ}C$ through anodizing. It was found to be significantly more difficult to make a porous oxide layer in the magnesium alloy compared to an aluminum alloy. The oxide layer made below $73^{\circ}C$ by anodizing had no porous layer. The electrolyte used in this study is DOW 17 solution. The surface morphology of the magnesium oxide layer was investigated by a scanning electron microscope. The pores made by anodizing were sealed by water and aqueous nano-diamond powder respectively. The hardness and corrosion resistance of the magnesium alloy was increased by the anodizing and sealing treatment with nano-diamond powder.

Study on Improvement of Corrosion Resistance and Wear Resistance by Anodizing and Sealing Treatment with Nano-diamond Powder on aluminum (알루미늄의 아노다이징과 나노 다이아몬드 분말 봉공처리에 의한 내식성과 내마모성 향상에 관한 연구)

  • Kang, Soo Young;Lee, Dae Won
    • Journal of the Korean institute of surface engineering
    • /
    • v.47 no.3
    • /
    • pp.121-127
    • /
    • 2014
  • In this study, in order to improve corrosion resistance and wear resistance of aluminum, surface treatment was made by anodizing with oxalic acid solution and sealing with nano-diamond powder. Average size of nano-diamond powder was 30nm. Anodizing with oxalic acid made many pores in the aluminum oxide layer. Pore size and oxide thickness were investigated by scanning electron microscope (SEM). Pore size increased as temperature increased and voltage increased. It was possible to make oxide layer with pore diameter more than 50 nm. Oxide thickness increased as temperature and voltage and treatment time increased. Oxide layer with above $10{\mu}m$ thickness was made. Aluminum oxide layer with many pores was sealed by water with nano-diamond powder. Surface morphology was investigated by SEM. After sealing treatment with nano-diamond powder, corrosion resistance, wear resistance and hardness increased.

A Study on the Tribological Characteristics of a Frying Pan Coated with PTFE and Nano-Diamond (나노다이아몬드가 첨가된 프라이팬 불소수지코팅의 Tribological 특성 연구)

  • Lee, Jin-Ho;Kim, Hyun-Soo;Yoon, Han-Ki;Kim, Tae-Gyu
    • Journal of Ocean Engineering and Technology
    • /
    • v.23 no.6
    • /
    • pp.99-104
    • /
    • 2009
  • PTFE has good mechanical and chemical stability at a wide range of temperatures and demonstrates a low friction coefficient value. PTFE is being used for self-lubricating parts in industry. But it shows a high wear rate. Thus, PTFE and nano-diamond powder were mixed into a composite and the wear properties of a PTFE coating layer on Al6061 was investigated. A ball-on-disk type of wear tester was used under a dry condition and different temperatures of oil. After the wear test, the wear track wasexamined by optical microscope. The PTFE-diamond showed the lowest friction coefficient (0.02) of all the lubricants in the experiments. The friction coefficient was shown to be directly related to the diamond powder in the PTFE coating. Adhesion estimations were performed by a scratch test, which is mainly used for coatings. The critical load between the coating and substrate was defined through analyses of the friction load, normal load curve, and acoustic emissions, along with optical microscope observations. The scratch test results showed that an import item (SWISS) gave the highest critical load values.

Characteristics of a Polycrystalline Diamond Thin Film Deposited on a-plane Sapphire Substrate (a-plane 사파이어기판에 증착된 Polycrystalline Diamond 박막의 특성)

  • Tan, Xing Yan;Jang, Tae Hwan;Kwon, Jin Uk;Kim, Tae Gyu
    • Journal of the Korean institute of surface engineering
    • /
    • v.53 no.3
    • /
    • pp.109-115
    • /
    • 2020
  • In this study, polycrystalline diamond was synthesized by chemical vapor deposition (CVD). Diamond films were deposited on a-plane sapphire substrates while changing the concentration of methane for hydrogen (CH4/H2), and the concentrations of methane were 0.25, 0.5, 1, 2, 3 and 4 vol%, respectively. Crystallinity and nucleation density according to changes in methane concentration were investigated. At this time, the discharge power, vacuum pressure, and deposition time were kept constant. In order to deposit polycrystalline diamond, the sapphire substrate was etched with sulfuric acid and hydrogen peroxide (ratio 3:7), and the sapphire surface was polished for 30 minutes with 100 nm-sized nanodiamond particles. The deposited diamond thin film was analyzed by a scanning electron microscope (SEM), a Raman spectra, Atomic force microscope (AFM) and an X-ray diffractometer (XRD). By controlling the ratio of methane to hydrogen and performing appropriate pre-treatment conditions, a polycrystalline diamond thin film having excellent crystallinity and nucleation density was obtained.

