플라이애시와 슬래그 혼합 알칼리 활성 시멘트의 미세구조 특성 (Microstructural Characteristics of Alkali-Activated Cements Incorporating Fly Ash and Slag)

  • 장정국
    • 도시과학
    • /
    • 제7권1호
    • /
    • pp.39-43
    • /
    • 2018
  • This study investigates microstructural characteristics of alkali-activated cements incorporating slag and fly ash. Samples were prepared with four fly ash:slag ratios, i.e., 100:0, 90:10, 70:30 and 50:50, and they were synthesized by using an alkali activator. Microstructural characteristics of the alkali-activated cements were determined by XRD, TGA, SEM, N2 gas adsorption/desorption methods, and compressive strength test. The results showed that properties of alkali-activated fly ash/slag were significantly affected by slag contents. Alkali-activated fly ash/slag with slag content of 30-50% showed higher compressive strength than ordinary Portland cement paste. An increase in slag content resulted in a denser microstructure, which composed of amorphous gel, therefore contributed to strength development of the material.

Hydration Mechanism of Alkali Activated Slag Cement

  • Jong Cheol Kim;Keun Ho Auh;Sung Yun Hong
    • The Korean Journal of Ceramics
    • /
    • 제5권1호
    • /
    • pp.35-39
    • /
    • 1999
  • For many years, alkali activated blast furnace slag cement containing no ordinary portland cement has received much attention in the view of energy saving and its many excellent properties. We examined the structural change of slag glass which was activated by alkali metal compounds using IR spectroscopy. The properties of hydrated products and unhydrated slag grains was characterized by XRD and micro-conduction calorimeter. Ion concentration change in the liquid during the hydration of blast furnace slag was also studied to investigated the hydration mechanism.

  • PDF

활성제를 사용한 슬래그 미분말 혼합 모르타르의 강도 (Strength of Alkali-Activated GGBF Slag Mortar)

  • 문한영;신화철;권태석
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2001년도 봄 학술발표회 논문집
    • /
    • pp.481-486
    • /
    • 2001
  • Ground granulated blast-furnace slag shows very high strength when proper alkali-activator exists. This paper deals with setting time, heat evolution rate and the strength development of alkali-activated slag cement activated by KOH, Ca(OH$)_{2}$, $Na_{2}$ $So_{4}$ , and alum(potassium aluminum sulfate). Alkali-activated slag mortar is studied by comparison with GGBF slag cement mortar. The experimental results indicate that for moisture curing at $25^{\circ}C$, the addiction of either 4% $Na_{2}$ $So_{4}$ or 4% alum increases the strength of GGBF slag cement mortar consisting of 50% GGBF slag and 50% portland cement at early age. Strength of activated GGBF slag cement mortars at 1, 3 and 7 days exceeded that of GGBF slag cement mortar. A conduction calorimeter was used to monitor early age hydration.

  • PDF

알칼리활성화 슬래그-레드머드 흙포장재의 레드머드 대체율에 따른 백화 특성 (Efflorescence Characteristics of Alkali-Activated Slag-Red Mud Soil Mixed Pavement of Red Mud Substitution Rate)

  • 강혜주;이영원;오두연;이규영;강석표
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2015년도 추계 학술논문 발표대회
    • /
    • pp.153-154
    • /
    • 2015
  • This study is alkali-activated slag-red mud soil mixed pavement of efflorescence characteristics analysis of mitigation measures is drawn to the red mud substitution rate in accordance with the alkali-activated slag-red mud soil mixed pavement of efflorescence characteristics were exhibited. As a result of alkali-activated slag-red mud soil mixed pavement is more substitution rate increases appeared to efflorescence is increased.

  • PDF

알칼리 활성화 슬래그 시멘트 모르타르의 내황산성 (Resistance of Alkali Activated Slag Cement Mortar to Sulfuric Acid Attack)

  • 민경산;이승헌
    • 한국세라믹학회지
    • /
    • 제44권11호
    • /
    • pp.633-638
    • /
    • 2007
  • The setting time of alkali activated slag cement tends to be much faster than ordinary Portland cement, and its compressive strength had been higher from the 1 day but became lower than that of the cement on the 28 days. According to the results of the surface observation, weight loss, compressed strength, and erosion depth tests on the sulphuric acid solution. It has been drawn that alkali activated slag cement has a higher sulphate resistance than ordinary Portland cement, and in particular, the alkali activated slag cement added 5 wt% alumina cement has little deterioration on the sulphuric acid solution. The reason why the alkali activated slag cement has higher sulphate resistance than other hardened cement pastes is that it has no $Ca(OH)_2$ reactive to sulphate ion, and there is little $CaSO_4{\cdot}2H_2O$ production causing volume expansion, unlike other pastes. And it is supposed that $Al(OH)_3$ hydrates with high sulphate resistance, which is produced by adding the alumina cement increases the sulfate resistance.

