• 제목/요약/키워드: Uni-axial tensile test

검색결과 13건 처리시간 0.028초

C-Mn-Si계 변태유기소성강의 성형성에 미치는 베이나이트 변태온도 및 응력상태의 영향 (Effects of Bainitic Transformation Temperature and Stress State on the Formability of C-Mn-Si TRIP Steels)

  • 전현조;오진후;박찬경
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.156-160
    • /
    • 2001
  • The effects of TRansformation Induced Plasticity(TRIP) phenomena on the plastic deformation of 0.2C-1.5Si-1.5Mn multiphase steels have been investigated at various heat treatment and stress conditions. In order to estimate the formability, the hole expansion(HE) tests and the tensile tests were carried out. The formability evaluated from the uni-axial tensile tests was quite different from the formability measured from multi-axial HE-tests. Consequently, the formability in the multi-axial stress state decreased due to the extinction of the retained austenite relatively at earlier deformation stage and the production of irregular α' martensite. However, the defects of TRIP-steels were initiated exactly at the boundary between transformed martensite and ferrite matrix regardless of stress state. In addition, new experimental formula is proposed in order to predict the multi-axial formability of the TRIP steels from the results of uniaxial tensile test.

  • PDF

알루미늄 6061 압출재의 제조공정에 따른 온간액압성형성과 기계적 특성 연구 (Hydroformability and mechanical properties of A16061 tubes on different extrusion type)

  • 이혜경;장정환;권승오;이영선;문영훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 춘계학술대회 논문집
    • /
    • pp.254-257
    • /
    • 2007
  • In this study, hydroformability and mechanical properties of pre- and post- heat treated Al6061 tubes at different extrusion type were investigated. For the investigation, as-extruded, full annealed and T6-treated Al 6061 tubes at different extrusion type were prepared. To evaluate the hydroformability, uni-axial tensile test and free bulge test were performed at room temperature and $200^{\circ}C$. Also mechanical properties of hydroformed part at various pre- and post-heat treatments were estimated by tensile test. And the tensile test specimens were obtained from hexagonal prototype hydroformed tube at $200^{\circ}C$. As for the heat treatment, hydroformability of full annealed tube is 25% higher than that of extruded tube. The tensile strength and elongation were more than 330MPa and 12%, respectively, when hydroformed part was post-T6 treated after hydroforming of pre- full annealed tube. However, hydroformed part using T6 pre treated tube represents high strength and low elongation, 8%. Therefore, the T6 treatment after hydroforming for as-extruded tube is cost-effective. Hydroformability of Al6061 tube showed similar value for both extrusion types. But flow stress of seam tube showed $20{\sim}50MPa$ lower value.

  • PDF

온간액압성형특성에 미치는 압출제조공정과 열처리 조건의 영향 (Effect of process type and heat treatment conditions on warm hydroformability)

  • 이혜경;권승오;박현규;임홍섭;이영선;문영훈
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2007년도 추계학술대회 논문집
    • /
    • pp.132-135
    • /
    • 2007
  • In this study, hydroformability and mechanical properties of pre- and post- heat treated Al6061 tubes at different extrusion type were investigated. For the investigation, as-extruded, full annealed and T6-treated Al6061 tubes at different extrusion type were prepared. To evaluate the hydroformability, uni-axial tensile test and free bulge test were performed at room temperature and $250^{\circ}C$. Also mechanical properties of hydroformed part at various pre- and post-heat treatments were estimated by tensile test. And the tensile test specimens were obtained from hexagonal prototype hydroformed tube at $250^{\circ}C$. As for the heat treatment, hydroformability of full annealed tube is 25% higher than that of extruded tube. The tensile strength and elongation were more than 330MPa and 12%, respectively, when hydroformed part was post-T6 treated after hydroforming of pre- full annealed tube. However, hydroformed part using T6 pre treated tube represents high strength and low elongation, 8%. Therefore, the T6 treatment after hydroforming for as-extruded tube is cost-effective. Hydroformability of Al6061 tube showed similar value for both extrusion types. But flow stress of seam tube showed $20{\sim}50MPa$ lower value.

  • PDF

Al6061압출재를 이용한 온간액압성형품의 성형성 및 물성에 미치는 열처리조건의 영향 (Effect of Heat Treatment Conditions on Formability and Property of Warm Hydroformed Parts for Al 6061 Extruded Tube)

  • 이혜경;권승오;장정환;이영선;문영훈
    • 열처리공학회지
    • /
    • 제20권4호
    • /
    • pp.181-186
    • /
    • 2007
  • Effect of heat treatment conditions on formability and property of warm hydroformed parts for Al 6061 extruded tubes was investigated in this study. For the investigation, as-extruded, fully annealed and T6-treated Al 6061 seamless tubes were prepared. To evaluate the warm hydroformability, uni-axial tensile test and free bulge test were performed at various pre- and post-heat treatment conditions. And the tensile test specimens were obtained from hexagonal prototype hydroformed parts at $250^{\circ}C$. As a result, hydroformability of fully annealed tube is 25% higher than that of extruded tube. The tensile strength and strain of hydroformed part reach to 330 MPa and 12%, respectively, when the part was T6 treated after warm hydroforming. However, the hydroformability of T6 pre-treated tube is relatively low due to the decreased elongation, 8%.

