• Title/Summary/Keyword: specified splice strength

Search Result 10, Processing Time 0.025 seconds

Compression Lap Splice Length in Concrete of Compressive Strength from 40 to 70 MPa (40-70 MPa 콘크리트에서의 철근 압축이음 길이)

  • Chun, Sung-Chul;Lee, Sung-Ho;Oh, Bo-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.21 no.4
    • /
    • pp.401-408
    • /
    • 2009
  • A compression lap splice becomes an important issue due to development of ultra-high strength concrete. Current design codes regarding compression lap splice do not utilize merits of the improved strength of ultra-high strength concrete. Especially, a compression lap splice can be calculated longer than a tension lap splice according to the codes because they do not consider effects of compressive strength of concrete and transverse reinforcement. This anomaly confuses engineers in practice. Design equation is proposed for compression lap splice in 40 to 70 MPa of compressive strength of concrete. The proposed equation is based on 51 specimens conducted by authors. Basic form of the equation includes main parameters which are derived from investigating test results. Through two-variable non-linear regression analysis of measured splice strengths, a strength equation of compression lap splices is then derived. A specified splice strength is defined using a 5% fractile coefficient and a lap length equation is constructed. By the proposed equation, the anomaly of lap lengths in tension and compression is got rid of. In addition, the equation has a reliability equivalent to those of the specified strengths of materials.

Simplified Design Equation of Lap Splice Length in Compression

  • Chun, Sung-Chul;Lee, Sung-Ho;Oh, Bo-Hwan
    • International Journal of Concrete Structures and Materials
    • /
    • v.4 no.1
    • /
    • pp.63-68
    • /
    • 2010
  • With the emergence of ultra-high strength of concrete, the compression lap splice has become an important area of interest. According to ACI 318-08, a compression splice can be longer than a tension splice when high-strength concrete is used. By reevaluating the test results of compression splices and performing regression analysis, a simplified design equation for splice length in compression was developed based on the basic form of design equations for development/splice lengths of deformed bars and hooks in tension. A simple linear relation between $l_s/d_b$ and $f_{sc}\sqrt{f'_c}$ was assumed, and yields good values for the correlation coefficient and the mean and the COV (coefficient of variation) of the ratios of tests to predictions of splice strengths in compression. By including the 5% fractile coefficient of 0.83, a design equation for splice length in compression was developed. The splice length calculated using the proposed equation has a reliability that is equivalent to other provisions for reinforcing bars.

Design Equations of Compression Splice Strength and Length in Concrete of 100 MPa and Less Compressive Strength (100 MPa 이하 콘크리트의 철근 압축 이음 강도와 이음 길이 설계)

  • Chun, Sung-Chul;Lee, Sung-Ho;Oh, Bo-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.2
    • /
    • pp.211-217
    • /
    • 2011
  • Although a compression splice length does not need to be longer than a tension splice length due to end bearing effect, current design codes impose a longer compression lap splice than a tension lap splice in high strength concrete. Hence, new criteria for the compression lap splice including concrete strength effect need to be found for economical design of ultra-high strength concrete. An experimental study has been conducted using column specimens with concrete strength of 80 and 100 MPa with transverse reinforcement. The test results showed that splice strengths improved when the amount of transverse reinforcement increased. However, end bearing strength did not increase when larger amount of transverse reinforcement is provided within the spliced zone. Therefore, the splice strength enhancement was attributed to the improvement of bond. From regression analysis of 94 test results including specimens made with concrete strength of 40 and 60 MPa, a new design equation is proposed for compression lap splice in the concrete compressive strength ranging from 40 to 100 MPa with transverse reinforcement. By using the proposed equation, the incorrect design equations for lap splice lengths in tension and compression can be corrected. In addition, the equation has a reliability equivalent to those of the specified strengths of materials.

