• Title/Summary/Keyword: annual ring angle

Search Result 14, Processing Time 0.021 seconds

Studies on the Fundamental Properties of the Wood of Gumgangsong(Pinus densoflora for. erecta Uyeki) (Part 1) (강송의 기초적 재질에 관한 연구(제1보))

  • 김정환;이원희;홍선천
    • Journal of the Korea Furniture Society
    • /
    • v.10 no.2
    • /
    • pp.55-61
    • /
    • 1999
  • This research was carried out to investigate the fundamental properties such as the structure of annual ring, density distribution, compressive strength with parallel to grain, relative crystallinity, and microfibril angle of Gumgangsong(Pinus densoflora for. erecta Uyeki). The wood specimens, Gumgangsong and Sonamu(Pinus densiflora S. et Z.), for this experiment were prepared at Ulijingoon Sokwangri and Kyungpook university's forest in Kyungpook province, respectively. Average annual ring width is $2.0mm{\pm}0.3$ in heartwood of Gumgangsong. The respectively of heart wood was over 60 percent in Gumgangsong and 20~50 percent in Sonamu. Heartwood density were ranged from 0.5 to $0.8{\;}g/cm^3$ in Gumgangsong and from 0.4 to $0.5{\;}g/cm^3$ in sonamu. Compressive strength in Gumgangsong and Sonamu was about $30{\pm}5MPa$ and $25{\pm}5MPa$, resepectively. But the relative crystallinity and microfibril angle of two species were not different clearly. From these results of Gumgangsong and Sonamu, therefore, it was considered the main difference factors for both species were annual ring width and heartwood percentage.

  • PDF

Microfibril Angle Characteristics of Korean Pine Trees from Depending on Provinces

  • KIM, Ji-Yeol;KIM, Soo-Chul;KIM, Byung-Ro
    • Journal of the Korean Wood Science and Technology
    • /
    • v.48 no.4
    • /
    • pp.569-576
    • /
    • 2020
  • This study investigated the characteristics of microfibril angle(MFA) in order to see if there was any difference in pine tree lumber quality among the three mountain areas surrounding the Taebaek Mountains in Korea - Yeongdong (Goseong-gun), Yeongseo (Hongcheon-gun) and Yeongnam (Bonghwa-gun). Pine trees of each mountain area were divided into earlywood and latewood in relation to heartwood part (1959 ~ 1961, 3 annual rings) and sapwood part (2002 ~ 2004, 3annual rings), and measured at tangential section. The microfibril angle showed significant differences between mountain areas. In general, Goseong Mountain was found to have 37.35°, followed by Hongcheon Mountain 32.42° and Bonghwa Mountain 25.75°, in order. The sapwood part had larger angle than heartwood part; and earlywood, than latewood. Variation within a single annual ring tended to be smaller from earlywood toward latewood.

Changes in Cellular Characteristics and Qualities of Matured and Juvenile Wood from Reforested Tree of Pinus koraiensis (잣나무 조림목(造林木)의 조직특성(組織特性)의 변동(變動)과 성열재(成熱材)·미성열재(未成熱材)의 재질(材質))

  • Kang, Sun-Koo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.21 no.2
    • /
    • pp.73-80
    • /
    • 1993
  • Pinus koraiensis is one of the most important reforestation species which had widely been planted around the country. Therefore, there are great research needs on the fundamental properties of wood to extend the frequency of uses and adequate availabilities. Research results on the characteristics of anatomical wood properties and changes are summarized as follows: 1. At a horizontal direction of tree trunk, the tracheid length at outer wood gradually becomes shorter as it reaches to pith. The tracheid length having between 32 and 42 annual rings showed over 2.5 times longer than that of pith, and also its length increases from the bottom to the top of the stem. 2. The tracheid diameters in latewood showed a little fluctuations, and the shortest near to the pith in earlywood. The tracheid diameters in earlywood are more than 2 times those of latewood, and the differences between the mature and juvenile wood in earlywood are less than 10${\mu}m$. 3. The tracheid wall thickness in early wood showed a little fluctuations. On the contrary, tracheid wall thickness in latewood rapidly increases from the pith to the bark. The tracheid wall of mature wood showed 10 to 20% thicker than that of juvenile wood. 4. The fibril angle at the secondary walls of tracheid within an annual ring showed higher degree in earlywood than that of latewood. The highest tracheid fibril angle was observed at around the pith of both earlywood and latewood. Then, fibril angle slowly decreased toward outer wood, and was stabilized after 15 years. 5. Structural boundaries between mature and juvenile wood from Pinus koraiensis are divided by 13 to 19 annual ring and distance of 5 to 8cm from the pith.

