• Title/Summary/Keyword: seawater attack

Search Result 54, Processing Time 0.02 seconds

Assessment on the Seawater Attack Resistance of Antiwashout Underwater Concrete (수중불분리성 콘크리트의 해수침식에 대한저항성 평가)

  • 문한영;김성수;안태송;이승태;김종필
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.683-688
    • /
    • 2001
  • In case of constructing the concrete structures under seawater environment, the concrete suffers from deterioration due to penetration of various ions such as chloride, sulfate and magnesium in seawater. Tn the present study, Immersion tests with artificial seawater were carried out to investigate the resistance to seawater attack of antiwashout underwater concrete. From the results of compressive strength, it was found that blended cement concrete due to mineral admixtures such as fly ash(FA) and ground granulated blast-furnace slag(SGC), were superior to ordinary portland cement concrete with respect to the resistance to seawater attack. Moreover, XRD analysis indicated that the formed reactants of ordinary portland cement paste by sulfate and magnesium ions led to the deterioration of concrete. As expected, however, the blended cements with FA or SGC have a good resistance to seawater attack. This paper would discuss the mechanism of seawater deterioration and benefical effects of antiwashout underwater concretes with mineral admixtures.

  • PDF

Freeze-Thaw Resistance of Blended Cement Concrete using Seawater (해수를 사용한 혼합시멘트계 콘크리트의 동결융해 저항성)

  • 문한영;김성수;이승태;김종필;박광필
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.05a
    • /
    • pp.725-730
    • /
    • 2002
  • The durability of concrete involves resistance to freeze-thaw action, corrosion, permeation, carbonation, chemical attack and so on. Generally, properties of concrete have been well understood under the separate action of these deterioration mechanisms. However, in practice, the degradation of concrete usually is the result of combined action of physical and chemical attack and can be accelerated by the combined action of several deterioration mechanisms. In the present study, to evaluate the combined deterioration by freeze-thaw action and seawater attack, ground granulated blast-furnace slag or silica fume concrete with water or seawater as mixing water was exposed to 210 cycles of freeze-thaw action. Tests were conducted to determined the relative dynamic modulus of elasticity and compressive strength. Furthermore, The XRD, SEM and EDS analysis were performed on the deteriorated part of concrete due to freeze-thaw action and seawater attack.

  • PDF

Freeze-Thaw Resistance and Void Characteristic of Blended Cement Concrete using Seawater (해수를 사용한 혼합시멘트계 콘크리트의 동결융해 저항성 및 공극특성)

  • Kim, Seong-Soo;Lee, Seung-Tae;Jung, Ho-Seop;Park, Kwang-Pil
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.589-592
    • /
    • 2006
  • The durability of concrete involves resistance to freeze-thaw action, corrosion, permeation, carbonation, chemical attack and so on. Generally, properties of concrete have been well understood under the separate action of these deterioration mechanisms. However, in practice, the degradation of concrete usually is the result of combined action of physical and chemical attack and can be accelerated by the combined action of several deterioration mechanisms. In the present study, to evaluate the combined deterioration by freeze-thaw action and seawater attack, ground granulated blast-furnace slag or silica fume concrete with water or seawater as mixing water was exposed to 300 cycles of freeze-thaw action. Tests were conducted to determined the relative dynamic modulus of elasticity and compressive strength. Furthermore, The MIP analysis were performed on the deteriorated part of concrete due to freeze-thaw action and seawater attack.

  • PDF

A Experimental Study on the Seawater Attack Resistance of Grouting Mixtures (내해수성 주입재 배합에 관한 실험적 연구)

  • Chun, Byungsik;Choi, Dongchan;Kim, Younghun;Kim, Jinchun
    • Journal of the Korean GEO-environmental Society
    • /
    • v.11 no.1
    • /
    • pp.53-59
    • /
    • 2010
  • In seawater deposition condition, the corrosion and chemical attack of grouts are similar to those of concrete structure. Used in domestic MSG (Micro Silica Grouting) mixtured large amounts of silicate materials containing as cement powder is $8,000cm^2/g$ of the specific surface area or more due to the high hydration activity and high-strength, high durability, and features, $C_3A$ content of less than 5% to meet the standards chemical attack of seawater was evaluated as a cement material. Therefore, in this paper, with excellent seawater attack resistant MSG in combination with rapid hardening mineral was used, those of seawater characteristics were evaluated experimentally. Typically, sodium-silicate minerals or rapid hardening cements are used in domestic. About the homogel specimens with combination of MSG and rapid hardening agents for compressive strength, weight and length change characteristics were evaluated experimentally, and so we could present the excellent seawater resistant grouts combination.

A Study on the Resistance to Seawater Attack of Mortars and Concretes Incorporating Limestone Powder (석회석미분말을 혼입한 모르타르 및 콘크리트의 내해수성 연구)

  • Lee, Seung Tae;Jung, Ho Seop
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.15 no.1
    • /
    • pp.129-137
    • /
    • 2011
  • This study aims to evaluate the resistance to seawater attack of mortars and concretes incorporating limestone powder (0, 10, 20 and 30% of cement by mass). In order to achieve this goal, both chemical resistance by seawater and chloride ions penetration resistance of mortars or concretes were regularly monitored. From the test results, it was observed that the durability of cement matrix was greatly dependent on the replacement ratios of limestone powder. In other words, performance of cement matrix with 10% limestone powder was similar to that of OPC matrix. However, it was found that a high replacement ratio of limestone powder was ineffective to resist seawater attack.