Capacity and Length of Compression Lap Splice in Unconfined Concrete of 100MPa and Less Compressive Strength (횡보강근이 없는 100 MPa 이하 콘크리트의 철근 압축이음 강도와 이음길이)

  • Chun, Sung-Chul;Lee, Sung-Ho;Oh, Bo-Hwan
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.5
    • /
    • pp.659-666
    • /
    • 2010
  • Although the compression splice needs not be longer than the tension slice due to existence of end bearing, current design codes impose a longer compression lap splice than a tension lap splice in high strength concrete. Hence, new criteria for the compression lap splice including the effects of concrete strength need to be sought for economical design involving ultra-high strength concrete. An experimental study has been conducted with column specimens in concrete strength of 80 and 100 MPa. Test results show that the splice strength can be evaluated to be proportional to square root of compressive strength of concrete. Bar stress developed by end bearing is not affected by splice length and is expressed with a function of the square root of concrete strength. Mean value of stresses developed by end bearing is 16.5 square root of $f_{ck}$. The stresses developed by bond in compression splices are nearly identical to those in tension splices and, therefore, strength increment of compression splices is attributed to end bearing only. From regression analysis of 58 tests, a design equation is proposed for compression lap splice in 40 to 100 MPa of compressive strength of concrete. By the proposed equation, the anomaly of lap lengths in tension and compression is got rid of. In addition, the equation has a reliability equivalent to those of the specified strengths of materials.

Applicability of Current Design Code to Class B Splice of SD600 Re-Bars (SD600 철근의 B급 겹침 이음에 대한 현행설계기준의 적용성)

  • Choi, Won-Seok;Chung, Lan;Kim, Jin-Keun;Park, Hong-Gun
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.4
    • /
    • pp.449-459
    • /
    • 2011
  • An experimental study was performed to evaluate the applicability of current design code to the class B splice of SD600 reinforcing bars. Twelve simply supported beam and slab specimens with re-bar splices were tested under monotonic loading. Parameters for this test were re-bar diameter, concrete cover thickness, concrete strength, and stirrup spacing. Concrete strengths ranged 24.7~55.3 MPa. Most of the specimens were designed to satisfy the class B splice length specified by current design code. Average bar stresses resulting from this test were compared with the predictions by the KCI code provisions. Based on the result, the applicability of the current design code to SD600 re-bars were evaluated. The re-bar splices gave satisfactory performance for all D13 re-bar splices and for D22 and D32 splices with transverse reinforcement. On the basis of the test result, for D22 and the greater diameter bars, the use of either transverse reinforcement of the thicker concrete cover was recommended.

Evaluation on Structural Performance of Precast Bridge Deck Joint using HSFRC (고강도 강섬유보강콘크리트를 적용한 프리캐스트 바닥판 이음부의 구조성능 평가)

  • Lee, Han-Joo;Chung, Chul-Hun;Shin, Dong-Ho;Park, Se-Jin;Kim, In-Gyu
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.21 no.6
    • /
    • pp.196-205
    • /
    • 2017
  • In precast deck system, structural performance and serviceability are mostly determined by the connection methods between the precast decks. This study proposes precast deck system with asymmetric ribbed connection details using High Strength Fiber Reinforced Concrete(HSFRC) with filler. To verify the proposed method, the flexural performance experiment was carried out with variation of joint cross section type and splice rebar details. From the test results, regardless of joint details, spliced tensile rebars of specimens were deformed to yielding strain level. Also, all types of specimens resulted in sufficient flexural performance. These test results show that the minimum lap splice length specified in current Korea Highway Bridge Design Code is conservative for precast deck joint using HSFRC. Therefore, splice details can be simplified and joint width can be reduced by using HSFRC with filler between the precast decks, and the proposed precast deck systems can be applied to the connection part of precast decks effectively.

Experimental Study on Lap Splice of Headed Deformed Reinforcing Bars in Tension (인장력을 받는 확대머리 이형철근의 겹침이음에 관한 실험적 연구)

  • Kim, Seung-Hun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.18 no.5
    • /
    • pp.59-67
    • /
    • 2014
  • In tension lap splices of straight deformed bars, KCI Code (KCI2012) and ACI Code (ACI318-11) requires that the lap lengths for class B splice are 1.3 times as development length. KCI2012 contains development length provisions for the use of headed deformed bars in tension and does not allow their tension lap splices. The purpose of this experimental study is to evaluate that KCI2012 equation for the development length, $l_{dt}$, of headed bars can be used to calculate the lap length, $l_s$, of headed deformed bars in grade SD400 and SD500, having specified yield strength of 400 and 500 MPa. Test results showed that specimens with $l_s$ equal to $1.3l_{dt}$ had maximum flexural strengths as 1.16~1.31 times as the nominal flexural strengths, flexural failure mode, and ductility. These observations indicate that $1.3l_{dt}$ is suitable to the tensile lap length of headed deformed bars in grade SD400 and SD500.