Study on Anodizing at Constant Current for Sealing Treatment of Nano-diamond Powder (나노 다이아몬드 분말 봉공처리 적용을 위한 정전류에서의 알루미늄 양극산화 제조 연구)

  • Kang, Soo Young;Lee, Dae Won
    • Journal of Powder Materials
    • /
    • v.21 no.2
    • /
    • pp.114-118
    • /
    • 2014
  • In this study, an aluminum oxide layer for sealing treatment of nano-diamond powder was synthesized by anodizing under constant current. The produced pore size and oxide thickness were investigated using scanning electron microscopy. The pore size increased as the treatment time increased, current density increased, sulfuric acid concentration decreased, which is different from the results under constant voltage, due to a dissolution of the oxide layers. The oxide layer thickness by the anodizing increased as temperature, time, and current density increased. The results of this study can be applied to optimize the sealing treatment process of nano-diamond particles of 4-10 nm to enhance the resistances of corrosion and wear of the matrix.

Thermal conductivity characteristics of commercial heat exchange fluids applying diamond nano-powder (다이아몬드 나노분말을 적용한 상용 열교환 유체의 열전도도 특성)

  • Son, Kwun;Lee, Jung-Seok;Park, Tae-Hee;Park, Kweon-Ha
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.38 no.1
    • /
    • pp.1-7
    • /
    • 2014
  • Nanofluids, suspending nano-particles of various materials, have a good heat transfer characteristics compared with pure base fluids. For the reason, nanofluids have been considered as one of the measure to improve energy efficiency, and studied to apply on a working fluid of a high performance heat exchanger. This study tested thermal conductivities of nanofluids applying diamond nano-powder on DI water, ethylene glycol, and ethyl alcohol. Nanofluids are fabricated by matrix synthetic method, and the volume percent of diamond nano-powder contained in the base fluid are 0.1, 0.3, 0.5, and 1vol%. As a result, thermal conductivities are enhanced with applying diamond nano-power. Especially, the conductivity is highly increased up to 23% at 1vol% nanofluid applying diamond nano-powder on DI water.

Nano-scale Patterning on Diamond substrates using an FIB (FIB를 이용한 다이아몬드 기판 위의 나노급 미세 패턴의 형상 가공)

  • Song, Oh-Sung;Kim, Jong-Ryul
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.7 no.6
    • /
    • pp.1047-1055
    • /
    • 2006
  • We patterned nano-width lines on a super hard bulk diamond substrate by varying the ion beam current and ion beam sources with a dual beam field ion beam (FIB). In addition, we successfully fabricated two-dimensional nano patterns and three-dimensional nano plate modules. We prepared nano lines on a diamond and a silicon substrate at the beam condition of 30 kV, 10 pA $\sim$ 5 nA with $Ga^+$ ion and $H_2O$ assisted ion sources. We measured each of the line-width, line-depth, etched line profiles, etch rate, and aspect ratio, and then compared them. We confirmed that nano patterning was possible on both a bulk diamond and a silicon substrate. The etch rate of $H_2O$ source can be enhanced about two times than that of Ga source. The width of patterns on a diamond was smaller than that on a silicon substrate at the same ion beam power The sub-100 nm patterns on a diamond were made under the charge neutralization mode to prevent charge accumulation. We successfully made a two-dimensional, 240 nm-width text of the 300-lettered Lord's Prayer on a gem diamond with 30 kV-30 pA FIB. The patterned text image was readable with a scanning electron microscope. Moreover, three dimensional nano-thick plate module fabrication was made successfully with an FIB and a platinum deposition, and electron energy loss spectrum (EELS) analysis was easily performed with the prepared nano plate module.

  • PDF