A Study on the Sericin Fixation of Raw Silk Fibers by Fixing with the Mixtures of Various Amines and Formalin (아민류와 포르말린 혼합액에 의한 실크 생사의 세리신 정착에 관한 연구)

  • Park, Geon-Yong
    • Textile Coloration and Finishing
    • /
    • v.21 no.1
    • /
    • pp.67-72
    • /
    • 2009
  • To investigate the strong and effective sericin fixing agents and conditions, raw silk fibers were treated with the mixtures of urea-formalin, thiourea-formalin and melamine-formalin as sericin fixing agents, respectively. And the treated raw silk fibers were degummed by the degumming liquors of alkaline detergent and sodium carbonate to confirm the hardness of sericin fixation. The weight of raw silk fibers was decreased in the process of sericin fixation treating at 80$^{\circ}C$ for 60min. The effective sericin fixation was obtained by treating at $60{\sim}80^{\circ}C$ for 15min with the mixture of melamine and formalin. The mixture of melamine and formalin showed an outstanding ability of sericin fixation because the three amino groups of melamine were able to cross-link the hydroxy amino acids of sericin such as serine with the assistance of formalin.

The Influence of Additives Added to the Melamine and Formalin Mixtures on Sericin Fixation of Raw Silk Fibers (멜라민과 포르말린 혼합액의 첨 가제들이 실크 생사의 세리신 정착에 미치는 영향)

  • Park, Geon-Yong
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.10 no.2
    • /
    • pp.412-417
    • /
    • 2009
  • In order to investigate the effective sericin fixation of raw silk fibers the influence of various additives added to the melamine and formalin mixtures on sericin fixation was studied. When raw silk fibers were treated with wetting agent but without subsequent washing before sericin fixation, the strong sericin fixation was obtained by fixing sericin. Adding hydrogen peroxide to the melamine and formalin mixture made sericin fixation worse, resulting weaken the sericin hardness of fixed raw silk fibers and tight bonding of the fibers. On the other hand, it was confirmed that adding sodium hydrosulfite to the melamine and formalin mixtures gave better sericin hardness of fixed raw silk fibers without the bonding of fibers. Supplying additional melamine with he low concentration of sodium hydroxide to the melamine and formalin mixture(melamine:formalin= 1:6) resulted in very good sericin fixation. But adding hydrochloric acid or methanol to the same mixture had no effect on the sericin fixation, and adding magnesium chloride to it made the hardness of sericin fixation even worse.

The Study on the Sericin Fixation by Formalin and Glutaraldehyde Mixture (Formalin과 Glutaraldehyde 혼합 처리에 의한 세리신정착)

  • 배도규
    • Journal of Sericultural and Entomological Science
    • /
    • v.36 no.2
    • /
    • pp.152-156
    • /
    • 1994
  • The sericin fixation of raw silk by formalin and glutaraldehyde mixed solutions was done and the effect of sericin fixtion by various conditions on degumming ratio, whiteness and physical properties was investigated and discusse. The obtained results were summarized as follows ; The sericin fixation by 1% formalin solution and upward, regardlles the concentration of glutaraldehyde solution, improved the whitenes of raw silk to 96% level of non fixed raw silk. The decrease of whiteness by degumming was prevented effectively by treatment of formalin and glutaraldehyde mixed solutions. The complete sericin fixation was obtained by the treatment of mixed solution including above 0.5% formalin solution. The proper treatment of sericin fixation can make increase the values of tenacity and elongation of silk.

  • PDF

Sericin-Fixed Silk Fiber as an Immobilization Support of Enzyme

  • Lee Ki Hoon;Kang Gyung Don;Shin Bong Seob;Park Young Hwan
    • Fibers and Polymers
    • /
    • v.6 no.1
    • /
    • pp.1-5
    • /
    • 2005
  • In this study, we attempted to evaluate a novel use of sericin-fixed silk fiber (SFx) as an immobilization support of enzyme. Sericin was fixed on the silk fiber using glutaraldehyde as a fixation reagent. After 6 hours of fixation, the degree of fixation increases linearly with linear decrease of the amount of bound $\alpha$-chymotrypsin (CT). This suggests that the increase of the degree of fixation is due to the further crosslinking of free aldehyde groups on the surface of sericin-fixed silk fiber (SFx). Even though perfect fixation was not achieved, sericin did not dissolve seriously and could be removed by further washing. The specific activity did not differ significantly after 6 hours of fixation. The activity of immobilized CT on SFx decreased to its half after 6 hours of incubation at 50$^{\circ}C$. However, it retained $78\%$ of initial activity even after 1 hour of treat­ment with $100\%$ ethanol. As a result, the SFx could be used as an immobilization support of enzyme in non-aqueous media at ambient temperature.

