DOI QR코드

DOI QR Code

Wear Characteristics and Thermal Stability of PA66/silane treated MoS2 Composites

  • Nam, Ki-dong (Department of Chemical Engineering, Kyung Hee University) ;
  • Gu, Bo-ram (Department of Chemical Engineering, Kyung Hee University) ;
  • Ryu, Sung-hun (Department of Chemical Engineering, Kyung Hee University)
  • Received : 2020.12.01
  • Accepted : 2020.12.17
  • Published : 2020.12.31

Abstract

We functionalized a wear-resistant carbon-based MoS2 filler to solve its limited wear condition problem. The filler exhibits excellent lubricative properties. The surface modification of MoS2 was carried out using a (3-glycidyloxypropyl)trimethoxysilane (GPTMS) silane coupling agent to improve the low compatibility and dispersibility of the filler that generally degrade the performance of composites. A silane coupling agent was employed for the functionalization of MoS2, and its effect on the wear resistance of MoS2/Polyamide-6,6 was investigated. The silanization of MoS2 was identified by contact angle analysis and Fourier-transform infrared, energy dispersive X-ray, and X-ray photoelectron spectroscopies. The wear resistance of the composite was found to be improved significantly by the surface functionalization of MoS2.

Keywords

References

  1. Seok Han Yoon, "자동차용화학소재 : 자동차용섬유화학소재 개발 동향", 공업화학전망 16권6호 (2013).
  2. M.Y. Lyu, "Application Trend of Plastics: Manufacturing Technology of Plastics for Lightweight Automobile", 소성가공 443-450 (2015).
  3. S.G Lee, "자동차용 복합재료", 기계저널 39권2호, (1997).
  4. H.Unal, "Abrasive wear behaviour of polymeric materials", Materials & Design vol 26 705-710 (2005). https://doi.org/10.1016/j.matdes.2004.09.004
  5. B. N. Ravi Kumar, "Effect of Abrasives on Three-Body Abrasive Wear Behaviour of Particulate-Filled Polyamide66/Polypropylene Nanocomposites", Composite Interfaces vol 17 (2010).
  6. S. M. Lee, "Effect of carbon-nanotube length on friction and wear of polyamide 6,6 nanocomposites", Wear (2014).
  7. Riadh Autay, "Effect of hygrothermal aging on mechanical and tribological behaviors of short glass-fiberreinforced PA66", Thermoplastic Composite Materials (2019).
  8. Y. Xing, "Study on the Friction and Wear Behaviors of Modified PA66 Composites", Polymer-Plastics Technology and Engineering (2009).
  9. H. Hunke, "Plasma modified Polytetrafluoroethylene (PTFE) lubrication of α-olefin-copolymer impact-modified Polyamide66", Wear (2015).
  10. Seung-Soo Kim, "Pyrolysis Characteristics of the Mixture of Waste Fishing Net and Waste Ship Lubricating Oil", Industrial and Engineering Chemistry (2008).
  11. S. C. Kang, "The Friction and Wear of the Plastic (Polymer) Bearing Materials in Lubricated Condition", 한국과학기술부 (1991).
  12. E. Basavaraj, "A Study on Mechanical, Thermal, and Wear Characteristics of Nylon 66/Molybdenum Disulfide Composites Reinforced With Glass Fibers", Polymer composites (2012).
  13. T. Kubart, "Temperature dependence of tribological properties of MoS2 and MoSe2 coatings, Surface and Coatings Technology (2005).
  14. Paula Ussa Aldana, "WS2 nanoparticles anti-wear and friction reducing properties on rough surfaces in the presence of ZDDP additive", Tribology International (2016).
  15. J. Korzekwa, "Wear Mechanism of Al2O3/WS2 With PEEK/BG Plastic", Tribology (2014).
  16. YR Liang, "Mechanical and tribological properties of nitrile rubber filled with modified molybdenum disulphide", Plastics, Rubber and Composites (2016).
  17. M. Khodaei, "Superhydrophobicity on aluminum through reactive-etching and TEOS/GPTMS/nano-Al2O3 silane-based nanocomposite coating", Surface and Coatings Technology (2019).
  18. Kaline Pagnan Furlan, "Self-lubricating composites containing MoS2: A review", Tribology International (2018).
  19. Stanislav Presolski, "Covalent functionalization of MoS2", Materials today (2016).
  20. Ning Kong, "Advantages of using self-lubricating, hard, wear-resistant MoS2-based coatings", RSC Advances (2020).