• Title/Summary/Keyword: air-dry density

Search Result 92, Processing Time 0.029 seconds

Determination of Air-dry Density of Wood with Polychromatic X-ray and Digital Detector

  • Kim, Chul-Ki;Kim, Kwang-Mo;Lee, Sang-Joon;Lee, Jun-Jae
    • Journal of the Korean Wood Science and Technology
    • /
    • v.45 no.6
    • /
    • pp.836-845
    • /
    • 2017
  • Gravimetric method is usually used to evaluate air-dry density, which is governing physical or mechanical properties of wood. Although it had high evaluation accuracy, the method is time consuming process. Thus, this study was conducted to estimate air-dry density of wood with high accuracy by using polychromatic X-ray and digital detector as alternative of gravimetric method. To quantify polychromatic X-ray projection for evaluating air-dry density, Lambert-Beer's law with the integral value of probability function was used. The integral value was used as weighting factor in the law, and it was determined by conducting simple test at various penetration depths and tube voltage. Mass attenuation coefficient (MAC) of wood also calculated by investigating polychromatic X-ray projection according to species, penetration depth and tube voltage. The species had not an effect on change of MAC. Finally, an air-dry density of wood was estimated by applying the integral value, MAC and Lambert-Beer's law to polychromatic X-ray projection. As an example, the relation of the integral value (${\alpha}$) according to penetration depth (t, cm) at tube voltage of 35 kV was ${\alpha}=-0.00091t{\times}0.0184$ while the regression of the MAC (${\mu}$, $cm^2/g$) was ${\mu}=0.5414{\exp}(-0.0734t)$. When calculation of root mean squared error (RMSE) was performed to check the estimation accuracy, RMSE at 35, 45 and 55 kV was 0.010, 0.013 and $0.009g/cm^3$, respectively. However, partial RMSE in relation to air-dry density was varied according to tube voltage. The partial RMSE below air-dry density of $0.41g/cm^3$ was $0.008g/cm^3$ when tube voltage of 35 kV was used. Meanwhile, the partial RMSE above air-dry density of $0.41g/cm^3$ decreased as tube voltage increased. It was conclude that the accuracy of estimation with polychromatic X-ray and digital detector was quite high if the integral value and MAC of wood were determined precisely or a condition of examination was chosen properly. It was seemed that the estimation of air-dry density by using polychromatic X-ray system can supplant the gravimetric method.

Anatomical Characteristics and Air-dry Density of Young Trees of Teak Clones Planted in Indonesia

  • Hidayati, Fanny;Ishiguri, Futoshi;Marsoem, Sri Nugroho
    • Journal of the Korean Wood Science and Technology
    • /
    • v.45 no.4
    • /
    • pp.463-470
    • /
    • 2017
  • The objectives of this study are to obtain the basic knowledge of anatomical characteristics and wood properties of thinning trees of young teak (Tectona grandis L.F.) for fulfill the timber demand in Indonesia. Nine thinning trees of 5-year-old teak clone trees were used for analyzing the cell morphology and air-dry density. Vessel diameters in pore and outer pore zones were 165 and $90{\mu}m$, respectively. Mean value of fiber diameter, cell wall thickness, and fiber length in outer pore zone were $14.6{\mu}m$, $2.07{\mu}m$, and 1.04 mm, respectively. In addition, mean value of air-dry density was $0.55g/cm^3$. The measurement and values of vessel diameter, fiber diameter, cell wall thickness, fiber length and air-dry density in the experimental had lower than those in the older teak. Therefore, it could be suggested that the wood from thinning young teaks was not appropriate as construction material, but it could be used for furniture which do not need high of strength properties. Furthermore, since the measurements values of anatomical characteristics were still increasing from pith to bark, it could be suggested that 5-year-old teak clones are still in a juvenile phase. Positively significant correlations were found between air-dry density and cell wall thickness, indicating that cell wall thickness is strongly correlated with wood density of teak.

