• Title/Summary/Keyword: hydrothermal process

Search Result 351, Processing Time 0.03 seconds

Dehydration and RDF Production of Organic Sludge with Hydrothermal Pre-treatment Process (증기열 전처리공정을 이용한 유기성 슬러지의 건조 및 성형연료화)

  • Park, Se-Joon;Choi, Yong-Sung;Lee, Kyung-Sup
    • The Transactions of the Korean Institute of Electrical Engineers P
    • /
    • v.58 no.4
    • /
    • pp.526-531
    • /
    • 2009
  • This paper suggests the dehydration and RDF(Refuse Derived Fuel) production of organic sludge, livestock manure and sewerage sludge causing environmental problems, with hydrothermal pre-treatment process. The renewable technology from the organic wastes must involve short treatment time required, reusable energy source, anti-odor and viruses, low cost for the treatment, and well-fertilization. The hydrothermal pre-treatment process promotes to evaporate moisture in the sludge after being shortly treated in a reactor, which is supplied steam and heat by an external boiler, due to the pressure with steam breaks the cell walls of the sludge, so this process removes the internal moisture of the cell. Then, the treated sludge(solid-state) is mixed with waste vinyls called RDF(6,706kcal/kg).

Dehydration and RDF Production of Organic Wastes with Pressurized Hydrothermal Treatment Process (증기가압형 처리공정을 이용한 유기성 폐기물의 건조처리 및 고형연료화)

  • Park, Se-Joon;Choi, Young-Chan;Choi, In-Kyu
    • Transactions of the Korean hydrogen and new energy society
    • /
    • v.20 no.5
    • /
    • pp.439-446
    • /
    • 2009
  • This paper investigates the dehydration and RDF (Refuse Derived Fuel) production of organic wastes, livestock manure and sewerage sludge with pressurized hydrothermal treatment process. The renewable technology for the organic wastes must involve short treatment time required, reusable energy source, anti-odor and viruses, low cost for the treatment, and well-fertilization. The pressurized hydrothermal treatment process promotes to evaporate moisture in the waste after being shortly treated in a reactor, which uses steam and heat supplied by an external boiler. By the pressurized steam, the cell walls of the waste break and effectively release the internal moisture. Then, the dried waste can be mixed with waste vinyls to produce RDF with a higher heating value as high as 6,700 kcal/kg.

Torrefaction and Hydrothermal Carbonization (HTC) of Dead Leaves

  • Saqib, Najam Ul;Park, Seong-Kyu;Lee, Jai-Young
    • Journal of Soil and Groundwater Environment
    • /
    • v.19 no.5
    • /
    • pp.45-52
    • /
    • 2014
  • Torrefaction and hydrothermal carbonization (HTC) are productive methods to reclaim energy from lignocellulosic biomass. The hydrophobic, homogenized, energy dense and carbon rich solid fuel can be obtain from torrefaction and hydrothermal carbonization. Dead leaves were carbonized in a stainless steel reactor of volume 200 ml with torrefaction ($250-270^{\circ}C$) for 120 minutes and hydrothermal carbonization ($200-250^{\circ}C$) for 30 minutes, with mass yield solid fuel ranging from 57-70% and energy content from 16.81MJ/kg to 22.01 MJ/kg compare to the biomass. The char produced from torrefaction process possess high energy content than hydrothermal carbonization. The highest energy yield of 89.96% was obtained by torrefaction at $250^{\circ}C$. The energy densification ratio fluctuated in between 1.15 to 1.30. On the basis of pore size distribution of the chars, the definition of the International Union of Pure and Applied Chemistry (IUPAC) was used as a classification standard. The pore diameter was ranging within 11.09-19 nm which play important role in water holding capacity in soil. Larger pores can hold water and provide passage for small pores. Therefore, it can be concluded that high pore size char can be obtained my HTC process and high energy content char of 22.01 MJ/Kg with 34.04% increase in energy can be obtain by torrefaction process.

