• Title/Summary/Keyword: compaction density

Search Result 421, Processing Time 0.026 seconds

The Investigation Study of Compaction Density by Waste Composition Change in Landfill Site (매립장의 반입쓰레기 성상변화에 따른 다짐밀도 조사연구)

  • Jung, Byung-Gil;Choi, Young-Ik;Kim, Jung-Kwon
    • Journal of Environmental Science International
    • /
    • v.17 no.4
    • /
    • pp.397-403
    • /
    • 2008
  • The purpose of this study is to investigate weighted compaction density according to a leading density in truck, a compaction density of solid waste and composition ratios of solid waste fur calculation of a capacity of the landfill sites. The experiments for calculations of in-place density at landfill site have been conducted in S landfill site at B City. The size of vessel for measuring the compaction density was $1m^3(1m{\times}1m{\times}1m)$. The experiment tests have been carried out methods (1 time for bulldozer and 4 times for compactor) that do contain all of specification at the landfill site. Average of the loading density at the landfill site was $0.264\;ton/m^3$ ($0.113{\sim}0.487\;ton/m^3$). When the loading density for each compositions was compared, the composition of the highest average loading density ($0.474\;ton/m^3$) was miscellaneous wastes. The composition of the lowest average loading density ($0.120 ton/m^3$) was general solid waste. The reported results indicated that the compaction density at the landfill site was $0.538\;ton/m^3$, which was calculated with weighted incoming ratios of compositions. The ranges of the density for each composition were from $0.021\;ton/m^3$ to $0.221\;ton/m^3$. When the compaction density for each composition was compared, the composition with the highest average compaction density ($0.221\;ton/m^3$) was miscellaneous wastes. The composition with the lowest average compaction density ($0.021\;ton/m^3$) was general solid wastes.

Property of New SEGLESS that is Segregation-free Steel Powder Mixture for Warm Compaction

  • Nishida, Satoshi;Furuta, Satoshi
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09b
    • /
    • pp.731-732
    • /
    • 2006
  • Recently warm compaction techniques are focused on and commercialization of one high-density compaction process in the P/M industry. Another development is a new SEGLESS using a developed lubricant that reduces ejection force at room temperature compaction. It is possible to achieve high-density by reducing lubricant amount. In this paper we confirmed that green density was $7.35g/cm^3$ at 686MPa of compaction pressure when the new SEGLESS was applied to relatively lower temperature warm compaction process, such as $80^{\circ}C$.

  • PDF

The Study on the Compaction Characteristics of Underground Structural Backfill with Reclaimed Soil (준설토를 이용한 지하구조물 뒷채움 다짐특성에 관한 연구)

  • 김영웅;박기순;손형호;김종국
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 1999.03a
    • /
    • pp.357-364
    • /
    • 1999
  • The purpose of this study is to analysis the grain distribution and compaction characteristics of structural backfill with reclaimed soil. Five(5) reclaimed soil samples which passed #200 sieve have been used in the test. The study showed that the maximum dry density and the bearing value rate turned out to be becoming smaller when the more the quantity passed #200 sieve, the smaller the soil grain. The maximum dry density value calculated from the compaction md relative density test showed wet method > compaction method > dry method. The correlation coefficient between Rc and Dr based on the grain distribution and the compaction characteristics showed that the maximum dry density value by the wet method is little higher than the compaction method and dry method.

  • PDF

Development of High Strength Sintered Steel by High Pressure Warm Compaction Using Die Wall Lubrication

  • Matsumoto, Nobuhiko;Miyake, Toshitake;Kondoh, Mikio;Ando, Kimihiko;Tanino, Hitoshi
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.197-198
    • /
    • 2006
  • The high pressure compaction without internal lubricant and the high green density even with the pore free density were achieved by the newly developed die wall lubricant for warm compaction. This developed die wall lubricated warm compaction followed by high temperature sintering resulted in not only the superior mechanical property but also the low dimensional change. In this paper, the effects of increasing the green density on the sintered density, the dimensional change and the mechanical property are mainly discussed

  • PDF

Influence of Mold Temperature, Lubricant and its Additional Quantity on Compressibility in Warm Compaction

