• Title/Summary/Keyword: Ultrasonic spray pyrolysis

Search Result 122, Processing Time 0.028 seconds

The Characteristics of Silica Powders Prepared by Spray Pyrolysis Applying Droplet Classification Apparatus (액적 분급 장치를 적용한 분무열분해 공정으로부터 합성된 실리카 분말의 특성)

  • Kang, Yun-Chan;Ju, Seo-Hee;Koo, Hye-Young;Kang, Hee-Sang;Park, Seung-Bin
    • Korean Journal of Materials Research
    • /
    • v.16 no.10
    • /
    • pp.633-638
    • /
    • 2006
  • Silica powders with spherical shape and narrow size distribution were prepared by large-scale ultrasonic spray pyrolysis applying the droplet classification apparatus. On the other hand, silica powders prepared by large-scale ultrasonic spray pyrolysis without droplet classification apparatus had broad size distribution. Droplet classification apparatus used in this paper applied the principles of cyclone and dispersion plate with small holes. The droplets formed from the ultrasonic spray generator applying the droplet classification apparatus had narrow size distribution. The droplets with fine and large sizes were eliminated by droplet classification apparatus. The optimum flow rate of the carrier gas and diameter of the hole of the dispersion plate were studied to reduce the size distribution of the silica powders prepared by large-scale ultrasonic spray pyrolysis. The size distribution of the silica powders prepared by large-scale ultrasonic spray pyrolysis at the optimum preparation conditions was 0.76.

Preparation of Multicomponent Ceramic Powders by Ultrasonic Spray Pyrolysis

  • Youn, Jeong-Han;Chung, Byung-Joo;Sim, Soo-Man
    • The Korean Journal of Ceramics
    • /
    • v.6 no.1
    • /
    • pp.58-63
    • /
    • 2000
  • The preparation of Y-doped $SrZrO_3$powder by ultrasonic spray pyrolysis was investigated as a representative system, in order to produce fine, single phase multicomponent oxide powders. A precursor solution containing metal nitrates, citric acid and ethylene glycol was atomized glycol was atomized with an ultrasonic spray nozzle. Gel particles formed by organic functional groups were pyrolyzed and subsequently calcined at $800^{\circ}C$ to obtain well-crystallized, single perovskite phase. Most of large particles exhibited macroscopic pores and weak agglomeration between primary particles. However, strong agglomeration was observed in the surfaces of large particles. The effect of the microstructures of these particles on size reduction to submicron particles was described.

  • PDF

Synthesis of Ceria Nanosphere by Ultrasonic Spray Pyrolysis

  • Kim, Jong-Young;Kim, Ung-Soo;Cho, Woo-Seok
    • Journal of the Korean Ceramic Society
    • /
    • v.46 no.3
    • /
    • pp.249-252
    • /
    • 2009
  • Nanocrystalline ceria particles were prepared by using the ultrasonic spray pyrolysis method. The prepared ceria particles were found to be spherical and non-agglomerated by the SEM and TEM analyses. It was found that carrier gas influences the size and morphology. It was found that the air stream of carrier gas results in porous agglomerated structure of ceria abrasives, whereas solid nano-sphere can be obtained in a more oxidizing atmosphere.

Synthesis of Homogeneous La0.8Sr0.2CrO3 Powders Using an Ultrasonic Spray Pyrolysis Method

  • Kim, Chang-Sam;Hwang, Seong-Ik;Kim, Shin-Woo
    • Journal of the Korean Ceramic Society
    • /
    • v.44 no.5 s.300
    • /
    • pp.148-150
    • /
    • 2007
  • A process to synthesize $La_{0.8}Sr_{0.2}CrO_3$ (LSC), which is a promising material for use as a separator in a soild oxide fuel cell, is investigated in this study. LSC powders without secondary Phases could be synthesized with ultrasonic spray pyrolysis and a heat treatment at $1200^{\circ}C$ for 20 h; however, it showed an average diameter of $0.6{\mu}m$ with a wide particle size distribution. On the other hand, LSC powders synthesized with spray pyrolysis at $800^{\circ}C$, heat-treated at $900^{\circ}C$ for 5 h, ball-milled and finally heat-treated again at $1200^{\circ}C$ for 20 h showed a smaller average diameter of $0.3{\mu}m$ and narrower size distribution. Very few particles above $0.5{\mu}m$ were found. Thus, a proper combination of the heat treatment and milling process after spray pyrolysis it determined to be very important in synthesizing fine and uniform LSC perovskite powders.

Direct Preparation of fine Powders of Bi-Pb-Sr-Ca-Cu-O by Ultrasonic Spray Pyrolysis (초음파 분무열분해에 의한 Bi-Pb-Sr-Ca-Cu-O의 미분체 제조)

  • 주명희;박도순;김윤수
    • Journal of the Korean Ceramic Society
    • /
    • v.28 no.5
    • /
    • pp.353-358
    • /
    • 1991
  • Fine powders of the 2212 superconducting phase of bismuth system have been prepared directly from solution using ultrasonic spray pyrolysis. The fine superconducting powders produced by pyrolysis were characterized for the size, shape, and crystalline phase by SEM and XRD. The pyrolysis temperature, flow rate of the carrier gas, residence time of the droplets greatly influenced the size, shape, and crystalline phase. The optimum temperature and flow rate of the carrier gas for the preparation of fine powders of the 2212 superconduting phase were found to be 830$^{\circ}C$and 3ι/min, respectively.