Photocatalytic Decomposition of Rhodamine B on PbMoO4 Using a Surfactant-assisted Hydrothermal Method

  • Hong, Seong-Soo
    • Clean Technology
    • /
    • v.24 no.3
    • /
    • pp.206-211
    • /
    • 2018
  • Lead molybdate ($PbMoO_4$) were successfully synthesized using a facile surfactant-assisted hydrothermal process and characterized by XRD, Raman, PL, BET and DRS. We also investigated the photocatalytic activity of these materials for the decomposition of Rhodamine B under UV-light irradiation. From XRD and Raman results, well-crystallized $PbMoO_4$ crystals have been successfully synthesized with a facile surfactant-assisted hydrothermal process and had 52-69 nm particle size. The $PbMoO_4$ catalysts prepared at $160^{\circ}C$ showed the highest photocatalytic activity. The PL peak was appeared at about 540 nm at all catalysts and it was also shown that the excitonic PL signal was proportional to the photocatalytic activity for the decomposition of Rhodamine B.

Hydrothermal Synthesis of 6mol% Yttria Stabilized Cubic ZrO2 Nano Powders (이트리아 안정화 지르코니아 나노 분말 합성)

  • Lee, Jae-Hoon;Bae, Sung-Hwan
    • Korean Journal of Materials Research
    • /
    • v.27 no.8
    • /
    • pp.445-450
    • /
    • 2017
  • YSZ (Yttria-stabilized zirconia) is a ceramic material that is used for electronic and structural materials due to its excellent mechanical properties and specific electrical characteristics according to the Yttrium addition. Hydrothermal synthesis has several advantages such as fine particle size, uniform crystalline phase, fast reaction time, low process temperature and good dispersion condition. In order to synthesize YSZ nanoparticles with high crystallinity, hydrothermal synthesis was performed at various concentrations of NaOH. The hydrothermal process was held at a low temperature ($100^{\circ}C$), with a short process time (2,4,8 hours); the acidity or alkalinity of solution was controlled in a range of pH 2~12 by addition of NaOH. The optimum condition was found to be pH 12, at which high solubility levels of Y(OH) and Zr(OH) were reported. The synthesized nano powder showed high crystallinity and homogenous composition, and uniform particle size of about 10 nm.

Hydrothermal Synthesis of Fe Based MOFs with Energy Economy Approach

  • Israr, Farrukh;Kim, Duk Kyung;Kim, Yeongmin;Oh, Seung Jin;Ng, Kim Choon;Chun, Wongee
    • Journal of Energy Engineering
    • /
    • v.24 no.2
    • /
    • pp.55-58
    • /
    • 2015
  • The mesoporous metal organic framework structure Fe-BTC was successfully synthesized by hydrothermal process with noticeable yield. The synthesis operation was conducted at intermediate temperature and for shortened operation time as compared to conventional procedures. This process approach with reduced operating temperature and shortened operation time may open an opportunity window towards process economy with reduction in energy consumption. A simple mathematical approach of diffraction indexing using X-ray diffraction patterns of synthesized powder was employed to confirm its crystalline nature and to investigate its high temperature stability. The crystallite size was calculated by using Debye-Scherrer equation.

Improvement of Biomass Degradation by Fenton Oxidation and Reusability of the Fenton Oxidation Solution (펜톤산화에 의한 바이오매스 분해향상과 펜톤산화 용액 재사용 평가)

  • Jeong, So-Yeon;Lee, Jae-Won
    • New & Renewable Energy
    • /
    • v.16 no.4
    • /
    • pp.83-91
    • /
    • 2020
  • In this study, the reusability of the Fenton oxidation solution was evaluated to reduce the cost of the pretreatment process. Biomass was sequential subjected to Fenton oxidation-hydrothermal treatment and enzymatic hydrolysis to produce monosaccharides. The liquid solution recovered after Fenton oxidation contained OH radicals with a concentration of 0.11 mol/L. This liquid solution was reused for a new Fenton oxidation reaction. After Fenton oxidation, hydrothermal treatment was performed under the same conditions as before, and 9.34-13.63 g/L of xylose was detected. This concentration was slightly lower than that of a fresh Fenton oxidation solution (16.51 g/L) but was higher than that obtained by hydrothermal treatment without Fenton oxidation (2.72 g/L). The degradation rate during hydrothermal pretreatment involving Fenton oxidation was 36.02%, which decreased (29.24-31.05%) slightly when the liquid solution recovered after Fenton oxidation was reused. However, the degradation rate increased compared to that measured from hydrothermal treatment without Fenton oxidation (15.21%). Moreover, the yield after enzyme hydrolysis decreased in the following order: fresh Fenton oxidation-hydrothermal treatment (89.64%) > Fenton oxidation with reused solution-hydrothermal treatment (74.84%) > hydrothermal treatment without Fenton oxidation (32.05%).