자동차용 합금화 용융아연도금강판의 도금층 미소물성 및 파괴 거동 (Microproperties and Fracture Behavior of Galvannealed Coating Layer of Automobiles)

  • 박춘달;고대철;김병민
    • 한국정밀공학회지
    • /
    • 제24권3호
    • /
    • pp.91-99
    • /
    • 2007
  • Fractures of galvannealed coating layer during actual press forming in automotive applications were observed by scanning electron microscopy in order to understand fracture mechanism. Fracture behaviors of galvannealed coating layer in extra deep drawing quality steels and high strength steels have been studied by performing the tests describing the representative plastic deformation in sheet metal forming such as uni-axial tensile test, compression test, bi-axial test and plane strain test. Growth and direction of cracks were deeply related to the plastic deformation modes and history. The material properties of galvannealed coating layer were investigated by nano-indentation test equipped with Berkovich diamond indentor for the specimens. Hardness and elastic modulus of the coating layer were higher than bared steels and that was the reason for crack of coating layer. Flat friction test and drawbead friction test were performed to observe the effect of the surface morphology on the frictional characteristics. The micro-plasto hydrodynamic lubrication were appeared and played an important role in reducing the coefficient of friction.

Study of Al-Alloy Foam Compressive Behavior Based on Instrumented Sharp Indentation Technology

  • Kim Am-Kee;Tunvir Kazi
    • Journal of Mechanical Science and Technology
    • /
    • 제20권6호
    • /
    • pp.819-827
    • /
    • 2006
  • The stress-strain relation of aluminum (Al) alloy foam cell wall was evaluated by the instrumented sharp indentation method. The indentation in a few micron ranges was performed on the cell wall of Al-alloy foam having a composition or Al-3wt.%Si-2wt.%Cu-2wt.%Mg as well as its precursor (material prior to foaming). To extract the stress-stram relation in terms of yield stress ${\sigma}_y$, strain hardening exponent n and elastic modulus E, the closed-form dimensionless relationships between load-indentation depth curve and elasto-plastic property were used. The tensile properties of precursor material of Al-alloy foam were also measured independently by uni-axial tensile test. In order to verify the validity of the extracted stress-strain relation, it was compared with the results of tensile test and finite element (FE) analysis. A modified cubic-spherical lattice model was proposed to analyze the compressive behavior of the Al-alloy foam. The material parameters extracted by the instrumented nanoindentation method allowed the model to predict the compressive behavior of the Al-alloy foam accurately.

연성파괴 이론을 적용한 튜브 온간액압성형의 성형한계 예측 (Prediction for Forming Limit of Tube Warm Hydroforming Based on the Ductile Fracture Criteria)

  • 이혜경;문영훈;이정환;이영선
    • 소성∙가공
    • /
    • 제16권6호
    • /
    • pp.426-431
    • /
    • 2007
  • Hydroformability and fracture criteria of FE analysis based on ductile fracture were investigated in warm hydroforming of A16061 tube. To evaluate the hydroformability, uni-axial tensile test and bulge test were performed at room temperature and $200^{\circ}C$. The measured flow stresses were used as input parameters for FE analysis. The damage values were calculated by FE analysis based on ductile fracture criteria at maximum radius of free bulged tubes. Damage values were compared of hexagonal shaped hydroformed parts. As a result, the formability by critical damage value for extruded tube is lower than that of full annealed tube up to 0.5.

부식이 존재하는 기존 노후 관로에서 인장 시편 가공 시 그립 가공 타당성에 대한 연구 (Validation Study on Processing Grip Part of Tensile Specimen Acquired from Corroded Pipeline)

  • 남영준;김정현;배철호;임윤묵
    • 대한토목학회논문집
    • /
    • 제40권2호
    • /
    • pp.191-195
    • /
    • 2020
  • 부식된 관로의 상태를 평가하기 위해서 수행하는 직접평가 중 인장 실험을 수행하였다. 부식된 관로에서 절삭 가공하여 인장 시편을 취득하면, 관로의 관경에 따라 곡률이 변화하고 실제 평평한 시편의 거동과 달라질 수 있어 이를 확인하기 위한 연구를 수행하였다. 시편의 전 영역이 평평한 경우, 곡률이 있는 경우 그리고 시편에 곡률이 존재하면서 그립 부분만 평평하게 가공한 경우에 대해서 부식이 없는 경우와 부식이 존재하는 경우(두께 대비 25, 50 %의 단일 부식)로 나누어 해석을 진행하였다. 부식이 존재하게 되면 응력 집중이 단면 감소부에서 확실하게 나타나 그립의 가공 여부가 시편의 인장거동에 영향을 거의 주지 않는다는 것을 해석을 통해 확인하였다. 또한 실제 부식이 있는 시편에 대하여 3D 스캔을 진행하고 이를 반영한 해석 모델을 만들어 실험 결과와 비교 분석하였다.

Cu첨가 극저탄소 고 강도강의 가공성에 미치는 Al과 B의 영향 (Effect of Aluminium and Boron on Formability for Cu Bearing Extra Low Carbon Steel Sheets)

  • 김성일;정경환;홍문희
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 춘계학술대회 논문집
    • /
    • pp.302-305
    • /
    • 2009
  • This paper examines the effect of nitride formation on formability for Cu bearing high strength extra low carbon (ELC) steel sheets. For this purpose, we have investigated the effect of addition of aluminium (Al) and boron (B) on texture and precipitation behavior of the ELC steel during continuous annealing. Mechanical properties and microstructures of the ELC steel sheets were analyzed as well using uni-axial tensile test, electron back-scattered diffraction (EBSD) technique and transmission electron microscopy (TEM) following pilot rolling and continuous annealing. It has been found that the addition of Al and B increases the precipitation of AlN and BN. What is more, the scavange of solute nitrogen is effective in increasing the formability of the ELC steels. In addition, the Al and B addition improves the aging property of the ELC steel.

  • PDF