Characteristics of Grain Orientation and Grain Boundaries of the $ZrB_2$-ZrC Composites Densified by Spark Plasma Sintering

방전플라즈마소결법으로 제조된 $ZrB_2$-ZrC 복합체의 결정립 방위분포 및 결정입계의 특성

  • Shim, Seung-Hwan (Department of Ceramic Engineering, CPRC, Hanyang University) ;
  • Kim, Kyoung-Hun (Department of Ceramic Engineering, CPRC, Hanyang University) ;
  • Shim, Kwang-Bo (Department of Ceramic Engineering, CPRC, Hanyang University)
  • 심승환 (한양대학교 세라믹공학과) ;
  • 김경훈 (한양대학교 세라믹공학과) ;
  • 심광보 (한양대학교 세라믹공학과)
  • Published : 2001.10.31

Abstract

The grain orientation distribution and grain boundary characterization of $ZrB_2$-ZrC composites sintered by a SPS(Spark Plasma Sintering) method, a new sintering technique were analyzed by the EBSP technique and then their crystallographic results have been compared with those of a sintered specimen using a PLS(Pressureless Sintering) method. In the $ZrB_2$-ZrC composite manufactured by SPS, (0001) planes of $ZrB_2$ were oriented in the direction normal to the specimen surface. In the case of PLS, those of $ZrB_2$ were oriented normal to the electron beam. In both cases of PLS and SPS, ZrC grains had the randomly oriented grain structure. The grain boundary characterization showed that low angle grain boundaries in the PLS and SPS processed materials constituted about 10% and 8% of the total number of boundaries, respectively, represented the only slight difference between the proportion of low angle grain boundary. However, in the distribution of CSL(Coincident Site Lattice) boundaries, it was shown the higher proportion of CSL boundaries with $\Sigma$ 3,5,7,9, 11 in the SPS processed material.

새로운 소결법인 방전플라즈마소결법(SPS: Spark Plasma Sintering)으로 제조된 $ZrB_2$-ZrC 복합체의 결정립 방위분포 및 결정입계의 특성을 EBSP(Electron Back-Scattered Pattern)법으로 분석하여 상압소결법(PLS, Pressureless Sintering)에 의한 시편과 비교하였다. 방전플라즈마 소결법으로 제조된 시편의 $ZrB_2$ 결정립은 상압소결된 시편과는 다르게 (0001)면이 시편표면에 수직한 배향(normal direction)을 나타냈으며, ZrC 결정립은 두 경우 무질서한 배향을 나타냈다. 결정입계 특성 분석에서 low angle $(<15^{\circ})$의 분포는 상압소결법인 경우 전체 입계 중 약 10%, 방전플라즈마 소결법은 8%로 두 소결체에서 큰 차이를 보이지 않았으나, CSL(Coincident Site Lattice) 입계의 분포에서는 방전플라즈마 소결법으로 제조된 복합체에서 $\Sigma$ 3,5,7,9,11의 CSL 분포가 상압소결법에 비해 높은 분율을 나타냈다.