  • Ushirozako, Tsutomu;Yamamoto, Masayuki
    • Proceedings of the Korean Powder Metallurgy Institute Conference
    • /
    • 2006.09a
    • /
    • pp.195-196
    • /
    • 2006
  • In recent years, demands for sintered ferrous material with higher strength are increasing. To satisfy these demands, studies and commercial use of the die wall lubrication method, the warm compaction method and the combination of both methods are widely carried out to achieve high density. The die wall lubrication warm compaction method makes it possible to achieve high density by reducing internal lubricant through die wall lubrication, although the method involves several issues such as prolonged cycle time due to lubricant spraying and difficulty in spraying lubricant in the case of compacting with complicated geometry. Meanwhile, the conventional warm compaction method requiring no die wall lubricant application cannot achieve such a high density as in the case of die wall lubrication warm compaction due to higher volume of internal lubricant. However, this report discloses our study result in which the possibility of improving density is exhibited by using a lubricant type with superior dynamic ejection property that can reduce volume of lubricant additive.

  • PDF

Optimum Compaction Test of Roller Compacted Concrete Pavement (롤러전압 콘크리트포장의 적정 다짐실험 방안 고찰)

  • Chung, Gun Woo;Lee, Seung Woo
    • International Journal of Highway Engineering
    • /
    • v.17 no.3
    • /
    • pp.27-33
    • /
    • 2015
  • PURPOSES : To ensure appropriate RCC properties with sufficient strength development and workability, it is necessary to secure a proper level of consistency. It is also necessary to secure maximum dry density, which is an important factor for increasing the interaction of aggregate interlocking, leading to an augmentation of RCC strength. On the other hand, the dry density of RCC can be changed owing to the compaction conditions, water content, and particle size distribution. A Proctor test and a modified Proctor test were used for determining the optimum water content needed to achieve maximum dry density with different amounts of compaction energy. A Vebe test, on the other hand, was used for checking the level of consistency, which is important for producing a workable mixture. METHODS : To confirm the degree of compaction at various particle sizes, RCC mixtures with different sand/aggregate ratios were evaluated. The Proctor test and modified Proctor test were applied to these mixtures to check the effect of the aggregate gradation and compaction energy on the maximum dry density and optimum water content. During each test, three specimens were produced for all types of water content under each aggregate gradation. A compaction curve and the optimum water content and maximum dry density for each aggregate gradation were then obtained for both tests. The range of water content for the appropriate consistency of each aggregate gradation was determined through a Vebe test. The optimum water content was then evaluated based on this range. RESULTS : The compaction test results show that the modified Proctor test provides a higher maximum dry density and lower optimum water content compared with the standard Proctor test. For the modified Proctor test, two cases of aggregate gradation (s/a = 30% and 70%) had the optimum water contents outside of the appropriate water content range. For the standard Proctor test, on the other hand, none of aggregate gradations provided the optimum water content within the desired range. CONCLUSIONS : The modified Proctor test should be used for an RCC mixture design because it can provide adequacy between maximum dry density and consistency. Moreover, the compaction roller has become highly developed for higher compaction energy.

Effect of Coarse Materials on Compaction of Soil (조립재가 흙의 다짐에 미치는 영향)

  • 윤충섭;김호일;김현태
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.33 no.4
    • /
    • pp.84-95
    • /
    • 1991
  • The compaction ratio of the field dry density to the maximum dry density is generally adopted as the index of quality control for embankment of earthfill structures such as Earth Dam, Sea Dike, River Bank and Road. In case of coarse materials are included in the earth material, the compaction ratio will be varied in wide range since the dry density is influenced by quantity of coarse material in the soil. The treatment for the coarse material should be controlled carefully in testing. In this study, the compaction characteristics of the soil contained the coarse materials were researched and calibration of the suitability of field quality control methods were carried out. 28 Samples were made of clay(CL) and sandy soil (SM) mixed with gravel whose content were 0, 4, 6, 8, 10, 12, 15, 20, 25, 30, 35, 40, 45, and 60% in Weight. The compaction characteristics depending on the coarse material content were analysed through 4 types of compaction tests which are A-1, B-i, C-i and D-1. The adjusting coefficients for density and moisture content namely a and ${\beta}$ respectively were proposed in order to consider the effects depending on content of the coarse materials. The test methods to control reasonably and promptly the quality of earthfill were proposed after analysing the ranges of possible errors on the relative compaction ratio between laboratory compaction methods and field density testing methods.