  • PDF

Effect of Annual Ring Angles on Static Bending Strength Performances of Cross-Laminated Woods Made with Spruce (연륜경사각이 가문비나무 직교형적층재의 정적 휨 강도성능에 미치는 영향)

  • Sung, Eun-Jong;Kwon, Chang-Bae;Ryu, Hyun-Soo;Byeon, Hee-Seop;Park, Han-Min
    • Journal of the Korean Wood Science and Technology
    • /
    • v.42 no.3
    • /
    • pp.290-300
    • /
    • 2014
  • In this study, cross-laminated woods were made with spruce wood and the effects of annual ring angles of perpendicular direction laminae on static bending strength performance were investigated. Static bending strength performances of parallel laminated woods with all layers composed of laminae perpendicular to the grain ($P_{\bot}$ type) were in the order of $90^{\circ}$ > $0^{\circ}$ > $45^{\circ}$. The MOE and MOR for the $45^{\circ}$ annual ring angle were 0.0989 GPa and 3.25 MPa, and it showed the lowest values. By placing longitudinal-direction laminae in the core of $P_{\bot}$ type, the strength performances were markedly improved. In the case of cross-laminated woods with perpendicular-direction laminae in the faces ($C_{\bot}$ type), the bending strength performances were in the order of $90^{\circ}$ > $0^{\circ}$ > $45^{\circ}$, but the differences among annual ring angles were less than those of the parallel-laminated woods. In the case of cross-laminated woods with perpendicular-direction laminae in the core ($C_{\parallel}$ type), the bending strength performances were in the order of $45^{\circ}$ > $90^{\circ}$ > $0^{\circ}$ unlike $P_{\bot}$ type and $C_{\bot}$ type. The MOE and MOR for the $45^{\circ}$ annual ring angle were 12.0 GPa and 55.8 MPa, and it showed the highest values.

Analysis of Species and Tree-Ring Dating of Wood Elements Used for the Daewoongjeon Hall of Youngguksa Temple (영국사 대웅전 목부재의 수종 및 연륜연대 분석)

  • Son, Byung-Hwa;Park, Won-Kyu;Yoon, Doo-Hyung
    • Journal of architectural history
    • /
    • v.15 no.2
    • /
    • pp.23-38
    • /
    • 2006
  • During the repair and restoration of the Daewoongjeon Hall of Youngguksa Temple, species identification and tree-ring dating for both present wood elements and charred ones excavated under the Hall, were conducted. The species of 74 wood elements of Daewoongjeon Hall, were identified as Pinus densiflora Sieb. et Zucc. and only 1 was identified as exotic Pinus species. The latter wood, which was used in the laths, seems to have been replaced during past repairs. Many documentary records and various artifacts pertaining to Youngguksa Temple are being excavated, but none described precisely the construction date of the present Daewoongjeon Hall. Also, from beneath the Daewoongjeon Hall, cornerstone and foundation of previous building and several charred wood elements were excavated. In comparing the direction of the stone columns of foundation of the previous structure and the existing Daewoongjeon Hall, the previous structure was rotated in an angle of approximately $15^{\circ}$. Therefore, in order to find the association of the previous structure with the present Daewoongjeon Hall, tree-ring dating was conducted. The dating of 41 original timbers and 14 roof-filling timbers of the present construction elements revealed that the last annual ring was of A. D. 1703 with complete latewood, indicating that those woods was cut some time between the autumn of 1703 and spring of 1704, and the building was erected in 1704 when we assume no period of wood storage. The year of the last annual ring of the charred elements, which were excavated from beneath the Daewoongjeon Hall, was analyzed as 1674. The cutting year of the woods used for the present building began in 1698, therefore, it can be presumed that the Daewoongjeon Hall before the fire was a structure that was elected shortly after 1674 and that a catastrophic fire occurred some time between 1674 and 1698.