Moist Air Density Calculation for Air Condition (공기 상태량에 대한 습공기 밀도 계산)

  • Kim, Jong-Woo
    • Transactions of the KSME C: Technology and Education
    • /
    • v.2 no.2
    • /
    • pp.105-111
    • /
    • 2014
  • Generally the lower part of the Earth's atmosphere, which is 20km above the ground, is called "air." The composition of this area is almost consistent consisting of nitrogen, oxygen, and other gases. Air density refers to the mass per unit volume of earth atmosphere. Though air is made of the mixed gases in a constant composition, the water vapor is one of the very changeable components. The density of moist air is lower than the dry one at the same temperature and pressure. As the density varies according to the pressure and temperature, this paper attempts to explore the main factors in the air quantity calculation by examining first the density calculation process according to the air property, and second the relation between the actual and standard air flow.

Effect of Moisture Contents and Density of Paulownia tomentosa on Acoustical Properties (함수율과 밀도가 참오동나무재의 음향 특성에 미치는 영향)

  • Yoo, Tae-Kyung;Jung, Hee-Suk
    • Journal of the Korean Wood Science and Technology
    • /
    • v.25 no.2
    • /
    • pp.61-66
    • /
    • 1997
  • Paulownia wood has been used as sound board for Korean traditional musical instruments such as Keomungo(Korean lute), Kayagum(twelve-stringed Korean harp) and Changgu(hour-glass shaped drum), etc. The acoustic properties of wood affected not only by dimensions but also by density and stiffness of wood. Due to inhomogeneity and hygroscopicity of wood. the acoustic properties of wood are inconsistent. To clarify the effect of moisture content and air dry density on acoustic properties, longitudinal vibration experiment was accomplished in 3 moisture content levels of 9.6, 11.1 and 12.5% and in 3 air dry density levels of 0.22, 0.25 and 0.28g/$cm^3$. The results were as follows: As the moisture content increased, the fundamental frequency. specific dynamic Young's modulus and sound velocity decreased, but the internal friction increased so that loss of energy increased. The values in damping of sound radiation were rapidly decreased at 12.5%. It meant that the damping of internal friction was larger than damping of sound radiation at high moisture content. As the air dry density increased, the fundamental frequency, specific dynamic Young's modulus and sound velocity increased, but the internal friction and damping of sound radiation decreased so that loss of energy decreased. And acoustic converting efficiency was hardly influenced by increasing air drying density.

  • PDF

Evaluation of Methods for Determination of Bulk Density of Eight Kinds of Forage under Air-dry and Wet Conditions

  • Sekine, J.;Kamel, Hossam E.M.;El-Seed, Abdel Nasir M.A. Fadel;Hishinuma, M.
    • Asian-Australasian Journal of Animal Sciences
    • /
    • v.16 no.8
    • /
    • pp.1126-1130
    • /
    • 2003
  • The conditions of measurement for the determination of bulk density were evaluated to assess the bulkiness of 8 kinds of forage. The bulkiness of the forages was determined with 4 different sizes of forage samples with 7 different pressure application under air-dry and wet conditions. The dry bulk density (DBD) curvilinearly regressed with the pressure applied. The particle size of the samples and kinds of forage used in the present study did not affect changes in values of DBD determined under pressures over $20g/cm^2$ up to $200g/cm^2$. The values of the wet bulk density (WBD) increased as an increment of particle size, but were not always regressed on the particle size of the 8 kinds of forage. The DBD determined on 8 mm particles showed a higher correlation coefficient with neutral detergent fiber (NDF) contents. The DBD may be a useful tool for the assessment of NDF in forage, when it is determined under condition of a pressure of $100g/cm^2$ or over with a particle size of 8 mm. The WBD may not be utilized for the direct measurement of the physical characteristics of forage, but may be required a thorough consideration on water solubility of forages. Further studies are needed to clarify the DBD contribution to the prediction of forage intake by ruminants.

Effect of Foam Volume ratio and Curing Temperature on Compressive Strength of Lightweight using Bottom Ash Aggregates (바텀애시 경량골재 콘크리트 압축강도에 대한 기포 혼입률 및 양생온도의 영향)

  • Lee, Kwang-Il;Yang, Keun-Hyeok
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2019.05a
    • /
    • pp.168-169
    • /
    • 2019
  • This study examined the effect of foam volume ratio and curing temperature the air dry density and compressive strength of lightweight concrete using bottom ash. Test results showed that the lightweight concrete possessed the compressive strength of 3.4~22.7 MPa at the air dry density of 1,041~1,583 kg/m3.