Behavior of tension lap spliced sustainable concrete flexural members

  • Al-Azzawi, Adel A.;Daud, Raid A.;Daud, Sultan A.
    • Advances in concrete construction
    • /
    • v.9 no.1
    • /
    • pp.83-92
    • /
    • 2020
  • The use of spliced reinforcing bars in sustainable concrete members to manage inadequate bars length is a common practical issue which is may be due to some limitations. The lap splicing means two bars overlapped in parallel with specified length called the splice length in order to provide the required bond between the two bars. The bond between sustainable concrete and spliced steel bars is another important issue. The normal strength sustainable concrete specimens of sizes 1700×150×150 mm with tension reinforcement lap spliced were selected according to testing device length limitations. These members were designed to fail in flexure in order to investigate the lap spliced tension bars effect. The selected lap spliced tension bars were of 10 mm size with smooth and deformed surfaces in order to investigate the surface nature accompanied with the splice nature. The sustainable concrete mechanical properties and mix workability were also studied. This study reveals that the effect of number of spliced bars on the response of beams reinforced with smooth bars is found to be more obvious than deformed one. Finite element modeling in three dimensions was carried out for the tested beams using ABAQUS software. A parametric study is carried out using finite elements on considering the following parameters, concrete compressive strength, load type and opening in cross section (hollow section) for weight reduction purposes.The laboratory and numerical results show good agreements in terms of ultimate load and deflection with an average difference of 10% and 15% in ultimate load and deflection respectively.

Seismic Performance Evaluation of Dry Precast Concrete Beam-Column Connections with Special Moment Frame Details (특수모멘트골조 상세를 갖는 건식 프리캐스트 콘크리트 보-기둥 접합부의 내진성능평가)

  • Kim, Seon Hoon;Lee, Deuck Hang;Kim, Yong Kyeom;Lee, Sang Won;Yeo, Un Yong;Park, Jung Eun
    • Journal of the Earthquake Engineering Society of Korea
    • /
    • v.27 no.5
    • /
    • pp.203-211
    • /
    • 2023
  • For fast-built and safe precast concrete (PC) construction, the dry mechanical splicing method is a critical technique that enables a self-sustaining system (SSS) during construction with no temporary support and minimizes onsite jobs. However, due to limited experimental evidence, traditional wet splicing methods are still dominantly adopted in the domestic precast industry. For PC beam-column connections, the current design code requires achieving emulative connection performances and corresponding structural integrity to be comparable with typical reinforced concrete (RC) systems with monolithic connections. To this end, this study conducted the standard material tests on mechanical splices to check their satisfactory performance as the Type 2 mechanical splice specified in the ACI 318 code. Two PC beam-column connection specimens with dry mechanical splices and an RC control specimen as the special moment frame were subsequently fabricated and tested under lateral reversed cyclic loadings. Test results showed that the seismic performances of all the PC specimens were fully comparable to the RC specimen in terms of strength, stiffness, energy dissipation, drift capacity, and failure mode, and their hysteresis responses showed a mitigated pinching effect compared to the control RC specimen. The seismic performances of the PC and RC specimens were evaluated quantitatively based on the ACI 374 report, and it appeared that all the test specimens fully satisfied the seismic performance criteria as a code-compliant special moment frame system.

Time Dependent Reduction of Clamping Forces of High Strength Bolt F13T (시간에 따른 F13T 고장력 볼트의 체결력 감소)

  • Jo, Jae Byung;Seong, Taek-Ryong
    • KSCE Journal of Civil and Environmental Engineering Research
    • /
    • v.29 no.4A
    • /
    • pp.291-297
    • /
    • 2009
  • Relaxation of high strength bolts was investigated. Block type and splice type specimens were fabricated with different types of bolts and different clamping lengths. Bolts were tightened to the specified torque. Clamping forces were measured through strain gauges installed on the shafts of bolts, while specimens were kept in a constant temperature and humidity. In all cases, ratio of clamping force reduction is less than 10%. Test results of different types of specimens and bolts and different clamping lengths were compared each other by using a simple model, which is suggested in this study for the estimation of bolt relaxation. The suggested model shows reasonably good agreements with test results for all cases. No difference is found between F13T and F10T bolts, but Dacro coated bolts shows higher relaxation than black bolts by approx. 30%. And also the comparison of test results shows that ratios of bolt relaxation become larger as clamping lengths of bolt shorter and the number of faying surfaces greater.