알칼리활성화 슬래그-레드머드 흙포장재의 레드머드 대체율에 따른 기공특성 (Porosity of Alkali-Activated Slag-Red Mud Soil Mixed Pavement of Red Mud Substitution Rate)

  • 강혜주;김병기;김재환;강석표
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2016년도 추계 학술논문 발표대회
    • /
    • pp.91-92
    • /
    • 2016
  • Red mud is an inorganic by-product produced from the mineral processing of alumina from Bauxite ores. the development of alkali-activated slag-red mud cement can be a representative study aimed at recycling the strong alkali of the red mud as a construction material. This study is to investigate the pore characteristics of alkali-activated slag-red mud soil pavement according to the red mud content. The results showed that the porosity of alkali-activated slag-red mud soil pavement increased but the compressive strength of that decreased as the red mud content increased.

  • PDF

레드머드 대체율에 따른 폴리머 혼입 알칼리활성화 슬래그-레드머드 시멘트모르타르의 강도 및 기공특성 (Strength and Pore Characteristics of Alkali-activated Slag-Red Mud Cement Mortar used Polymer According to Red Mud Content)

  • 권성준;강석표
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제20권2호
    • /
    • pp.26-33
    • /
    • 2016
  • 알칼리활성화 슬래그-레드머드 시멘트는 알칼리활성화 시멘트 연구의 일환으로서 시멘트 조성에서 알칼리자극제, 고로슬래그와 레드머드로 구성되어져 있으며, 포틀랜트 시멘트를 사용하지 않는 클링커 프리 시멘트(Clinker Free Cement)를 의미한다. 본 논문에서는 포틀랜트 시멘트를 전혀 사용하지 않고 고분자 유기화합물인 재유화형 분말 폴리머를 혼입한 알칼리활성화 슬래그 시멘트에 레드머드의 대체율을 달리하여 강도특성, 기공특성 등을 기존 포틀랜트 시멘트와 비교 평가하였다. 그 결과 알칼리활성화 시멘트에 레드머드를 대체할 경우 C-S-H 광물상과 에트린가이트가 주요 수화생성물로 포틀랜트 시멘트와 비교하여 조직이 치밀하고 대체율 10%까지는 압축강도 및 휨강도가 증가하였다.

알칼리 자극제를 혼입한 고로슬래그 모르타르의 건조수축 특성에 관한 실험적 연구 (An Experimental Study on the Properties of Drying Shrinkage for Alkali-Activated Slag Mortar)

  • 천정환;김재훈;지남용
    • 한국건축시공학회:학술대회논문집
    • /
    • 한국건축시공학회 2006년도 춘계학술논문 발표대회 제6권1호
    • /
    • pp.97-100
    • /
    • 2006
  • This paper report the result of the investigation on the properties of drying shrinkage for alkali-activated slag mortar in different relative humidity Commonly we know that drying shrinkage means lost more moisture but the mechanism of drying shrinkage of alkali activated slag mortar is not entirely due to the quantity of weight loss of water from mortar. pore size distribution and the calcium silicate hydrate gel characteristics have a critical influence on the magnitude of drying shringkage to alkali activated slag mortar. For this investigation, Ca(OH)2, Na2SiO4 were as alkali activator with 5 dosages(6%, 9%, 12%, 15%, 20%) and curing condition were three different relative humidity(35%, 65%, 95%) at $20{\pm}3^{\circ}C$

  • PDF

순환골재를 사용한 알칼리활성화 슬래그-레드머드 흙포장재의 특성 (Properties of Alkali-activated Slag-Red Mud Soil Pavement Using Recycled Aggregate)

  • 강석표
    • 한국건설순환자원학회논문집
    • /
    • 제4권3호
    • /
    • pp.276-283
    • /
    • 2016
  • 레드머드는 보오크사이트 원광석에서 생산되는 알루미나의 선광과정에서 발생되는 무기질 부산물이다. 인 레드머드를 활용하고자 하는 연구가 국내에서 이루어지고 있다. 강알카리성의 레드머드를 건설산업용 촉진제로서 활용하고자 하는 연구로서 알칼리활성화 슬래그-레드머드 시멘트가 국내외적으로 발표되고 있다. 본 논문은 순환골재 대체율에 따른 알칼리활성화 슬래그-레드머드 건식 흙포장재의 최적함수율, 압축강도, 흡수율, 백화발생 특성에 대하여 비교 검토하였다. 그 결과 순환골재 대체율이 증가할수록 알칼리활성화 슬래그-레드머드 흙포장재의 최적 함수비, 물흡수계수, 백화면적은 증가하고 압축강도는 감소하였다.

자극제의 종류에 따른 알칼리 활성화 슬래그 모르타르의 기초 특성 (Fundamental Properties of Alkali Activated Slag Mortar with Different Activator Type)

  • 안양진;문경주;소승영;소양섭
    • 한국콘크리트학회:학술대회논문집
    • /
    • 한국콘크리트학회 2006년도 추계 학술발표회 논문집
    • /
    • pp.789-792
    • /
    • 2006
  • The purpose of this study is to investigation the fundamental properties of alkali activated slag of type and concentration of alkali activator. In this paper sodium silicate, sodium carbonate and sodium hydroxide were used as alkaline activator and their concentration were 1, 3, 5 and 7 $Na_2O$ weight percent. The physical properties of alkali activated blast furnace slag cement mortar (AAS) were investigated by flow test and compressive strength. And the hydration properties of AAS characterized by X-ray diffraction and scanning electron microscope. Result show that Alkali activated slag mortar strengths were continuously increased with adding amount and ages. C-S-H were formed to be the main products up to 28days of hydration.

  • PDF