Abstract

Alumina/silver nanocomposites were fabricated using a soaking method through a sol-gel route to construct an intra-type nanostructure. The pulse electric-current sintering (PECS) technique was used to sinter the nanocomposites. Several specimens were annealed after sintering. The microstructure, mechanical properties, critical frontal process zone (FPZ) size, and thermo-mechanical properties of the nanocomposites were estimated. The relative densities of the specimens sintered at 1350 and $1450^{\circ}C$ were 95% and 99%, respectively. The maximum value of the three-point bending strength was found to be 780 MPa for the $2{\times}2{\times}10 mm$ specimen sintered at $1350^{\circ}C$. The fracture toughness of the specimen sintered at $1350^{\circ}C$ was measured to be $3.60 MPa{\cdot}m^{1/2}$ using the single-edge V-notched beam (SEVNB) technique. The fracture mode of the nanocomposites was transgranular, in contrast to the intergranular mode of monolithic alumina. The fracture morphology suggested that dislocations were generated around the silver nanoparticles dispersed within the alumina matrix. The specimens sintered at $1350^{\circ}C$ were annealed at $800^{\circ}C$ for 5 min, following which the maximum fracture strength became 810 MPa and the fracture toughness improved to $4.21 MPam^{1/2}$. The critical FPZ size was the largest for the specimen annealed at $800^{\circ}C$ for 5 min. Thermal conductivity of the alumina/silver nanocomposites sintered at $1350^{\circ}C$ was 38 W/mK at room temperature, which was higher than the value obtained with the law of mixture.

Keywords

References

  1. D. O'Sullivan, M. Poorteman, P. Descamps, F. Cambier, A. Leriche, and B. Thierry, 'Optimization of Alumina-Silicon Carbide Dispersion and the Fabrication of Nanocomposites Ceramic Materials,' Key Eng. Mater., 9-100 247-56 (1995)
  2. R. W. Davidge and T. J. Green, 'The Strength of Twophase Ceramic/glass Materials,' J. Mater. Sci., 3 629-34 (1968) https://doi.org/10.1007/BF00757910
  3. K. Niihara, 'New Design Concept of Structural Ceramicsceramic nanocomposites,' J. Ceram. Soc. Jpn., 99 974-81 (1991) https://doi.org/10.2109/jcersj.99.974
  4. K. Niihara and A. Nakahira, 'Particulate Strengthened Oxide Ceramics-Nanocomposites'; pp. 637-44, Advanced Structural Inorganic Composites, P. Vincenzini (Editor), Elsevier Science Publishers B. V., 1991
  5. M. Nawa, T. Sekino, and K. Niihara, 'Microstructure and Mechanical Properties of $Al_2O_3/Mo$ Nanocomposites,' Japan Society of Powder and Powder Metallurgy, 39 [12] 1104-8 (1992) https://doi.org/10.2497/jjspm.39.1104
  6. T. Ohji, Y. K. Jeong, Y. H. Choa, and K. Niihara, 'Strengthening and Toughening Mechanisms of Ceramic Nanocomposites,' J. Am. Ceram. Soc., 81 [6] 1453-60 (1998) https://doi.org/10.1111/j.1151-2916.1998.tb02503.x
  7. H. kondo, T. sekino, Y. H. Choa, and K. Niihara, 'Mechanical Properties of $3Y-ZrO_2/Ni$ Composites Prepared by Reductive Sintering,' Key Eng. Mater., 161-163 419-22 (1999) https://doi.org/10.4028/www.scientific.net/KEM.161-163.161
  8. H. Awaji, S. M. Choi, and E. Yagi, 'Mechanisms of Toughening and Strengthening in the Ceramic-based Nanocomposites,' Mechanics of Materials, 34 411-22 (2002) https://doi.org/10.1016/S0167-6636(02)00129-1
  9. S. M Choi and H. Awaji, 'Nanocomposites-A New Material Design Concept,' Sci. and Tech. of Advanced Mater., 6 2-10 (2005) https://doi.org/10.1016/j.stam.2004.07.001
  10. U. Leela-adisorn, T. Matsunaga, Y. Kobayashi, S. M. Choi, and H. Awaji, 'Soaking Method for Fabrication of Alumina- based Nanocomposites,' Ceramics Int., 31 803-09 (2005) https://doi.org/10.1016/j.ceramint.2004.09.007
  11. W. B. Chou and W. H. Tuan, 'Toughening and Strengthening of Alumina with Silver Inclusions,' J. Euro. Ceram. Soc., 15 291-95 (1995) https://doi.org/10.1016/0955-2219(95)90351-I
  12. H. Awaji, S-M. Choi, and E. Yagi, 'Mechanisms of Toughening and Strengthening in Ceramic-based Nanocomposites,' Mech. of Mater., 34 411-22 (2002) https://doi.org/10.1016/S0167-6636(02)00129-1
  13. H. Awaji and Y. Sakaida, 'V-Notch Technique for Singleedge Notched Beam and Chevron Notch Methods,' J. Am. Ceram. Soc., 73 [11] 3522-23 (1990) https://doi.org/10.1111/j.1151-2916.1990.tb06490.x
  14. I. Levin and D. Brandon, 'Metastable Alumina Polymorphs: Crystal. Structures and Transition Sequences,' J. Am. Ceram. Soc., 81 [8] 1995-2012 (1998) https://doi.org/10.1111/j.1151-2916.1998.tb02581.x
  15. R. W. Davidge, R. J. Brook, F. Cambier, M. Poorteman, A. Leriche, D. O'Sullivan, S. Hampshire, and T. Kennedy, 'Fabrication, Properties, and Modelling of Engineering Ceramics Reinforced with Nanoparticles of Silicon Carbide,' British Ceramic Transaction, 96 [3] 121-27 (1997)
  16. H. Awaji., T. Matsunaga, and S. M. Choi, 'Relation between Strength, Fracture Toughness, and Critical Frontal Process Zone Size in Ceramic,' Materials Trans., 47 1532-39 (2006) https://doi.org/10.2320/matertrans.47.1532

Cited by

  1. Novel and solvent-free cochineal-assisted synthesis of Ag–Al2O3 nanocomposites via solid-state thermal decomposition route: characterization and photocatalytic activity assessment vol.27, pp.9, 2016, https://doi.org/10.1007/s10854-016-5044-x
  2. Synthesis of Ag–AgO/Al2O3 nanocomposite via a facile two-step method for photodegradation of methylene blue vol.28, pp.17, 2017, https://doi.org/10.1007/s10854-017-7134-9
  3. Toughening mechanism and frontal process zone size of ceramics vol.117, pp.1365, 2009, https://doi.org/10.2109/jcersj2.117.623