  • PDF

Wood Quality of Trees Fertilized by Charcoals (목탄시비 수목의 재질)

  • Kim, Byung-Ro;Shin, Chang-Seob
    • Journal of the Korean Wood Science and Technology
    • /
    • v.36 no.3
    • /
    • pp.55-60
    • /
    • 2008
  • This study was carried out to investigate the effect of charcoal meal application on the quality of the wood. As the results, it was observed that annual ring width of seedlings was wider in the plots treated with charcoal meal than the control plots. Depending on the kind of charcoal, annual ring width was widest in the plot treated with Larix kaempferi charcoal, and then was observed in order of Pinus koraiensis > particle board > Quercus acutissima. Latewood percentage and specific gravity were lower in the plots treated with charcoal than the control plots and lowest in Larix kaempferi charcoal plot among the plots treated with charcoal. Tracheid length was longer in the plot treated with powder charcoal than the control plot but tracheid width was not significantly different from the control plot. The cell wall thickness of earlywood was not significantly different between the plot treated with charcoal and the control plot but that of latewood was thicker in the plots treated with charcoal than the control. Microfibril angle was smaller in the plot treated with granulated charcoal than the control plot. However, there was no significant difference between the plot treated with powder charcoal and granulated charcoal.

Evaluation of Bonding Strength of Larch Cross-Laminated Timber

  • Song, Yo-Jin;Hong, Soon-Il
    • Journal of the Korean Wood Science and Technology
    • /
    • v.44 no.4
    • /
    • pp.607-615
    • /
    • 2016
  • The delamination along the annual ring on the cross-section of laminae and the bonding strength according to the tangential angle between laminae were evaluated for the production of 3-ply cross-laminated timber (CLT) using domestic larch. Since there is no standard for CLT in Korea, the production and test of specimens for bonding strength followed the standard procedure of "Structural glued laminated timber" (KS F 3021). The standard specifies to exclude any measurement from the cracks of timbers resulted from drying or knots during delamination test of the glued laminated timbers. However, the failure of cross-sectional tissues along the annual rings was observed near the glue-line of all specimens during the delamination test. Because this phenomenon can generate defects in the CLT that may be exposed to various temperatures and relative humidities after the actual construction, the delamination percentage was measured by including this wood failure. As a result, the delamination percentage of the CLT which had been combined in such a way that the annual rings of outer lamina were directed inward was the lowest, which was around 13%, regardless of the annual ring direction of the middle lamina. On the other hand, the delamination percentage of the CLT which had been combined in such a way that the annual rings of outer lamina were directed outward was the highest, which was around 26%. Furthermore, end-split occurred in the outer lamina during the drying process of the boiling delamination test, which affected the delamination percentage. Therefore, the soaking delamination test was found to be more appropriate for evaluating the delamination strength of CLT. The block shear strength of larch CLT was $3.9{\pm}0.9$ MPa on average, which was 46% lower than the block shear strength requirement (7.1 MPa) of the standard, but satisfied the criteria of the block shear strength (3.5 MPa) of the European Standard (prEN 16351: 2013).

Studils on Micro Fibril Angle of Woody Plant Cell Wall(1) - Variation of Micro Fibril Angle on Tree Stem - (목재세포벽(木材細胞壁)의 MICRO FIBRIL 경사각(傾斜角)에 관(關)한 연구(硏究)(1) - 수간내(樹幹內) MICRO FIBRIL 경사각(傾斜角)의 변이(變異) -)

  • Chun, Su-Kyung;Lee, Won-Yong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.11 no.1
    • /
    • pp.5-11
    • /
    • 1983
  • This paper aims at gaining the informations atout the fibril angle at secondary walls of tracheids. The test specimens were taken from disks on stem wood of "Pinus koraiensis Sieb. et zucc". The method of measuring the fibirl angle was selected so-called "iodine method" that crystalline aggregates of iodine may be induced to form within the elongated interstices of the cellulose matrix of the secondary wall and that these elongated crystals are oriented parallel to the long axies of the fibrills of cellulose. The following conclusions may be drawn from the results of this investigation. 1) Gross average fibril angle was about $17.6^{\circ}$ on stem wood. 2) Its values seem to be greater for earlywood (avg.$19.8^{\circ}$) than for latewood tracheids (avg.$15.3^{\circ}$) in normal wood. 3) According to the increase of annual ring from pith to barks the orientation of fibril angle seems to be decrease gradually in normal wood. 4) In the case of height variation in trees the sample trees have a tendency to increase the orientation fibril angle to the increase of tree height in stem.

