Effect of Several Exterior Adhesive Types on Dimensional Stability of Bamboo Oriented Particleboard

  • Iswanto, Apri Heri;Munthe, Rensus;Darwis, Atmawi;Azhar, Irawati;Susilowati, Arida;Prabuningrum, Dita Sari;Fatriasari, Widya
    • Korean Journal of Materials Research
    • /
    • v.29 no.5
    • /
    • pp.277-281
    • /
    • 2019
  • The objective of this research is to evaluate the effect of adhesive types on dimensional stability of bamboo-oriented particleboard. The materials used in this research are bamboo tali(Gigantochloa apus J.A & J.H. Schult. Kurz), UF/MDI(8, 10, 12 % level), and MF, MDI, and PF at 7 % level. Particle and adhesive are mixed using a blending machine; then, mat forming and hot pressing processes are performed using adhesive-suitable temperature and time references. MDI resin is set at $160^{\circ}C$ temperature for 5 minutes. PF resin and MF resin are pressed at $170^{\circ}C$ for 10 minutes, and $140^{\circ}C$ for 10 minutes, respectively, while UF/MDI sets at temperature of $140^{\circ}C$ for 10 minutes. The results show that particleboard using PF resin produces the lowest thickness swelling value. The particleboard using UF/MDI resin also produces good response for thickness swelling value. Interesting things happen in that UF/MDI adhesive produces a thickness swelling value better than that of MDI resin. FTIR analysis on particleboard bonded by UF/MDI resin combination shows the presence of carbonyl group C=O vibration on multi substitution of urea at wave number of around $1,700cm^{-1}$.

Study on the Physical and Mechanical Properties of Particleboard and Oriented Strandboard Manufactured by Tulliptree (Liriodendron tulipifera L.) (백합나무를 이용하여 제조한 3층 파티클보드와 배향성 스트랜드보드(OSB)의 물성에 관한 연구)

  • Seo, Jun won;Gang, Gil woo;Jo, Gun hee;Park, Heon
    • Journal of the Korean Wood Science and Technology
    • /
    • v.46 no.1
    • /
    • pp.67-72
    • /
    • 2018
  • This study was conducted to investigate a potential of Yellow poplar (Liriodendron tulipifera L.) as a raw material for the manufacturing of particleboard (PB) and oriented strandboard (OSB). PB panels were prepared at the parameters of $0.7g/cm^3$ density, 15 mm thickness, three-layer, $E_1$ grade urea-formaldehyde (UF) resin, emulsion wax, and hardener. OSB panels were manufactured with a density of $0.65g/cm^3$, thickness of 10 mm, and $E_1$ grade of UF resin. Particle size of the face layer of PB was 20~80 mesh with 7~9% moisture content (MC), while that of core-layer was 3~20 mesh with 3~5% MC, which was similar to the production condition of commercial PB. As a result, the manufactured PB panels with 15.8 mm thickness, $0.7g/cm^3$ density, and 5.8% MC satisfied the requirement of bending strength of 15 type PB of Korean Industrial Standard (KS F 3104). Both internal bonding (IB) strength and surface screw withdrawal resistance also satisfied the requirement of 18 type PB of the standard. But, the edge screw withdrawal resistance satisfied the requirement of 15 type PB of the standard. These differences in properties could be due to the slenderness ratio of raw particles. In case of OSB panels with 10.7 mm thickness, $0.68g/cm^3$ density, and 5.8% MC satisfied all the requirements of bending strength, screw withdrawal resistance, and IB strength of 18 type PB of the standard. These results suggest that Yellow poplar wood has a good potential as a raw material for the production of PB and OSB.

Effects of Wood Particles and Steel Wire Compositions on Physical and Mechanical Properties of the Boards (목재(木材)파아티클과 철선(鐵線) 복합체(複合體)가 보오드의 물리적(物理的) 및 기계적(機械的) 성질(性質)에 미치는 영향(影響))

  • Park, Heon;Lee, Pill-Woo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.14 no.1
    • /
    • pp.3-44
    • /
    • 1986
  • In order to obtain the basic physical and mechanical properties of steel wire reinforced particleboard, particleboards were formed with large particles through 2.11 mm (12 meshes) and retained on 1.27mm (20 meshes) sieves and small particles through 1.27mm (20 meshes) and retained on 0.42mm (60 meshes) sieves from the plywood mill wastes of meranti (Shorea spp.) in the form of pallmanchips, applying urea-formaldehyde resin as an adhesive on the particle surface in 10 percent on the oven dried weight of particles, and arranging steel wires of 1mm in diameter 5,10,15,20, and 25mm in longitudinal and transverse direction with crossing in the mid of the board depth in single layer boards, 10mm in longitudinal or transverse direction without crossing in two layers and 10mm in longitudinal and transverse directions with and without crossing in three steel wire layers boards. The stepwise 9-minutes-multi-pressing schedule in 5 minutes at 35 kgf/$cm^2$, 2.5 minutes at 25 kgf/$cm^2$. and 1.5 minutes at 15 kgf/$cm^2$ was applied for $300{\times}200{\times}13$mm board at the temperature of 160$^{\circ}C$ in a hot press. Specific gravity, thickness swelling, bending properties of modulus of rupture (MOR), modulus of elasticity(MOE), work to proportional limit, and work to ultimate load, internal bond (IB), and screw holding power(SHP) of the reinforced boards were analyzed on the wire openings and wire layers. The results obtained are summarized as follows; 1) In specific gravity, particleboards with large particles and small particles had higher value with more steel wire placements and more steel layers composition, 2) Particleboards with large particles in accordance with more steel wire liners composition gave very poor thickness swelling. 3) The mechanical properties of particleboards formed with large or small particles were reinforced with more steel wire layers. Therefore, bending strength was improved in modulus of rupture, modulus of elasticity, and work to ultimate load. Especiallv, particleboards with two or three steel wire layers showed the tension lamination effect when the steels in lower steel wire layer were oriented parallel to the board length. 4) The modulus of rupture, modulus of elasticity, and work to ultimate load in bending varied with opening area, distance of lengthwise wires multipled by distance of transverse wires. Particleboards formed with large particles resulted in higher value in modulus of rupture with 1.5-3 $cm^2$ opening area, 1-2cm distance between transverse wires, and 1.5-2.5cm distance between lengthwise wires. Particle boards formed with small particles showed higher value with 0.5-1.5$cm^2$ or 3.75-6.25 $cm^2$ opening area, 0.5 or 2.5cm distance between transverse wires. 5) In modulus of elasticity, particleboards formed with large particles with one steel wire layer suggested higher value with 5-3$cm^2$ opening area, 1-2.5cm distance between transverse wires and also 1-2.5 cm distance between lengthwise wires. Particleboards formed with small particles showed higher value with 0.75-1.25$cm^2$ or 3-6.25$cm^2$ opening area and 0.5 or 2.5cm distance between transverse wires. 6) Particleboards formed with large particles gaved higher value in work to ultimate load with 1-3$cm^2$ opening area. Particleboards formed with small particles showed increasing tendancy with decreasing opening area. 7) In internal bond and screw holding power, particleboards formed with large particles had increasing value in two and three steel wire layers compositions, but particleboards formed with small particles showed no difference. Particleboards formed with large particles containing one steel wire layer showed no difference in internal bond and screw holding power, and particleboards formed with small panicles containing one steel wire layer resulted in increasing value in internal bond and decreasing value in screw holding power in accordance with increase in opening area.