Crack-Free Fabrications of Yttria-Stabilized Zirconia Films Using Successive-Ionic-Layer-Adsorption-and-Reaction and Air-Spray Plus Method

  • Taeyoon Kim;Sangmoon Park
    • Korean Journal of Materials Research
    • /
    • v.34 no.2
    • /
    • pp.79-84
    • /
    • 2024
  • Thin films of yttria-stabilized zirconia (YSZ) nanoparticles were prepared using a low-temperature deposition and crystallization process involving successive ionic layer adsorption and reaction (SILAR) or SILAR-Air spray Plus (SILAR-A+) methods, coupled with hydrothermal (175 ℃) and furnace (500 ℃) post-annealing. The annealed YSZ films resulted in crystalline products, and their phases of monoclinic, tetragonal, and cubic were categorized through X-ray diffraction analysis. The morphologies of the as-prepared films, fabricated by SILAR and SILAR-A+ processes, including hydrothermal dehydration and annealing, were characterized by the degree of surface cracking using scanning electron microscopy images. Additionally, the thicknesses of the YSZ thin films were compared by removing diffusion layers such as spectator anions and water accumulated during the air spray plus process. Crack-free YSZ thin films were successfully fabricated on glass substrates using the SILAR-A+ method, followed by hydrothermal and furnace annealing, making them suitable for application in solid oxide fuel cells.

Selective Growth of Nanosphere Assisted Vertical Zinc Oxide Nanowires with Hydrothermal Method

  • Lee, Jin-Su;Nam, Sang-Hun;Yu, Jung-Hun;Yun, Sang-Ho;Boo, Jin-Hyo
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2013.08a
    • /
    • pp.252.2-252.2
    • /
    • 2013
  • ZnO nanostructures have a lot of interest for decades due to its varied applications such as light-emitting devices, power generators, solar cells, and sensing devices etc. To get the high performance of these devices, the factors of nanostructure geometry, spacing, and alignment are important. So, Patterning of vertically- aligned ZnO nanowires are currently attractive. However, many of ZnO nanowire or nanorod fabrication methods are needs high temperature, such vapor phase transport process, metal-organic chemical vapor deposition (MOCVD), metal-organic vapor phase epitaxy, thermal evaporation, pulse laser deposition and thermal chemical vapor deposition. While hydrothermal process has great advantages-low temperature (less than $100^{\circ}C$), simple steps, short time consuming, without catalyst, and relatively ease to control than as mentioned various methods. In this work, we investigate the dependence of ZnO nanowire alignment and morphology on si substrate using of nanosphere template with various precursor concentration and components via hydrothermal process. The brief experimental scheme is as follow. First synthesized ZnO seed solution was spun coated on to cleaned Si substrate, and then annealed $350^{\circ}C$ for 1h in the furnace. Second, 200nm sized close-packed nanospheres were formed on the seed layer-coated substrate by using of gas-liquid-solid interfacial self-assembly method and drying in vaccum desicator for about a day to enhance the adhesion between seed layer and nanospheres. After that, zinc oxide nanowires were synthesized using a low temperature hydrothermal method based on alkali solution. The specimens were immersed upside down in the autoclave bath to prevent some precipitates which formed and covered on the surface. The hydrothermal conditions such as growth temperature, growth time, solution concentration, and additives are variously performed to optimize the morphologies of nanowire. To characterize the crystal structure of seed layer and nanowires, morphology, and optical properties, X-ray diffraction (XRD), field emission scanning electron microscopy (FE-SEM), Raman spectroscopy, and photoluminescence (PL) studies were investigated.