The Study on the Sericin Fixation Mechanism (세리신 정착 기구에 관한 연구)

  • 배도규
    • Journal of Sericultural and Entomological Science
    • /
    • v.37 no.2
    • /
    • pp.137-141
    • /
    • 1995
  • The sericin fixation of raw silk by glutaraldehyde solutions with catalyst(serifix B) was done and the effect of sericin fixation by catalyst on reaction mechanism, whiteness and physical properties were investigated and discussed. The obtained results were summarized as follows; 1) The complete sericin fixation were obtained by glutaraldyhyde solution regardless the concentration of catalyst. 2) The tenacities of sericin fixed silk increased in comparison with that of nontreated silk. 3) There were not constant tendency in elongation of sericin fixed silk in comparison with nontreated silk. 4) The whiteness of sericin fixed silk treated glutaral-silk in comparison with nontreated silk. 5) FT-IR spectra were quite different from sericin fixed reagent and catalyst.

  • PDF

Fixation of Sericin of Silk Fabric by Epoxy Resin (Epoxy수지에 의한 견직물의 Sericin정착)

  • 문영배;남중희
    • Journal of Sericultural and Entomological Science
    • /
    • v.26 no.2
    • /
    • pp.16-25
    • /
    • 1984
  • The sericin fixation of silk fabrics by epoxy resins was studied in the presence of aqueous salt solution in different solvents at the indicated temperature for the desired time. Heavy weight gains were obtained in the reaction with glycerol diglycidyl ether (EX-313) and ethylene glycol diglycidyl ether (EX-810) catalyzed by potassium thiocyanate in such solvents as carbon tetrachloride and p-chloroethylene. The obtained results were summarized as follows; 1) The tested resins were found similar in reaction behavior to silk fabric. The effect of fixation and weight gains was higher in EX-810 than EX-313. 2) The weight gains were increased with reaction time and temperature, and degumming ratio reached a constant value in 90 min at 70$^{\circ}C$. 3) The weight gains and the degumming ratio reached an equilibrium at 3-5% of epoxy concentration. 4) The weight gains were remarkably influenced and increased by the concentration of salt solution. The degumming ratio reached an equilibrium over 0.5N concentration of salt. 5) The weight gains were increased with the dipping time in gently-sloping. The degumming ratio reached an equilibrium over 15 min dipping. 6) The effect of sericin fixation of hydrophobic solvents, such as Carbon Tetrachloride, p-Chloroeth-ylene, Cyclohexane, Xylene and Toluene, was found suitable. 7) The effect of drying temperature was not remarkable on the weight gains and the degumming ratio. 8) There was a slight decrease in the moisture regain of sericin-fixed silk and it may be possible to maintain the moisture regain in the sericin-fixed silk by the epoxy resins. 9) The results on testing physical properties of sericin-fixed silk fabric were as follows; The crease recovery was almost not different from undegummed fabric, but inferior to degummed fabric. The tensile strength was improving in accordance with the effect of sericin fixation, either the elongation did.

  • PDF

Sericin- Fixation of Raw Silk by Graft Copolymerization (Graft 공중합에 의한 생사 Sericin 정착)

  • 김신덕
    • Journal of Sericultural and Entomological Science
    • /
    • v.20 no.2
    • /
    • pp.40-44
    • /
    • 1978
  • Cerium (IV) ion-initiated graft copolymerizations of acrylonitrile to raw silk were investigated in an effort to carry out sericine-fixation. The change in ceric ammonium nitrate concentration exhibited a maximum in percentage of grafting at 0.003M. Also observed was that the change in nitric acid content in reaction media gave a maximum in percentage of grafting at 0.1M. Percentage of grafting was increased generally with increase in acrylonitrile concentration, reaction time and reaction temperature. Raw silk sericin grafted with acrylonitrile was not de gummed by boiling off test and optimum graft percentage was considered at 20%.