  • PDF

Characterization of Spherical NiO-YSZ Anode Composites for Solid Oxide Fuel Cells Synthesized by Ultrasonic Spray Pyrolysis

  • Lim, Chae-Hyun;Lee, Ki-Tae
    • Journal of the Korean Ceramic Society
    • /
    • v.51 no.4
    • /
    • pp.243-247
    • /
    • 2014
  • Spherical NiO-YSZ particles were synthesized by ultrasonic spray pyrolysis (USP). The morphology of the synthesized particles can be modified by controlling parameters such as precursor pH, carrier-gas flow-rate, and temperature of the heating zone. The synthesized spherical NiO-YSZ particles have rough surface morphology at high carrier-gas flow-rates due to rapid gas exhaustion and insufficient particle ordering. The Ni-YSZ cermet anode synthesized by ultrasonic spray pyrolysis at a flow rate of l L/min, with precursor solution at pH4, showed a higher maximum power density of 256 $mW/cm^2$ compared to a conventionally mixed Ni-YSZ anode (185 $mW/cm^2$) at $800^{\circ}C$. While the area-specific resistance of conventionally mixed Ni-YSZ anodes increases gradually with operation time (indicating performance degradation), the Ni-YSZ anode synthesized by USP does not exhibit any performance degradation, even after 500 h.

Spherical Bi2Te3 Powder Synthesized by Oxide-Reduction Process via Ultrasonic Spray Pyrolysis (초음파 분무 열분해법에 의한 산화물 환원 공정의 구형 Bi2Te3 분말 합성)

  • Song, Chul-Han;Jang, Dae-Hwan;Jin, Yun-Ho;Kong, Man-Sik
    • Journal of the Korean institute of surface engineering
    • /
    • v.50 no.2
    • /
    • pp.114-118
    • /
    • 2017
  • Bismuth telluride ($Bi_2Te_3$) and its alloys are well-known thermoelectric materials for ambient temperature applications. In this study, the dissolved Bi-Te precursor solution was used to synthesis metallic $Bi_2Te_3$ powder via ultrasonic spray pyrolysis and reduction process. The droplets of the Bi-Te precursor solution were decomposed to Bi-Te oxide powders by ultrasonic spray pyrolysis. The spherical $Bi_2Te_3$ powders were synthesized by reduction reaction in atmosphere of hydrogen gas at the temperature above $375^{\circ}C$ for 6h. The reduced $Bi_2Te_3$ powders have a mean particle size of $1.5{\mu}m$. The crystal structure of the powder was evaluated by X-Ray diffraction(XRD), and the microstructure with size and shape powders was observed by fieldemission scanning electron microscope(FE-SEM) and transmission electron microscope(TEM).

Effect of annealing on the magnetic behavior and microstructures of spherical NiZn ferrite particle prepared by ultrasonic spray pyrolysis

  • Nam, Joong-Hee
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.17 no.1
    • /
    • pp.11-17
    • /
    • 2007
  • The spherical NiZn ferrite particles were prepared by ultrasonic spray pyrolysis with mixed solution of aqueous metal nitrates. The NiZn ferrite particle was observed with nano-sized primary particles of about 10 nm or less before annealing which represented as paramagnetic behavior measured at 77 K and room temperature. The typical abnormal growth of primary particles like polyhedral primary particles was observed by annealing at 1273 K with Zn-concentration dependency. The XRD patterns showed good crystallinity of NiZn ferrite powder after annealing. In annealing process, the intra-particle sintering phenomenon was observed and the spherical particle morphology was collapsed at 1673 K. The saturation magnetization of NiZn ferrite powder for each annealing temperature was decreased with measuring temperature of $77{\sim}$300K.

The properties of ZnO/MgO films prepared by ultrasonic spray pyrolysis (초음파분무법으로 제조한 ZnO/MgO막의 특성)

  • Choi, Mu-Hee;Ma, Tae-Young
    • Journal of Sensor Science and Technology
    • /
    • v.14 no.5
    • /
    • pp.362-367
    • /
    • 2005
  • ZnO films were deposited on MgO substrates (ZnO/MgO) by ultrasonic spray pyrolysis. Substrate temperature varied from $250^{\circ}C$ to $350^{\circ}C$. The crystallographic properties and surface morphologies of the ZnO/MgO films were studied by X-ray diffraction and scanning electron microscopy. The properties of photoluminescence (PL) for the films were investigated by dependence of PL spectra on the substrate temperature and the annealing temperature. The ZnO/MgO films prepared at $350^{\circ}C$ showed the strongest Ultraviolet light emission peak at 18 K and 300 K among the films in this study. The annealing process increases the visible light emission, which is due to the increased oxygen vacancies.

Preparation of Iron Oxide-mixed ZnO films by Ultrasonic Spray Pyrolysis (초음파분무법을 이용한 산화철이 혼합된 ZnO막의 제조)

  • Choi Mu-Hee;Ma Tae-Young
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.19 no.1
    • /
    • pp.58-63
    • /
    • 2006
  • In this Paper, ZnO films mixed with iron oxide were prepared by an ultrasonic spray pyrolysis method. The chemical composition and structural properties as a function of the Fe atomic ratio in the deposition solution were studied. Zinc acetate and ferrous chloride were used as precursors of Zn and Fe, respectively. Fe atomic ratio to Zn varied from 0.15 to 10.0. Substrate temperature was fixed at $250^{\circ}C$. The crystallographic properties and surface morphologies of the films were studied by X-ray diffraction (XRD) and scanning electron microscopy (SEM), respectively. Electron probe X-ray microanalysis (EPMA) and X-ray photoelectron spectroscopy (XPS) were carried out to analyse the chemical composition and state of Zn and Fe atoms.