In recent year, Ferroelectric BLT($Bi_{4-x}$La$_{x}$Ti$_3$O$_{12}$) is a promising candidate materials. This study was Practiced to make good conditions of BLT targets. In this study, calcination and sintering temperature were kept at 75$0^{\circ}C$, 110$0^{\circ}C$ for 2 hour respectively. the density obtained 7.612, 7.98, 7.877 g/㎤ as La$_2$O$_3$ contents were 0.0mol%, 0.25mo1%, 0.5mol%. Especially, the lanthanum content of 0.5 mol% measured C-axis (117) preferred orientation more than the others targets in the XRD. In $\varepsilon$$_{r}$-f relationship using by HP 4194 A impedance analyzer, the 0.5 mol% observed above 200 relative dielectric constant. but the dissipation factor was higher than others targets at 100Hz~13MHz range. SEM photograph with the content of La$_2$O$_3$ was observed like rod and plate types.types.s.

Keywords