  • PDF

The Effect of Fixing Agents and Softner on Sericin Fixation of Trimethylolmelamine (트리메틸올멜라민의 세리신 정착에 있어 정착제와 유연제의 영향)

  • Park, Geon-Yong
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.18 no.5
    • /
    • pp.93-98
    • /
    • 2017
  • The fixing behaviors of raw silk yarns treated with melamine and formaldehyde at a molar ratio of 1:3 for trimethylolmelamine were investigated. Sericin was fixed during the fixing process, but a part of sericin I was removed simultaneously by hot water. The weight losses by fixing and the degumming losses by degumming greatly decreased with increasing concentrations of melamine and formaldehyde. The silk yarns fixed with 0.011 M melamine and 0.033M formaldehyde were significantly degummed due to the insufficient fixation of sericin and the alkaline hydrolysis of sericin by sodium carbonate during the degumming process. On the other hand, the silk yarns fixed with 0.055M melamine and 0.165M formaldehyde were degummed slightly (the degumming losses of 3-8%) due to the strong fixation of sericin, which might result from the many cross-linkages between the sericin I molecules, which were formed by trimethylolmelamine. Those fixed with the fixing solution containing 15% owf softener showed the lowest weight and degumming losses because under the condition of 15% owf softener, the cation of the softener can effectively form ionic bonds with the negatively charged side chain of aspartic acid in sericin. In addition, van der Waals' forces may be also formed between the hydrophobic tail of the softener and the hydrophobic region of sericin, which may help inhibit the removal of sericin I.

Studies on Sericin Fixation by Use of Alum Meal (명반처리에 의한 견직물개선연구 -Sericin 정착을 중심으로 하여-)

  • 최병희;남중희
    • Journal of Sericultural and Entomological Science
    • /
    • v.21 no.2
    • /
    • pp.11-19
    • /
    • 1979
  • This has been carried out how the sericin insoluble fixations of raw silk should be with potassium alum. This is learned from the leather tanning technique which the process works with collagen, a kind of proteins. Former reports had shown such works, however, they did not consider the moisture absorbability after their process reports by using chromium alum, formalin or vinyl acetate grafting. This report, however, paid attention to protect such absorbability as well as sericin fixation, so far it may be useful for plactical use of silk. In order to clear how the sericin is fixed with such chemicals, fundermental mechanism of weding process and chemical reaction against proteins were also discussed. The obtained results of the report are as followings. 1. Alum should not be treated for raw silk with high temperature bath like other reports because such treat induces raw silk to be stiffly after the treat. 2. It is recommended that raw silk should be treated with alum solution at room temperature for more than three hours. Even in this case, the use of only alum with raw silk could to fix sericin some how, but it increased the water proofness of the silk. 3. 1% of alum solution was found to be able to fix the sericin of raw silk. 4. In case we consider only sericin fixations, a combination treat of 1% alum for three hours and 0.5% NaOH for ten minutes method showed the best result. 5. In case we consider sericin insoluble fixation and moisture absorbility, the reversive combination of the above process was found to be the best results. 6. Sericin fixing evidence was shown with drying feature curves of wed each treated silk where we could to analyze how the chemical nature is changed after each treat. 7. Deguming ratio may be obtained up to 4.3% after the alum combination treat with regular raw silk. Such ratio was considered to be good enough for the purpose when the textile is washed with warm soap water. 8. Moisture absorbability of the combination treat of alum and NaOH was found to be good enough as well as non treated silk. 9. The tenacity and elongation of the treated silk did not change even after three month. 10. Above all, this method is considered to be better process than other coloured fixing (tannin method. Cr-alum method) or smell fixing (formalin method. vinyl acetate method).

  • PDF

Fixation of Silk Sericin (Sericin 정착에 관하여)

  • 남중희;김신덕
    • Journal of Sericultural and Entomological Science
    • /
    • v.20 no.2
    • /
    • pp.45-49
    • /
    • 1978
  • Sericin 정착은 친수성 단백질인 세리신을 화학처리에 의하여 소수성으로 변화시켜 fibroin 에 밀착, 응고시켜 생사를 양모와 유사한 섬유로 변화시켜 제품의 다양화를 기할 목적으로 많이 행하여졌으며 이에 따른 증량효과도 크게 기대되어진다. 종래의 세리신 정착방법들은 생사의 제리신 정착외에 공업적으로 그 가치가 크게 인정되었던 견사, 생사 층 등에도 광범위하게 응용되어 많은 특허가 있는데 이들 정착방법을 대별하면 (1) Aldehyde 처리에 의한 세리신 정착 (2) Cr 감류처리에 의한 세리신 정착 (3) Epoxy 화합물의 처리에 의한 세리신 정착 (4) 합성수지 처리에 의한 세리신 정착등을 들 수 있겠으며 그 중에서도 특히 Aldehyde 에 의한 정착 (주로 formaldehyde 사용) 과 Cr 감류에 의한 정착이 가장 많이 행해진 경향을 보인다. (중략)

  • PDF