Seawater Attack Resistance of Mortars Containing Mineral Admixtures (광물질혼화재 혼합 모르타르의 해수침식 저항성)

  • 문한영;이승태;최강식
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2002.10a
    • /
    • pp.527-530
    • /
    • 2002
  • In the present study, immersion test using artificial seawater was performed to evaluate the resistance of mortar specimens with or without ground granulated blast-furnace slag (SG) and fly ash (FA). Another variable was the fineness levels of SG (4,450, 6,000 and 8,000 ㎠/g). From the results of the immersion test for 270 days of exposure, the excellent resistance to seawater attack for SG mortar mixtures, especially in a high fineness levels, was confirmed. However, the reductions in compressive strength of FA mortar specimens was similar to those of OPC mortar specimens irrespective of replacement of FA.. In order to understand the deterioration mechanism due to seawater attack, X-ray diffraction (XRD) analysis were also carried out. Some reactants such as ettringite, gypsum, brucite and Friedel's salt were possibly detected through XRD technique.

  • PDF

Evaluation on the Deterioration and Resistance of Cement Matric due to Seawater Attack (시멘트 경화체의 해수침식에 의한 성능저하 및 저항성 평가)

  • 문한영;이승태;김홍삼
    • Journal of the Korea Concrete Institute
    • /
    • v.13 no.2
    • /
    • pp.175-183
    • /
    • 2001
  • Immersion tests with artificial seawater were carried out to investigate the resistance to seawater attack of 5 types of cement matrices. From the results of compressive strength and length change, it was found that blended cement mortars due to mineral admixtures, were superior to portland cement mortars with respect to the resistance to seawater attack. Moreover, XRD analysis indicated that the peak intensity ratio of low heat portland cement(LHC) paste, in portland cement pastes, had better results, and so did that of blended cement Paste. Pore volume of pastes by mercury intrusion porosimetry method demonstrated that total pore volume of ordinary portland cement(OPC) paste had a remarkable increase comparing with that of other pastes. In case of immersion of artificial seawater, the use of ground granulated blast-furnace slag and fly ash, however, showed the beneficial effects of 56% and 32% in reduction of total pore volume, respectively.

An expert system for making durable concrete for chemical exposure

  • Islam, Md. Nazrul;Zain, Muhammad Fauzi Mohd.;Basri, Hassan
    • Computers and Concrete
    • /
    • v.2 no.4
    • /
    • pp.293-307
    • /
    • 2005
  • The development and the main features of an expert system for modeling the requirements of durable concrete in chemical exposure, called the Durable Concrete Advisor for Chemical Exposure (DCACE), are described. The system was developed to help improve the quality of concrete exposed to chemical environment by minimizing mistakes and deficiencies in selecting concrete constituents. Using Kappa-PC expert system shell, an object-oriented model was developed where the rule-based reasoning operates on or across objects. The American Concrete Institute manual of concrete practice was chosen as the main source of knowledge. Other textual sources were also consulted for knowledge acquisition. The major objectives of the research were acquisition and formalization of the relevant knowledge and building an expert system for making durable concrete for chemical exposure regarding sulfate attack, acid attack, seawater attack and carbonation. Similar to most expert systems, this system has explanation facilities, can be incrementally expanded, and has an easy to understand knowledge base. The performance of the system is demonstrated by an example session. The system is user-friendly and can be used as an educational tool.

The Assessment of Chliride Attack of Concrete Structure in Marine Environment (해양환경하에 있는 콘크리트 구조물의 염해에 대한 고찰)

  • 문한영;김성수;류재석;김성섭
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 1996.04a
    • /
    • pp.83-88
    • /
    • 1996
  • Reinforced-concrete structures built on the seashore or in seawater are damaged from flying-salt of chloride ion in the seawater. Recently many bridges are being constructed under marine enviornment and there are many serious problems of chlofide attack owing to penetration of chloride ion. And up to now it has not only so little a seatch about damage from flying-salt and seawater but also little systematic study outcome about steel corrosion. In this study we investigate the concrete deterioration and steel corrosion of RC bridges on the seashore. Environmental conditions are investigated, and compressive strength, carbonation depth and steel-corrosion degree are measured.

  • PDF

A study on the distribution of airborne sea salt to the distance from seashore (해안으로부터 거리별 비래염분량의 분포에 대한 고찰)

  • Lee, Jong-Suk;Choi, Won-Sung;Moon, Han-Young
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2004.05a
    • /
    • pp.842-845
    • /
    • 2004
  • When the concrete structures are in contact with seawater, concentration of chloride for estimating chloride diffusion coefficient can be defined as the chloride concentration of sea water. However, in case the concrete structures, constructed in the seashore, aren't directly in contact with seawater, it is difficult to establish the interface concentration of chloride. In addition, marine concrete structures are greatly affected by salt attack such as rebar corrosion, among the cause of salt attack, airborne sea salt is primary factor. Therefore, in this study, salt attack environment by airborne sea salt was investigated in terms of the distance from seashore at 33 spots, 6 areas in East, West, South coast for 1 year. Results indicated that airborne sea salt is decreased by $y=a{\cdot}x^{-b}$ equation to the distance from seashore.

  • PDF