Thermal aging effect on fracture toughness of GTAW/SMAW of 316L stainless steel: experiments and applicability of existing CASS models

  • Youn, Gyo-Geun;Kim, Yun-Jae;Miura, Yasufumi
    • Nuclear Engineering and Technology
    • /
    • 제53권4호
    • /
    • pp.1357-1368
    • /
    • 2021
  • This paper presents thermal aging effect on fracture toughness properties of GTAW (gas tungsten arc welding) and SMAW (shielded metal arc welding) of 316L stainless steels, and investigates the applicability of the existing three thermal aging models for CASS (cast stainless steels). Thermal aging was carried out at 350 ℃ for up to 15,000h and at 400 ℃ up to 8,000h. After aging, tensile and fracture toughness tests using 0.5T C(T) specimens were carried out at room temperature and at 288 ℃. Comparing with the predictions using three (ANL, French and H3T) thermal aging models for CASS show that the predictions can be very non-conservative at operating temperature, and thus that the existing thermal aging models for CASS cannot be applied to the welded stainless steels.

AISI 316L 클래드강의 맞대기 용접부 입계부식과 예민화 거동에 관한 연구 (The Sensitization and Intergranular Corrosion Behavior of AISI 316L Clad Steel with Butt Welding)

  • 이철구;박재원
    • Journal of Welding and Joining
    • /
    • 제31권2호
    • /
    • pp.49-56
    • /
    • 2013
  • We have investigated traits of clad metals in hot-rolled clad steel plates, sensitization and mechanical properties of STS 316 steel plate and carbon steel(A516). Clad steel plates were butt-weld by SAW+SMAW, and with the time of heat treatment as the variable, heat treatment was conducted at $625^{\circ}C$, for 80, 160, 320, 640, 1280 minutes. As a way to evaluate it, sectioned weldments and external surfaces were investigated to reveal the degree of sensitization by mechanical property, etching and those of EPR test, results were compared with it. In short, the purpose of this study is suggesting some considerations in developing on-site techniques to evaluate the sensitization of stainless steels.

스테인리스강 용접부의 기계적 성질에 미치는 후열처리의 영향 (The influence of post weld heat treatment on mechanical properties of stainless steel weldment)

  • 한종만;한기형;이은배;허만주;한용섭
    • Journal of Welding and Joining
    • /
    • 제14권3호
    • /
    • pp.75-85
    • /
    • 1996
  • In this paper the influence of postweld heat treatment on mechanical properties of SMAW and FCAW stainless steel weldments was examined and the obtained results are as follows ; (1) The amount of $\delta$-ferrite formed by SMAW and FCAW process decreased with increasing holding temperature and time in post weld heat treatment(PWHT), and it was found that the reduced ferrite was transformed into sigma phase after $800^{circ}C{\times}50hr$ PWHT. This sigma phase, even though it was very small, resulted in brittleness of dissimilar weldment between carbon steel and stainless steel in bending test, however in similar weldment between stainless steel and stainless steel was not occured. (2) The chemical composition of sigma phase was measured to 28-30%Cr, 7-9%Mo, 4-6Ni in 316L weldment, and also 35-37%Cr, 0.9-1.0Mo, 6-8%Ni in 309L weldment by EDS analysis.

  • PDF

중성자 회절법에 의한 316L 스테인리스강 배관 다층용접부의 잔류응력 해석 (Analysis of Residual Stresses for the Multipass Welds of 316L Stainless Steel Pipe by Neutron Diffraction Method)

  • 김석훈;이재한
    • Journal of Welding and Joining
    • /
    • 제21권6호
    • /
    • pp.64-70
    • /
    • 2003
  • Multipass welds of the 316L stainless steel have been widely employed in the pipes of Liquid Metal Reactor. Owing to localized heating and subsequent rapid cooling by the welding process, the residual stress arises in the weld of the pipe. In this study, the residual stresses in the 316L stainless steel pipe welds were calculated by the finite element method using ANSYS code. Also, the residual stresses both on the surface and in the interior of the thickness were measured by HRPD(High Resolution Powder Diffractometer) instrumented in HANARO Reactor. The experimental data and the calculated results were compared and the characteristics of the distribution of the residual stress discussed.

Heat input effects on microstructure quenched and tempered steel ASTM A517 to stainless steel AISI 316L

  • Pezeshkian, Rouhollah Mohsen;Shafaiepour, Saiedeh
    • Journal of Welding and Joining
    • /
    • 제33권1호
    • /
    • pp.41-48
    • /
    • 2015
  • In this study, the effect of heat input on weld metal microstructure and the effects of dissimilar weld heat affected zone in quenched and tempered ASTM A517 on the stainless steel AISI 316L is investigated through the optimization of welding parameters. For this purpose, two welding techniques are used, tungsten-conventional gas and pulsed gas with weld wire ER 309MoL with Diameter 2.4 mm. Research showed that the grain size of the heat affected zone in pulsed welding is less compared with conventional welding; weld metal structure is fully austenitic, it has a finer structure in the pulsed method. Additionally, the growth of weld metal adjacent steel A517 is different from steel 316L. Further, investigation showed that the rate of dilution is less in the pulsed method and the impact energy is increased in each three regions of the weld metal and heat affected zones in the pulsed method; the fracture in the weld metal and heat affected zone of steel 316L is quite soft and it is semi-crispy in the heat affected zone of steel A517.

Tensile and impact toughness properties of various regions of dissimilar joints of nuclear grade steels

  • Karthick, K.;Malarvizhi, S.;Balasubramanian, V.;Krishnan, S.A.;Sasikala, G.;Albert, Shaju K.
    • Nuclear Engineering and Technology
    • /
    • 제50권1호
    • /
    • pp.116-125
    • /
    • 2018
  • Modified 9Cr-1Mo ferritic steel is a preferred material for steam generators in nuclear power plants for their creep strength and good corrosion resistance. Austenitic stainless steels, such as type 316LN, are used in the high temperature segments such as reactor pressure vessels and primary piping systems. So, the dissimilar joints between these materials are inevitable. In this investigation, dissimilar joints were fabricated by the Shielded Metal Arc Welding (SMAW) process with Inconel 82/182 filler metals. The notch tensile properties and Charpy V-notch impact toughness properties of various regions of dissimilar metal weld joints (DMWJs) were evaluated as per the standards. The microhardness distribution across the DMWJs was recorded. Microstructural features of different regions were characterized by optical and scanning electron microscopy. Inhomogeneous notch tensile properties were observed across the DMWJs. Impact toughness values of various regions of the DMWJs were slightly higher than the prescribed value. Formation of a carbon-enriched hard zone at the interface between the ferritic steel and the buttering material enhanced the notch tensile properties of the heat-affected-zone (HAZ) of P91. The complex microstructure developed at the interfaces of the DMWJs was the reason for inhomogeneous mechanical properties.