  • PDF

Analysis of Tree-rings for Inference of Periods in which Slow-moving Landslides Occur (나이테 분석을 통한 땅밀림 발생 시기 추정)

  • Park, Jae-Hyeon;Park, Seonggyun
    • Journal of Korean Society of Forest Science
    • /
    • v.109 no.1
    • /
    • pp.62-71
    • /
    • 2020
  • With the aim of restoring slow-moving landslide areas, this study collected fundamental data from tree-ring analysis of curved trees in these areas. We collected both upper and lower stem disks to measure the azimuth angles of six trees with growth curvature caused by tension cracks. Additionally, we analyzed various factors in the slow moving landslide area. The geological strata and main constitutive rocks in the study area were anorthosite-formed in the Precambrian period; moreover, there were no intrusive rocks, other geological strata, geological folds, or faults. The talus with weathered rocks was distributed in the upper zone of the slow-moving landslide area. According to annual-ring analysis of curved trees and terrain analysis by satellite imagery, slow-moving landslide occurred from the top to the bottom end of the slope between 1999 and 2011. There was a significant relationship (P < 0.01) between the azimuth angle of cracks caused by the slow-moving landslide and the angle of the curved trees. These results suggest that the occurrence of slow-moving landslides could be confirmed through analysis of annual-rings of curved trees, underground water levels, and terrain (by satellite imagery).

Studies on the Improvements for GAYAKUM Sounding Boards (가야금(伽倻琴) 향판재(響板材)의 개선(改善)에 관(關)한 연구(硏究))

  • Hong, Byung-Wha
    • Journal of the Korean Wood Science and Technology
    • /
    • v.18 no.4
    • /
    • pp.65-78
    • /
    • 1990
  • For the purpose of Improving the sounding boards for the conventional GAYAKUM, I was making approximately 202 specimens of radial board, 371 specimens of tangential board by cutting along the grain and the part of stem and 31 specimens of the disjointed traditional GAYAKUM made in Paulownia coreana. And it was conducted to measure specific gravity, dynamic Young's modulus, internal friction, resonant frequency, velosity of sound and width of annual ring by the method of the frexural vibration in a free-free bar in the audio frequency range. And it confirmed the juvenile wood by measuring wood fiber length of specimens. It was also conducted to investigate dynamic properties and moisture absorption by various heat-treatment and to test dynamic Young's modulus and internal friction for the disjointed conventional GAYAKUM. The results obtained were summarized as follow: 1. The Juvenile wood is located within about 7 annual rings from the pith in Paulownia coreana. 2. As increased with the specific gravity, the dynamic Young's modulus had more and more increased, but the internal friction had slightly decreased. 3. I think that radial board would be good for sounding board wood. because radial board is higher than tangential board in dynamic Young's mudulus and internal friction is lower than tangential board. 4. The value of mean dynamic Young's modulus on the conventional GAYAKUM, radial board and tangential board of 604 samples is $0.4283\pm0.037(\times10^{11}dyne/cm^2)$, $0.4316\pm(\times10^{11}dyne/cm^2)$ and $0.4234\pm0.112(\times10^{11}dyne/cm^2)$ respectively. The value of the radial board showed little higher than that of conventional GAYAKUM, but It had a similar tendency between conventional GAYAKUM and tangential board. 5. The annual ring width by four aspect is more narrow in north and west than that of others. 6. The values of specific gravity and dynamic Young's modulus in the mature wood showed higher than those of juvenile wood. 7. As the grain angle in the butt wood more increased to bark from pith, the dynamic Young's modulus were low. Then it was not good for sounding board. 8. It appeared that the heat-treatment for sounding board wood had a more effect to do the treatment of hotiron on surface after heat-treatment during 24 hours in $60^{\circ}C$ temperature. 9. As increased with the temperature, the rate of moisture absorption of heat-treatment wood had decreased. In conclusion, I thought that the sounding board wood for GAYAKUM would had the most effect to do the treatment of hotiron on surface after heat-treatment during 24 hours in $60^{\circ}C$ temperature using the radial board of mature wood.

  • PDF