  • PDF

FE Analysis of Alumina Green Body Density for Pressure Compaction Process (압축성형공정에 대한 알루미나 성형체 밀도분포의 FE 분석)

  • Im, Jong-In;Yook, Young-Jin
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.12 s.295
    • /
    • pp.859-864
    • /
    • 2006
  • For the pressure compaction process of the ceramic powder, the green density is very different with both the ceramic body shape and the processing conditions. The density difference cause non-uniform shrinkages and deformations, and make cracks in the sintered ceramics. In this paper, Material properties of the alumina powder mixed with binder and the friction coefficient between the powder and the tool set were determined through the simple compaction experiments: Also the powder flow characteristics were simulated and the green density was analyzed during the powder compaction process with Finite Element Method (FEM). The results show that the density distributions of the green body were improved at the optimized processing condition and both the possibility of the farming crack generation and rho deformation of the sintered Alumina body were reduced.

Experimental studys about Compaction in Soil (흙의 다짐에 관한 실험적 연구)

  • 이석찬
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.14 no.2
    • /
    • pp.2661-2667
    • /
    • 1972
  • In the construction of earth dam, embankment, highway by filling, a compaction is to increase the density of applying pressure. By compaction interspaces between the soil graivos decrease so that density and adhesion increase but void and permeability decrease. Good compaction results in higher stablilty. The effect of the compaetion depends on a number of factors, of which the most important are soil charactesistics. Water content, and external force. In this study discussed is about sandy loam that since, with indentical force exerted and indentical compaction method, the effect of the compaction will be different due to the soil characteristics, the change of optimum moisture content and of maximum dry density by compaction yields difference in Compaction for a same sample.

  • PDF

A Study on the Mechanical Compaction of Pervious Materials (투수성 성토재료의 기계다짐에 관한 연구)

  • 윤충섭
    • Magazine of the Korean Society of Agricultural Engineers
    • /
    • v.23 no.3
    • /
    • pp.65-77
    • /
    • 1981
  • The Compaction of fill dam is very important for increasing of the safty of dam. Vibration roller is used for the compaction of pervious materials such as sand and gravel. The principal objects of this study are to give a comstruction criteria of vibration roller and to find out the relationship between dry density and permeabity of pervious soil after compaction. The results in this study are summerized as follows. 1.The relationship between maximum dry density (Υdmax) and optimum moisture content(Wo) of modified compaction test is Υdmax=2. 74-0. 064w0 2.The maximum dry density decrease with increasing fine particle(n) and the relative formular is n==ae-brdmax 3.The maximum dry density is influenced more by passing rate of number 200 sieve than 4 sieve. 4.The coefficient of permeability are similar when the degrees of compaction are equal even though the spreading thickness of soil are different. 5.The coefficient of permeability(K)is greatly influence by fine particle passing number 200 sieve, and those relationship is inversely proportionate. 6.The K values of pervious soil are from 10-0 cm/sec to 10-4 cm/sec when degree of compaction by a modified method is from 90 to 95percent. 7.The coarser material is little influenced on the permeability with different density. 8.The increasing rate of permeability with decreasing degree of compaction is more influened by fine pacticle than number 200 sieve. When degree of compaction decrease from 100 percent to 90 percent the K values of SM and GM increase about 20 times but GW increase 6 times only. 9.The effect of compaction by vibration roller is greatly influenced by 6 passes and the increasing rate of the effect is decraased at 8 passes. 10. In order to get the degree of compaction of 95 percent or more, 6 to 8 passes of roller are generall required with 30 cm thickeness of soil for 4.5 ton to 6.5 ton vibration roller and 7 to 8 passes is required with 50cm thickness for 8 to 12 ton roller.

  • PDF