  • PDF

Fabrication of Mn-Zn Ferrite by Hot Petroleum Drying Method (석유증발 건조방법에 의한 Mn-Zn Ferrite의 제조에 관한 연구)

  • 변수일
    • Journal of the Korean Ceramic Society
    • /
    • v.16 no.2
    • /
    • pp.69-76
    • /
    • 1979
  • This study attempted to characterize the powder and sintered specimen of Mn-Zn ferrite that was prepared by Hot Petroleum Drying Method. The results of the experiment were as follows: 1. The mixed sulfate powder prepared by Hot Petroleum Drying Method was homogeneous and very reactive. The ferrite formation of this powder occurred at lower temperature than the one prepared by Sulfate Dry Mixing Method. 2. The calcined oxide powder prepared by Hot Petroleum Drying Method was found to be agglomerated, and therefore it was very difficult to compact this powder. 3. The sintered density was 4.95g/㎤, 97% of the theoretical density, when the specimen was prepared by Hot Petroleum Drying method, calcined at 90$0^{\circ}C$ in air for 3h, sintered at 1,30$0^{\circ}C$ in air for 3h, and then cooled in nitrogen. 4. The discontinuous grain growth occurred at lower temperature in the specimen prepared by Hot Petroleum Dyring Method than in the one prepared by Sulfate Dry Mixing Method. The discontinuous grain growth was considered to be due to the presence of liquid formed by addition of CaO and $SiO_2$.

  • PDF

Thermal Conductivity Measurement of Sand-Water Mixtures Used for Backfilling Materials of Vertical Boreholes or Horizontal Trenches (지중열교환기 수직 보어홀 및 수평 트렌치 뒤채움재로서 모래-물 혼합물의 열전도도 측정)

  • Sohn, Byong-Hu
    • Korean Journal of Air-Conditioning and Refrigeration Engineering
    • /
    • v.20 no.5
    • /
    • pp.342-350
    • /
    • 2008
  • This paper presents the results of a laboratory study on the thermal conductivity of sand (silica, quartzite, limestone and masonry sand)-water mixtures used in ground heat exchanger backfilling materials. Nearly 150 tests were performed in a thermal conductivity measuring system (TPSYS02) to characterize the relationships between the thermal conductivity of mixtures and the water content. The results show that the thermal conductivity of mixtures increases with increasing dry density and with increasing water content. The results also show that for constant water contents and a dry density value, the thermal conductivity of mixtures increases with increasing thermal conductivity of solid particles. The measurement results were also compared with the most widely used empirical prediction models for the thermal conductivity of soils.

Electrical Resistivity at Room Temperature and Relation between Physical Properties of Core Samples from Ulleung Island (울릉도 시추 코어의 상온 전기비저항과 물성 간의 상관성)

  • Lee, Tae Jong;Lee, Sang Kyu;Yun, Kwan-Hee
    • Geophysics and Geophysical Exploration
    • /
    • v.18 no.4
    • /
    • pp.171-180
    • /
    • 2015
  • Electrical resistivity of 23 core samples from Ulleung Island at dry or saturated condition has been measured along with dry density and effective porosity, and the relations between the properties has also been discussed. Upper and lower bounds of electrical resistivity at room temperature can be provided by the dry- and saturated-resistivity, respectively. Injecting nitrogen gas to the pore space at the very end of drying process can prevent humid air from getting into the pore space, so that measurement of dry-resistivity can be less affected by humidity in the air. Dry density and porosity have very close correlation; the ratio between increase of porosity and the decrease of density showed distinct relation to the rock types, such that basaltic rocks showed higher ratio while trachytic rocks showed lower. Saturated resistivity showed close correlation to density and effective porosity of the rock sample, while dry resistivity didn't.

Evaluation of Compressive Strength of Lightweight Aggregate Concrete using Bottom Ash Aggregates and Air Foam (기포가 혼입된 바텀애시 골재 경량 콘크리트의 압축강도 평가)

  • Lee, Kwang-Il;Yang, Keun-Hyeok
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2018.11a
    • /
    • pp.112-113
    • /
    • 2018
  • The present feasible tests are to develop the lightweight concrete using bottom ash aggregates and performed air foam for applying to sustainable high-insulation panel. The main variables investigated are water-to-binder, foam volume ratio, and curing conditions. Test results showed that the lightweight concrete possessed the compressive strength of 5~9 MPa at the air dry density of 951~1,139 kg/m3.

  • PDF