AN EXPERIMENTAL STUDY ON THE EFFECT OF DENTINAL PRETREATMENT ON BOND STRENGTH BETWEEN GLASS IONOMER CEMENT AND DENTIN

상아질 전처리 방법이 상아질과 Glass Ionomer Cement간의 결합강도에 미치는 영향에 대한 실험적 연구

  • Chung, Sang-Baek (Department of Conservative Dentistry, College of Dentistry, Wonkwang University) ;
  • Im, Mi-Kyung (Department of Conservative Dentistry, College of Dentistry, Wonkwang University)
  • 정상백 (원광대학교 치과대학 치과보존학교실) ;
  • 임미경 (원광대학교 치과대학 치과보존학교실)
  • Published : 1992.10.25

Abstract

This is a study on the effect of the dentinal pretreatment method to the bond strength between dentin and glass ionomer cement. In this study, 196 human molar teeth with sound crown were used. The dentin surfaces of these teeth were exposed with wet trimmer and polished with # 800 Emory paper and teeth were divided into 7 groups according to the pretreatment agent and method. Each group has 4 subroups of the kinds of glass ionomers. The shear bond strength were measured by Instron Universal Testing machine model 1122. The data of the evaluations were then subjected to statistical analysis using one way ANOVA and the result were as follows : 1. In Durelon liquid 20 sec scrubbing & Vitrebond filling subgroup, shear bond strength was highest with measurements of 72.41(kg/$cm^2$) and in no pretreatment & Shofu lining cement filling subgroup, lowest with measurements of 4.77(kg/$cm^2$). 2. In no pretreatment group, statistical significant differences were found between the subgroups of G-C lining cement and Shofu lining cement. 3. In Ketac conditioner 20 sec scrubbing group, Vitrebond were bonded stronger than others, and in Ketac conditioner 10 sec passive contact group, it has the significant difference with other glass ionomers except G-C lining cement. 4. The subgroup og G-C dentin conditioner 20 sec scrubbing & G-C lining cement filling was bonded to dentin stronger than the subgroup of no pretreatment & Shofu lining cement. In G-C dentin conditioner groups, both of 10 sec passive contact and 20 sec scrubbing, Vitrebond has highest bond strength among the subgroups. 5. The subgroup of Durelon liquid 10 sec passive contact & G-C lining cement filling was bonded to dentin stronger than the subgroup of no pretreatment & Shofu lining cement. Also in both Durelon liquid groups, Vitrebond were bonded to dentin with the highest strength among the subgroups.

Keywords